ABS Resin Plastic Pellets

ABS (Acrylonitrile Butadiene Styrene)

At Suke Plastics, we mainly supply ABS resin from these suppliers brands:

  • Chimei Polylac® ABS
  • FCFC Tairilac® ABS
  • LG Chem ABS
  • Ineos ABS
  • Yulong ABS
  • PetroChina Jieyang ABS
  • Toray Malaysia ABS
  • Shandong Eastech ABS
acrylonitrile butadiene styrene abs resin

Supply Various Grades of ABS pellets

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
ABSPA-704 LRPChi MeiPolylacLow residual monomer gradeMedical Application
ABSPA-709Chi MeiPolylacGeneral Purpose GradePlumbing fittings/front and rear vehicle spoiler/motorcycle fenders/safety helmets/water filter casings
ABSPA-709SChi MeiPolylacExtrusion gradePipe materials/appliances/large containers
ABSPA-727Chi MeiPolylacElectroplatingGeneral molding for decorative accessories, audio equipment panels, tire covers, toiletries, clock casings
ABSPA-746Chi MeiPolylacHigh flow gradeSuitable for thin wall and high impact strength molding parts
ABSPA-747Chi MeiPolylacGeneral Purpose GradeMotorcycle fenders, shoe heels, snow sport products, water filter casings
ABSPA-756Chi MeiPolylacHigh flow gradeLarge area or thin-walled molded products
ABSPA-757Chi MeiPolylacGeneral Purpose GradeHome appliance/Office appliance/electronic product casings/copier casings/telephone casings/boxes for cosmetics and so on.
ABSPA-757 ABChi MeiPolylacAntimicrobial Grade (Antibacterial Grade)Daily necessities/ Home appliances/ Building materials/ Medical related equipment/ Food contact items/ others
ABSPA-757FChi MeiPolylacLow residual monomer gradeFood containers, kettles, kitchenware, toys
ABSPA-763Chi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-764Chi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-765Chi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-765AChi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-765BChi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-777BChi MeiPolylacHigh heat gradeShells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
ABSPA-777DChi MeiPolylacHigh heat gradeShells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
ABSPA-777EChi MeiPolylacHigh heat gradeShells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
ABSPA-737Chi MeiPolylacHigh flow gradeLarge area or thin-wall molded products
ABSPA-757HChi MeiPolylacHigh flow gradeHousehold appliances, motorcycle parts, large area or thin-wall molded products
ABSPA-746HChi MeiPolylacHigh flow gradeSuitable for thin wall and high impact strength products
ABSPA-746MChi MeiPolylacHigh flow gradePaintable two wheeler application
ABSPA-756HChi MeiPolylacHigh flow gradeUltra-large area or ultra-thin-wall molded products
ABSPA-756SChi MeiPolylacHigh flow gradeLarge area or thin-wall molded products
ABSPA-747RChi MeiPolylacExtrusion gradeextrusion materials,Luggage/suitcases/refrigerator plating materials
ABSPA-747FChi MeiPolylacExtrusion gradeRefrigerator plating materials
ABSPA-747HChi MeiPolylacExtrusion gradeRefrigerator plating materials
ABSPA-747SChi MeiPolylacExtrusion gradeSheet extrusion and injection parts
ABSPA-709PChi MeiPolylacExtrusion gradePipe materials
ABSPA-763AHChi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-763HChi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-764BChi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-764GChi MeiPolylacFlame retardant gradeDisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-77NBChi MeiPolylacHigh heat gradeInterior Components for automotive.
ABSPA-726MChi MeiPolylacElectroplatingCar radiator front shields, car moldings, car license plates, automotive parts
