BASF
BASF Ultramid portfolio includes both PA6 and PA66. These materials come in a variety of molecular weights and viscosities. Manufacturers can select from grades that include additives or reinforcements like glass fibers or minerals. This versatility makes them suitable for automotive parts, electrical devices, home appliances, and general industrial use.
Basf available for bulk purchase
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PA6 | 8202HS BK102 | Basf | ULTRAMID® | General-purpose injection molding material, heat-stabilized, low-viscosity. | Automotive, Passenger cars, Connectors & Cable / CEE Plugs, Electronics / Switchgears, Fitting, Cabinet, Office chair, Office seating, Garden tool, DIY tool, Performance Polymers, CEE plugs, Furniture Fittings, Connectors & Relays, Electrical Control Units |
| PA6 | 8272G HS BK 102 | Basf | ULTRAMID® | Blow molding grade with 12% glass fiber reinforcement, excellent chemical resistance, creep resistance, good stiffness and mechanical strength, heat-stabilized, resistant to hydrocarbons, oils, and solvents, ultra-high viscosity. | Automotive, Passenger cars, Structural Inserts And Stiffeners, Air Ducts, Fuel System Components, Electrical Control Units, Seat structures |
| PA66 | A3EG3 | Basf | ULTRAMID® | 15% glass fiber reinforced, good stiffness, oil-resistant. | Passenger Cars, Water heaters, Boiler, Passenger Cars, Automotive, Bath & Sanitary Residential, Sanitary, Mobilephone cover, Speakers, AR & VR, Keyboard |
| PA66 | A3EG10 | Basf | ULTRAMID® | 50% glass fiber reinforced, high rigidity, oil-resistant. | Kitchen & Household, Automotive, Passenger cars, Electronics, Miniature Circuit Breakers, Switchgears, Bearing Cage, Engine Cover |
| PA66 | A3EG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, injection molding grade, high rigidity, excellent dimensional stability, oil-resistant. | Kitchen & Household, Automotive, Passenger cars, Connectors & Cable / Connectors, Electric / Miniature Circuit Breakers, Electronics / Switchgears |
| PA66 | A3EG6 | Basf | ULTRAMID® | 30% glass fiber reinforced, high dimensional stability, high rigidity, oil-resistant. | Connectors & Cable / Connectors, Electric / Lighting, Miniature Circuit Breakers, Electronics / Switchgears, Office chair, Sofa, Sitting cushion, Chair, Ball Bearings |
| PA66 | A3EG7 | Basf | ULTRAMID® | 35% glass fiber reinforced, high dimensional stability, high rigidity, oil-resistant. | Electrical Appliances / Dish Washer, Oven, Microwave , Water heaters, Boiler, Small Appliances / Housing, Functional parts , Kitchen & Household , Personal care |
| PA66 | A3HG2 | Basf | ULTRAMID® | 10% glass fiber reinforced, injection molding grade, good electrical insulation properties, medium stiffness. | Automotive, Passenger cars, Accessories / Mobilephone cover, Speakers, AR & VR, Keyboard, Ball Bearings, Performance Polymers, Connectors & Relays |
| PA66 | A3SK | Basf | ULTRAMID® | Injection molding grade, short cycle time, excellent flowability, oil-resistant. | Small Appliances / Housing, Functional parts , Kitchen & Household, Airbag, Bearing Cages, Connectors & Relays, CEE Plugs, Miniature Circuit Breakers, Switchgears, Performance Polymers |
| PA66 | A3UG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, halogen-free, low phosphorus content (approaching zero), oil-resistant. | Performance Polymers, LED Lighting, Power Electronics, Switchgears, (Leisure & Sport) Toys, Ball, Accessories, Automotive, Passenger cars |