ChiMei Flame Resistant PC Collection

🔹 Universal FR Baseline
GradeCore PositioningUL94 Multi-Thickness RatingAppearanceNotched Izod 23°C / -30°C (kJ/m²)UV StableKey FeatureRecommended Applications
PC-66001.0mm V-0 benchmark1.0 V-0 / 2.0 5VB / 3.0 5VAOpaque60 / 15—Non-halogen sulfonate FR systemConsumer electronics housings, connectors
PC-6600 J01PC-6600 pre-colored black1.0 V-0 / 2.0 5VB / 3.0 5VABlack60 / 15—Replaces in-house black masterbatchStandard black electronic enclosures
PC-67002.5mm V-0 transparent, mid-flow1.5 V-2 / 2.5 V-0 / 3.0 V-0Transparent60 / 15—Medium viscosity, easy processingTransparent housings, lamp panels
🔹 Low Smoke Density (Rail Transit)
GradeCore PositioningUL94 Multi-Thickness RatingAppearanceNotched Izod 23°C / -30°CUV / f1Key FeatureRecommended Applications
PC-616LSLow smoke density for rail1.0 V-0 / 2.0 5VB / 3.0 5VAOpaque60 / 15✅ UL 746C f1Low Smoke DensityRail transit interiors, metro cars
🔹 Low-Temperature Impact
GradeCore PositioningUL94 Multi-Thickness RatingAppearanceNotched Izod 23°C / -30°CUV / f1Key FeatureRecommended Applications
PC-681U1.5mm V-0, low-temp impact flagship1.5 V-0 / 3.0 5VAOpaque60 / 45 ⭐✅ UL 746C f1-30°C impact 45 kJ/m² (3× higher than peers)Cold-climate outdoor equipment, northern electrical gear
🔹 Outdoor, UV & Weather Resistant
GradeCore PositioningUL94 Multi-Thickness RatingAppearanceNotched Izod 23°C / -30°CUV / f1Key FeatureRecommended Applications
PC-66101.5mm V-0 outdoor opaque1.5 V-0 / 3.0 V-0 + 5VAOpaque60 / 15✅ UL 746C f1UV stable + f1 outdoor certifiedOutdoor electrical boxes, EV charging stations
PC-67103.0mm V-0 outdoor transparent3.0 V-0Transparent60 / 15✅ UL 746C f1Transparent + UV stableOutdoor transparent covers, warning light lenses
PC-6715VT1.5mm V-0 outdoor transparent, thin-wall1.5 V-0 / 3.0 V-0 + 5VATransparent60 / 15✅ UL 746C f1High clarity + thin-wall V-0 + UVPremium outdoor transparent housings
PC-6600C1.5mm V-0 weather + low-temp (Zhenjiang made)1.5 V-0Opaque55 / 30 (-40°C)✅ UL 746C f1Weather + low-temp (China-local UL E194560)China-market outdoor EV chargers
🔹 PFAS-Free New Grades (Provisional, EU Regulation Compliant)
GradeCore PositioningUL94 Multi-Thickness RatingAppearanceNotched Izod 23°C / -30°CUV / f1Key FeatureRecommended Applications
PC-6710NF3.0mm V-0 PFAS-Free transparent3.0 V-0Transparent60 / —✅ UV (no f1)PFAS-Free + UVEU-export transparent parts
PC-6715NF1.5mm V-0 PFAS-Free, full-thickness1.5 V-0 / 2.0 V-0 / 3.0 V-0Transparent60 / —✅ UV (no f1)PFAS-Free thin-wall full-thickness V-0EU-export thin-wall parts