Chimei Flame Retardant ABS Resin

  • Home /
  • Chimei Flame Retardant ABS Resin

Chimei Polylac® FR ABS — Full Grade Portfolio

Disclaimer: Typical values from Chimei ISO TDS; not a specification. UL94 colors/thickness must be verified against current UL Yellow Card. RoHS/REACH/halogen/PFAS status not confirmed unless report provided. Buyer must test suitability.

🔹 High-Impact FR (General Purpose)
GradePositioningUL94 (ISO TDS)MFI (220°C/10kg)Vicat (1kg)HDT (1.8MPa, Ann.)Izod @23°C
PA-763High-impact FRV-0 @1.5mm; 5VA @2.5mm25 ml/10min103°C96°C22 kJ/m²
🔹 High-Flow FR, High Heat (Thin-Wall & Precision Parts)
GradePositioningUL94 (ISO TDS)MFI (220°C/10kg)Vicat (1kg)HDT (1.8MPa, Ann.)Izod @23°C
PA-763AHHigh-flow; high heat; light stableV-0 @2.0mm; 5VB @2.0mm; 5VA @2.5mm45 ml/10min102°C92°C16 kJ/m²
PA-763HHigh-flow; light resistance; non-TBBAV-0 @1.5mm; 5VB @1.5mm; 5VA @2.5mm47 ml/10min102°C92°C17 kJ/m²
PA-765AHigh-flow; medium heat; high impactV-1 @1.5mm; V-0 @2.1mm; 5VB @2.1mm; 5VA @2.5mm48 ml/10min93°C84°C22 kJ/m²
🔹 Standard-Flow FR (Weather-Resistant / General Enclosures)
GradePositioningUL94 (ISO TDS)MFI (220°C/10kg)Vicat (1kg)HDT (1.8MPa, Ann.)Izod @23°C
PA-764Weather resistant; standard flowV-0 @1.5mm; 5VB @1.5mm; 5VA @2.5mm28 ml/10min101°C92°C13 kJ/m²
PA-764BStandard flow; thicker-wall FRV-0 @2.5mm; 5VB @2.5mm; 5VA @3.0mm26 ml/10min102°C93°C14 kJ/m²
PA-764GThin-wall V-0 @1.0mm; high density (1.22)V-2 @0.75mm; V-0 @1.0mm; 5VA @2.5mm34 ml/10min101°C92°C13 kJ/m²
🔹 High-Flow FR, Standard Heat (Easy Molding)
GradePositioningUL94 (ISO TDS)MFI (220°C/10kg)Vicat (1kg)HDT (1.8MPa, Ann.)Izod @23°C
PA-765Highest flow; general FRV-1 @1.0mm; V-0 @1.5mm; 5VB @1.5mm; 5VA @2.5mm58 ml/10min91°C83°C21 kJ/m²
PA-765BMedium impact; thicker-wall FRV-2 @1.5mm; V-0 @2.5mm; 5VB @2.5mm; 5VA @3.0mm44 ml/10min94°C85°C24 kJ/m²
🔹 Zhenjiang Chimei D-Series (TBBA-Based Standard Flow)
GradePositioningUL94 (ISO TDS)MFR (220°C/10kg)Softening Pt.HDT (1.8MPa, Ann.)Tensile (Yield)
D-1000Standard flow; TBBA; UL E194560V-0 @1.5mm; 5VA @3.0mm58 cm³/10min90°C83°C37 MPa
D-1200Standard flow; high rigidity; TBBAV-0 @2.5mm; V-0 @3.0mm (UL Yellow Card)47 cm³/10min92°C85°C38 MPa
D-1400Higher impact & elongation; TBBAV-2 @2.0mm; V-0 @3.0mm42 cm³/10min94°C85°C40 MPa

Note: D-Series MFR reported in cm³/10 min (ISO 1133, 220°C/10kg) per TDS. UL E194560 Yellow Card verified for all three D-grades.

Send Us a Message