ABSPA-737 A03Chi MeiPolylacStandard colorHome appliance/Large area or thin-wall molded products
ABSPA-757 J01Chi MeiPolylacStandard colorShells for household appliances/boxes for cosmetics/office appliances
ABSPA-757G J08Chi MeiPolylacStandard colorLCD TV front casing, LCD TV stands, LCD shells, DVD audio shells, digital photo frame boarders
ABSPA-757 A01Chi MeiPolylacStandard colorShells for household appliances, cosmetics containers, office appliances
ABSPA-747S A01Chi MeiPolylacStandard colorsheet-extrusion and high impact injection parts
ABSPA-797Chi MeiPolylacChemical resistance gradeKitchen and home appliances
ABSPA-707Chi MeiPolylacGeneral Purpose GradeTelephone casings, lamp seats, toys, office supplies, clock casings, buttons for household appliances
ABSPA-717CChi MeiPolylacGeneral Purpose GradeKitchen appliances, audio supplies, toilet seats, washing machines, vacuum cleaner housings, tool handle accessories
ABSPA-1730Chi Mei (Zhenjiang)PolylacGeneral Grade. Bulk Polymerization Process, bulk ABS. Low odor, low residual monomer, low gloss.Modification Applications: Small household appliances, internal electrical components, automotive door panel inner frames…
ABSPA-717CKChi Mei (Zhenjiang)PolylacGeneral Grade. High impact strength.Kitchenware, audio equipment, toilet seats, washing machines, vacuum cleaner housings, tool handles and accessories, etc.
ABSPA-707KChi Mei (Zhenjiang)PolylacGeneral Grade. High gloss, high rigidity, excellent flexural strength.Telephone housings, lamp holders, toys, office supplies, clock casings, small household appliances, etc.
ABSPA-757KChi Mei (Zhenjiang)PolylacGeneral Grade. High rigidity, high gloss, medium impact strength.TV front bezels, photocopier housings, telephone casings, cosmetic containers, wheel covers, etc.
ABSPA-749KChi Mei (Zhenjiang)PolylacGeneral Grade. Ultra-high impact strength.Safety helmets, motorcycle fenders, shoe heels, snow sports equipment, water filter housings, etc.
ABSD-180Chi Mei (Zhenjiang)PolylacGeneral Grade. High rigidity, high gloss, medium impact strength.TV front bezels, photocopier housings, telephone casings, cosmetic containers, wheel covers, etc.
ABSD-190Chi Mei (Zhenjiang)PolylacGeneral Purpose Grade. High gloss, high rigidity, excellent flexural strength.Telephone housings, lamp holders, toys, office supplies, clock casings, small home appliances, etc.
ABSPA-749SKChi Mei (Zhenjiang)PolylacExtrusion Grade. High impact strength; suitable for both extrusion and injection molding.Tubing, luggage, helmets, refrigerator components, etc.
ABSD-120Chi Mei (Zhenjiang)PolylacExtrusion Grade. High impact strength; suitable for both extrusion and injection molding.Tubing, luggage, helmets, refrigerator components, etc.
ABSD-1000Chi Mei (Zhenjiang)PolylacFlame Retardant Grade. Standard flow; 1.5mm V-0, 2.5mm 5VB, 3.0mm 5VA (TBBA-based).Set-top boxes, power switch panels, power sockets, car batteries, cash register housings, light boxes, DVD players, car audio control panels, etc.
ABSD-1200Chi Mei (Zhenjiang)PolylacFlame Retardant Grade. Standard flow; 1.5mm V-2, 2.5mm V-0, 2.5mm 5VB, 3.0mm 5VA (TBBA-based).Set-top boxes, power switch panels, power sockets, car batteries, cash register housings, light boxes, DVD players, car audio control panels, etc.
ABSD-1400Chi Mei (Zhenjiang)PolylacFlame Retardant Grade: 3.0mm V0 (TBBA Series)Set-top boxes, power switch panels, power outlets, car batteries, cash register housings, light boxes, DVD players, car audio control panels, etc.
ABSD-2200Chi Mei (Zhenjiang)PolylacHeat-Resistant Grade: High Impact StrengthAutomotive-related products, electronics, electrical appliances, etc.
