Chimei POLYLAC® ABS resin is a copolymer of styrene, acrylonitrile, and butadiene, known for its excellent mechanical properties and dimensional stability. With the lowest residual monomer globally, it’s ideal for machinery, electronics, and medical products. Compliant with RoHS and REACH, POLYLAC® ensures safety across diverse applications.

acrylonitrile butadiene styrene abs resin

Chimei ABS available for bulk purchase

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
ABSPA-704 LRPChi MeiPolylacLow monomer residue (EU 10/2011 Certification), comply with Bio-compatibility test (ISO10993)Medical Application
ABSPA-709Chi MeiPolylacUltra high impact strength/good low temperature resistancePlumbing fittings/front and rear vehicle spoiler/motorcycle fenders/safety helmets/water filter casings
ABSPA-709SChi MeiPolylacUltra-high impact resistancePipe materials/appliances/large containers
ABSPA-727Chi MeiPolylacHigh impact strength, high rigidity, high gloss, electroplating dedicatedGeneral molding for decorative accessories, audio equipment panels, tire covers, toiletries, clock casings
ABSPA-746Chi MeiPolylacHigh flowability, high impact strengthSuitable for thin wall and high impact strength molding parts
ABSPA-747Chi MeiPolylacUltra-High Impact StrengthMotorcycle fenders, shoe heels, snow sport products, water filter casings
ABSPA-756Chi MeiPolylacHigh flowability, high rigidity, high gloss. Performance is comparable to PA-757Large area or thin-walled molded products
ABSPA-757Chi MeiPolylacHigh rigidity/high gloss/medium impact strengthHome appliance/Office appliance/electronic product casings/copier casings/telephone casings/boxes for cosmetics and so on.
ABSPA-757 ABChi MeiPolylacAntimicrobial Grade,ISO 22196 (JIS Z 2801) ,GB/T 31402-2015Daily necessities/ Home appliances/ Building materials/ Medical related equipment/ Food contact items/ others
ABSPA-757FChi MeiPolylacLow monomer residue (EU 10/2011 Certification)Food containers, kettles, kitchenware, toys
ABSPA-763Chi MeiPolylacLight-resistance, heat-resistance, high-impact, 1.5mm V-0, 2.5mm 5VADisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-764Chi MeiPolylacLight resistance, heat resistance, 1.5mm V-0, 1.5mm 5VB, 2.5mm 5VADisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-765Chi MeiPolylacHigh-flowability, 1.0mm V-1, 1.5mm V-0, 1.5mm 5VB, 2.5mm 5VA (TBBA series)Displays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-765AChi MeiPolylacHigh flowability, 1.5mm V-1, 2.1mm V-0, 2.1mm 5VB, 2.5mm 5VA (TBBA series)Displays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-765BChi MeiPolylacGeneral flowability, 1.5mm V-2, 2.5mm V-0, 2.5mm 5VB, 3.0mm 5VA (TBBA series)Displays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-777BChi MeiPolylacHeat resistance, high impact strengthShells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
ABSPA-777DChi MeiPolylacUltra-high heat resistance, moderate impact strengthShells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
ABSPA-777EChi MeiPolylacUltra-high heat resistant, moderate impact strengthShells for heat producing household appliances, hair dryer tubes, iron casings, heaters, auto parts, water tank covers
ABSPA-737Chi MeiPolylacHigh flowabilityLarge area or thin-wall molded products
ABSPA-757HChi MeiPolylacHigh flowability, medium strengthHousehold appliances, motorcycle parts, large area or thin-wall molded products
ABSPA-746HChi MeiPolylacHigh flowability, high impact strengthSuitable for thin wall and high impact strength products
ABSPA-746MChi MeiPolylacHigh flowability, easily molded into big parts, good painting effectPaintable two wheeler application