ABSD-2400Chi Mei (Zhenjiang)PolylacHigh Heat-Resistant GradeAutomotive-related products, electronics, electrical appliances, etc.
ABSPA-757KFChi Mei (Zhenjiang)PolylacLow Residual Monomer Grade: Food Contact Compliant (Passed GB4806); Low Residual Monomer ContentFood containers, small household appliances.
TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
ABSAG15A1-HFormosa (FCFC)TairilacGeneral Purpose Grade. High gloss,Medium impactToys, Caculators, Phone, Clock housing, Stereo housing, Suitcase
ABSANC160Formosa (FCFC)TairilacSelf Extinguishing Grade. Flame retardantFlame retardant materials;Housing of LCD monitor, LCD-TVcomputers & OA machine
ABSAG12A0Formosa (FCFC)TairilacGeneral Purpose Grade. Super high impactHelmets, Shoe heels, Pipe fittings, Products of low-temp usage
ABSAG12A3Formosa (FCFC)TairilacGeneral Purpose Grade. High impactShoe heels, Toys, Clock housing, Stereo housing, Suitcase, The plate-like products
ABSAG15A3Formosa (FCFC)TairilacGeneral Purpose Grade. High gloss, Medium impactToys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
ABSAG15E3Formosa (FCFC)TairilacGeneral Purpose Grade. High gloss, High rigidToys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
ABSAG15E1Formosa (FCFC)TairilacGeneral Purpose Grade. High gloss, High rigidToys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
ABSAG100HFormosa (FCFC)TairilacGeneral Purpose Grade. Super high impactHelmets, Shoe heels, Pipe fittings, Products of low-temp usage
ABSAF3500Formosa (FCFC)TairilacHigh Flow Grade. High impactHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAF3560Formosa (FCFC)TairilacHigh Flow Grade. High impactHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAF3530Formosa (FCFC)TairilacHigh Flow Grade. High impact, Chemical resistantHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAF3535Formosa (FCFC)TairilacHigh Flow Grade. High impactHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAX4000Formosa (FCFC)TairilacHeat Resistant Grade. Medium high heatParts of cars, Electrical appliances, Hair dryer, Heat resistant parts
ABSAX4300Formosa (FCFC)TairilacHeat Resistant Grade. Medium high heat, Extrusion blow moldingParts of cars, Electrical appliances, Hair dryer, Heat resistant parts
ABSANC100Formosa (FCFC)TairilacHeat Resistant Grade, Flame retardantFlame retardant materials;Housing of LCD monitor, LCD-TV,computers & OA machine
ABSAG23ATFormosa (FCFC)TairilacElectroplating Grade (Mental Plating Grade). High impactWheel cover, Knobs, Tags,Door handle, Plating products
ABSAG10APFormosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products,Crash helmets,Pipes, Shoe heels
ABSAE8000Formosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products,Crash helmets,Pipes, Shoe heels
ABSAG10NPFormosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products,Crash helmets,Pipes, Shoe heels
ABSAE8700Formosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products, Crash helmet, Pipes, Shoe heels
ABSANC120Formosa (FCFC)TairilacSelf Extinguishing Grade. Flame retardantFlame retardant materials;Housing of LCD monitor, LCD-TVcomputers & OA machine
ABSAE10EPFormosa (FCFC)TairilacExtrusion Grade (Jet Black Extrusion Grade). Extrusion molding, Super high impact, High rigidPipes
ABSAX4100Formosa (FCFC)TairilacHeat Resistant Grade. Super high heatParts of cars, Electrical appliances, Hair dryer, Heat resistant parts
ABSAG16A1Formosa (FCFC)TairilacHealth Care Grade. High rigid, Medium impactScalpel shank, Asthma inhaler Meets the requirements of USP Plastic Class VI
ABSAG20GFFormosa (FCFC)Tairilac“20%GF Reinforced Grade. Dimensional stability, High heat resistantPrinter parts
TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
ABSAP163LG Chem/with high antistatic property and high impact strength.injection molding, Semiconductor
ABSHI121HLG Chem/Impact Resistance, General PurposeElectrical/Electronic Products, Miscellaneous Goods
ABSHI121ULG Chem/Injection molding,impact resistance and UV resistance.Electrical/Electronic Products, Miscellaneous Goods
ABSHI121UNSLG Chem/UV Resistance, Antistatic, Impact ResistanceElectrical/Electronic Products, Miscellaneous Goods
ABSHI130LG Chem/Injection molding,very high impact strength and bright white colorMotorcycle Interior Parts Refrigerator
ABSHI135LG Chem/Product for injection molding with high impact strength; High Rubber Content.Safety helmets, Miscellaneous goods
ABSHI140LG Chem/Injection molding, designed to have super high impact strength and bright white colorSafety Helmet Motorcycle Parts.
ABSHP100HLG Chem/with high impact, low temperature resistance and satisfactory spray paint effect. Opaqueness, Hot Stamping, Paintability,Helmets, watches, refrigerators
ABSHP100SLG Chem/Opaqueness, Hot Stamping, Paintability, Multi-axial Impact Strength, High StiffnessBags, fans, electric toothbrushes
ABSHP171LG Chem/General purpose injection molding grade with medium flow and high gloss.Router, Ear Phone, remote control, oxygen concentrator.
ABSHP181LG Chem/Injection molding, with high flow and excellent impact properties. Opaqueness, Hot Stamping, Paintability, Bright White, Colorability, Dimensional StabilityWashing machines, air conditioners, air purifiers, sweeping robots
ABSHT550LG Chem/High Gloss, High StiffnessElectrical/Electronic Products Electric Bike
ABSHT700LG Chem/High StiffnessPiano Key, Bobbin, Electrical/Electronic Products, Miscellaneous Goods
ABSSG175LG Chem/Injection molding, designed to have a super gloss level.Refrigerator, Washing Machine, Electrical/Electronic Products
ABSSG175GLG Chem/Injection molding, designed to have extra high gloss and high fluidity. Super Gloss, High Flow.Electrical/Electronic Products
ABSSG175HLG Chem/Super Gloss, UV Resistance.Refrigerator, Washing Machine, Electrical/Electronic Products.
ABSMP220-HLG Chem/Electroplating Grade (Mental Plating Grade).Excellent adhesion and processabilityAutomobiles Radiator Grille, Molding
ABSRS650LG Chem/Product for extrusion molding with high impact strength.General Extruded Sheet, Pipe, Bathroom Ceiling
ABSRS670LG Chem/Thermoforming, Chemical Resistance to Cyclopentane, High Impact Strength.Refrigerator
ABSRS681LG Chem/Extrusion grade, high strength and vacuum blister performance. Hot Stamping, Paintability, Chemical Resistance to Cyclopentane, Multi-axial Impact Strength, Curve Destruction Weight.Extruded Board, refrigerator liners, home profiles.
ABSSH610ALG Chem/Product for extrusion molding with high impact strength.General Extruded Sheet
ABSAF312ALG Chem/Injection molding, with 1.5mm V-0 flame retardancy and high flow. Hot Stamping, Paintability, imensional Stability.Switch panel, socket, Charge, electric control box
ABSAF312BLG Chem/Fire resistance (2.1mm V-0). Opaqueness, Hot Stamping, Paintability, High Gloss,Dimensional Stability, High Flow.Heater, electric control box, Charge bank, hair dryer.
ABSAF312CLG Chem/Opaqueness, Flame Retardancy, Hot Stamping, Paintability, High Gloss, Dimensional Stability, High Flow.Power switches, alarms, uninterruptible power supplies, security cameras
ABSAF362HLG Chem/fire resistance (3.2mm V-0)Blood pressure monitor, oxygen concentrator, pulse monitor
ABSAF364LG Chem/High Flame Retardancy, Medium Heat ResistanceHair Dryer, Terminal Box, Electrical/Electronic Products
ABSAF365LG Chem/Product for injection molding with 2.0mm V-0 flame retardancy.Batter Case, PCB Case, Electrical/Electronic Products
ABSAF365BLG Chem/Flame Retardant ABS product for injection molding, V-0 at 2.0mm.Electrical/ElectronicProducts,IT/OADevices,TV,MonitorHousing
ABSAF365F-LLG Chem/Flame Retardant ABS product for injection molding, V-0 at 2.0mm, high fluidity and good dimensional stability.Television, Bidet, Electrical/Electronic Products
ABSAF365HLG Chem/Opaqueness, Flame Retardancy, Medium Heat Resistance, Hot Stamping, Paintability, High Gloss, Bright White, Thermal Stability, ColorabilityControl cabinet, fireproof Board, router, Print
ABSAF365HBLG Chem/fire resistance (2.0mm V-0)Special for battery
ABSAF365HFLG Chem/Opaqueness, Medium Heat Resistance, Hot Stamping, Paintability, High Gloss, Bright White, Thermal Stability, Colorability, High Flow.Distribution boxes, medical equipment, speakers, frequency converters.
ABSAF365SLG Chem/Flame Retardant ABS product for extrusion and blow molding, V-0 at 2.0mmBattery Tray
ABSAF366LG Chem/Flame Retardant ABS product for injection molding, V-0 at 1.5mm.Batter Case, PCB Case, Electrical/Electronic Products
ABSAF366ALG Chem/Product for injection molding with 1.5mm V-0 flame retardancy and high fluidity.Electrical/Electronic Products, IT/OA Devices, TV, Monitor Housing
ABSAF366FLG Chem/Product for injection molding with 1.5mm V-0 flame retardancy and high fluidity.Television, Electrical/Electronic Products
ABSAF366HLG Chem/fire resistance (1.5mm V-0)Speakers, oxygen concentrators, heaters, toilet seats
ABSAF366HFLG Chem/fire resistance (1.5mm V-0).Opaqueness, Bright White.Industrial electronic control boxes, purifiers, heaters.
ABSAF367CLG Chem/Flame Retardancy V-0 at 2.5mmElectrical/Electronic Products, IT/OA Devices, TV, Monitor Housing.
ABSAF367HLG Chem/fire resistance (2.5mm V-0). High thermal resistance, and good Thermal stability.Blood pressure monitor, oxygen concentrator, power supply development, socket.
ABSEF378LLG Chem/Flame Retardancy, Non-HalogenMFP (Multi-Function Printer), Sound Bar, Electrical/Electronic Products
ABSFR500LG Chem/Flame Retardancy, ImflammabilityElectrical/Electronic Products
ABSFR500ALG Chem/A TBBA Flame Retardant ABS product for injection molding, V-0 at 1.5mmElectrical/Electronic Products
ABSFR500HLG Chem/A TBBA Flame Retardant ABS product for injection molding, V-0 at 2.5mm.Electrical/Electronic Products.
ABSFR530LG Chem/Flame Retardancy, Thermal Stability, Colorability,Imflammability.Electrical/Electronic Products Medical Equipment Housing.
ABSBM662LG Chem/Standard Purpose, High Heat Resistance, PaintabilitySpoiler
ABSER232LG Chem/High Heat Resistance, Metal Plating, Thermal Stability, Superior Surface Quality, High Flow.Bumper, Cockpit, Door Trim, Exterior ETC, Interior ETC, Outside Mirror, Rear Combination Lamp.
ABSER400LG Chem/Medium Heat Resistance, High Impact StrengthAutomotive Interior Parts, Automotive Exterior Parts, Sheet
ABSER400-CLG Chem/Medium Heat Resistance, Low TVOC, Low GlossGeneral Extruded Sheet, Edge Band
ABSER400-MLG Chem/Medium Heat Resistance, Non Painting, Low TVOC, Low GlossCockpit, Door Trim, Edge Band, Interior ETC
ABSER460LG Chem/Medium Heat ResistanceMotorcycle, Vacuum Cleaner, Electrical/Electronic Products, Miscellaneous Goods
ABSER468LG Chem/Medium Heat Resistance, High FlowElectrical/Electronic Products, Miscellaneous Goods.
ABSNF424LG Chem/High Heat Resistance, Low TVOCAutomotive Interior Components (e.g., vents, control panels); Consumer Electronics Housings; Household Appliances and Kitchenware; Office Equipment Parts.
ABSXR401LG Chem/Standard Purpose, High Heat Resistance, Paintability, High Impact StrengthAir Conditioner, Air Purifier, Battery, Bumper, Cockpit, Coffee Machine, Consent, Dehumidifier, Delivery Robot, Door Trim, Drone, Electric Bike, Exterior ETC, Fan, Fan Heater, Fire Alarm, Food Serving Robot, Interior ETC, Microwave Oven, Motorcycle, Multi Tap, Outside Mirror, PCB (Printed Circuit Board), Power Tool, Security Alarm, Set-Top Box, Switch, Terminal Box, Tractor, UPS (Uninterruptible Power Supply System), Water Purifier, Wireless Router.
ABSXR401BLG Chem/High Heat Resistance, Paintability, Chemical Resistance/
ABSXR404LG Chem/Standard Purpose, High Heat Resistance, Paintability, High StiffnessAir Conditioner, Battery, Bumper, Cockpit, Coffee Machine, Consent, Delivery Robot, Electric Bike, Electric Rice Cooker, Fan, Fan Heater, Fire Alarm, Food Serving Robot, Hair Dryer, Microwave Oven, Motorcycle, Multi Tap, Others, Outside Mirror, PCB (Printed Circuit Board), Power Tool, Rear Combination Lamp, Security Alarm, Set-Top Box, Spoiler, Switch, Terminal Box, Tractor, UPS, Water Purifier, Wireless Router.
ABSXR404TLG Chem/High Heat Resistance, Welding, Superior Surface Quality, Welding StrengthRear Combination Lamp
ABSXR409HLG Chem/Standard Purpose, Ultra High Heat Resistance, Non PaintingCockpit, Door Trim, Fire Alarm, Hair Dryer, Interior ETC, Microwave Oven, Rear Combination Lamp, Set-Top Box, Tractor, Wireless Router.
ABSXR410LG Chem/High Heat Resistance, Non Painting, Low TVOC, Low GlossCockpit, Door Trim, Interior ETC
ABSXR438LG Chem/Ultra High Heat Resistance, Paintability, Chemical Resistance, Dimensional Stability./
ABSXR440LG Chem/High Heat Resistance, Non Painting, Low TVOC, Low GlossCockpit, Door Trim, Interior ETC
ABSXR470LG Chem/Ultra High Heat Resistance, Low TVOCCockpit, Door Trim, Others
ABSXR474LG Chem/Ultra High Heat Resistance, Non Painting, Low TVOC/
ABSXR490LG Chem/Ultra High Heat Resistance, Non Painting, Low TVOC, Low GlossCockpit, Door Trim, Others
ABSXR630LG Chem/High Heat Resistance, Chemical ResistanceWindow Profile Insulation Bar
Type Grade No. Manufacturer Brand Grade/Features Use/Applications
ABS GP-22 Ineos Styrolution Terluran easy-flow Injection molding, Appliance housings, Household and sanitary appliances, Toys, Automotive components, Consumer products
ABS HI-10 Ineos Styrolution Terluran medium flow Injection molding, Compounding, Appliance housings, Lawn & garden components requiring superior toughness
ABS GP-35 Ineos Styrolution Terluran high-flow Injection molding, Thin wall components for telecommunications, Household and sanitary appliances, Toys, Automotive components, Electroplating
TypeGrade No.ManufacturerBrandGrade
ABSA-2020Yulong/General Purpose Grade
ABSA-2021Yulong/General Purpose Grade
TypeGrade No.ManufacturerBrandGrade
ABSHF-681PetroChina (KunLun)/High flow grade
ABS0215EPetroChina (KunLun)/General Purpose Grade
ABS0215APetroChina (KunLun)/General Purpose Grade
ABS0215HPetroChina (KunLun)/General Purpose Grade
TypeGrade No.ManufacturerBrandGrade
ABSL322Eastech Chemical/High-flow injection molding grade
ABSC442Eastech Chemical/Heat-resistant injection molding grade with low residue
ABSM4Eastech Chemical/Matte extrusion grade with high stretch ratio and smooth surface finish
ABSE332Eastech Chemical/Injection/Extrusion grade
ABSF332Eastech Chemical/General-purpose injection molding grade
ABSB432EEastech Chemical/General-purpose extrusion grade
ABSB532EEastech Chemical/General-purpose extrusion grade
ABSB732EEastech Chemical/Injection/Extrusion molding grade

What is ABS Resin?

Acrylonitrile Butadiene Styrene (ABS) is a high-performance, engineering-grade thermoplastic polymer known for its outstanding impact resistance, toughness, and excellent surface finish. As a versatile and cost-effective material, ABS resin is widely used across various industries, including automotive, electronics, appliances, and consumer products.

Other Names

  • Acrylonitrile Butadiene Styrene (ABS)
  • ABS Polymer
  • ABS Plastic
  • ABS Copolymer
  • ABS Pellets
  • ABS Granules

Appearance

  • milky white
  • off-white

Packaging

  •  25kg PE bags or jumbo bags

HS Code

  • 39033010

Key Properties of ABS Resin

Technical Data

PropertyGeneral Grade
Density (g/cm³)1.03 – 1.07 g/cm³
Tensile Strength (MPa)40 – 50 MPa
Flexural Modulus (MPa)2000 – 2500 MPa
Izod Impact Strength15 – 30 kJ/m²
Heat Deflection Temp (°C)85 – 105°C
Melt Flow Index (MFI)1 – 20 g/10 min

Applications of ABS Resin

ABS Resin Grades We Offer

Frequently Ask Questions

Find answers to the most common questions about ABS resin, including its composition, processing methods, certifications, and handling guidelines. Our expert responses help you make informed sourcing and application decisions.

What is ABS resin made of?

ABS (Acrylonitrile Butadiene Styrene) is a terpolymer composed of three monomers: acrylonitrile for chemical resistance and heat stability, butadiene for toughness and impact strength, and styrene for rigidity and a glossy finish. This combination results in a versatile thermoplastic with a good balance of mechanical, thermal, and aesthetic properties.

Is ABS resin safe for food contact applications?

Yes, food-grade ABS is available and complies with FDA and EU food contact regulations. Please specify your intended use when requesting a quote or sample, so we can provide the appropriate compliant grade.

Can ABS resin be electroplated or chrome-plated?

Yes. Electroplating-grade ABS is specially formulated to allow strong adhesion of metal coatings. It is commonly used for decorative chrome finishes in automotive and sanitary ware applications.

What is the difference between virgin ABS and recycled ABS?

Virgin ABS is made from new raw materials and offers consistent mechanical and aesthetic properties. Recycled ABS is more environmentally friendly and cost-effective, but may have slightly lower performance. It is ideal for non-critical applications.

Is ABS resin UV-resistant or suitable for outdoor use?

Standard ABS is not UV-stabilized and may degrade under prolonged sunlight. For outdoor applications, UV-stabilized ABS or ASA (Acrylonitrile Styrene Acrylate) is recommended due to better weather resistance and color retention.

What are the typical processing methods for ABS resin?

ABS can be processed via injection molding, extrusion, blow molding, thermoforming, and 3D printing. It offers good flow characteristics, thermal stability, and compatibility with various molding techniques.

What are the typical shrinkage and molding conditions for ABS?

ABS resin typically has a shrinkage rate of 0.4% to 0.7%. Recommended injection molding temperatures range from 200°C to 250°C, with mold temperatures between 40°C and 80°C. Processing conditions may vary by grade.

Is ABS resin environmentally friendly?

While ABS is not biodegradable, we offer recycled ABS grades to reduce environmental impact. All our resins comply with RoHS and REACH regulations. ABS is also recyclable and can be reused in various secondary applications.

What certifications do your ABS resins comply with?

Our ABS resins meet international standards such as RoHS, REACH, UL94 (for flame-retardant grades), and ISO 9001:2015. We can provide TDS, MSDS, and compliance declarations upon request.

How should ABS resin be stored and handled?

ABS resin should be stored in a dry, ventilated area away from direct sunlight and moisture. Keep the packaging sealed until use. If exposed to humidity, pre-drying may be required (typically at 80°C for 2–4 hours) before processing.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.