ABSPA-756HChi MeiPolylacUltra-high flowabilityUltra-large area or ultra-thin-wall molded products
ABSPA-756SChi MeiPolylacUltra-high flowability, moderate strength (same strength as 757)Large area or thin-wall molded products
ABSPA-747RChi MeiPolylacHigh impact strength profile extrusion materialsextrusion materials,Luggage/suitcases/refrigerator plating materials
ABSPA-747FChi MeiPolylacHigh rigidity profile extrusion materialsRefrigerator plating materials
ABSPA-747HChi MeiPolylacChemical resistance/vacuum forming/refrigerator plating materialsRefrigerator plating materials
ABSPA-747SChi MeiPolylacHigh strength for extrusion/injectionSheet extrusion and injection parts
ABSPA-709PChi MeiPolylacDedicated extruder pipesPipe materials
ABSPA-763AHChi MeiPolylacHigh-flowability, Light-resistance, heat-resistance,2.0mm V-0,2.0mm 5VB,2.5mm 5VA (Non-TBBA series)Displays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-763HChi MeiPolylacHigh-flowability, Light-resistance, heat-resistance,1.5mm V-0,1.5mm 5VB,2.5mm 5VA (Non-TBBA series)Displays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-764BChi MeiPolylacLight resistance, heat resistance 2.5mm V-0, 2.5mm 5VB, 3.0mm 5VADisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-764GChi MeiPolylacHighly flame retardant, high heat resistance, 0.75mm V-2, 1.0mm V-0, 2.5mm 5VADisplays, machine boxes, modems, power panels, power outlets, car batteries, cash register shells, printer casings, remote control, light boxes, fax machines, projectors, large-scale multifunctional peripherals, coffee machine, front and rear TV frames, DVD players, car audio consoles
ABSPA-77NBChi MeiPolylacLow VOC, heat resistanceInterior Components for automotive.
ABSPA-726MChi MeiPolylacElectroplating dedicatedCar radiator front shields, car moldings, car license plates, automotive parts
ABSPA-737 A03Chi MeiPolylacHigh flow/Medium ImpactHome appliance/Large area or thin-wall molded products
ABSPA-757 J01Chi MeiPolylacHigh rigidity/medium impact strength/standard black and pre-coloredShells for household appliances/boxes for cosmetics/office appliances
ABSPA-757G J08Chi MeiPolylacHigh gloss blackLCD TV front casing, LCD TV stands, LCD shells, DVD audio shells, digital photo frame boarders
ABSPA-757 A01Chi MeiPolylacHigh rigidity, medium impact strength, standard-white and pre-coloredShells for household appliances, cosmetics containers, office appliances
ABSPA-747S A01Chi MeiPolylacHigh strength for extrusion, injection, standard white pre-coloredsheet-extrusion and high impact injection parts
ABSPA-797Chi MeiPolylacChemical resistance and high impact resistanceKitchen and home appliances
ABSPA-707Chi MeiPolylacHigh gloss, ultra-high rigidity, especially good tensile strengthTelephone casings, lamp seats, toys, office supplies, clock casings, buttons for household appliances
ABSPA-717CChi MeiPolylacHigh impact strengthKitchen appliances, audio supplies, toilet seats, washing machines, vacuum cleaner housings, tool handle accessories
ABSPA-1730Chi Mei (Zhenjiang)PolylacGeneral Grade. Bulk Polymerization Process, bulk ABS. Low odor, low residual monomer, low gloss.Modification Applications: Small household appliances, internal electrical components, automotive door panel inner frames…
ABSPA-717CKChi Mei (Zhenjiang)PolylacGeneral Grade. High impact strength.Kitchenware, audio equipment, toilet seats, washing machines, vacuum cleaner housings, tool handles and accessories, etc.
ABSPA-707KChi Mei (Zhenjiang)PolylacGeneral Grade. High gloss, high rigidity, excellent flexural strength.Telephone housings, lamp holders, toys, office supplies, clock casings, small household appliances, etc.
ABSPA-757KChi Mei (Zhenjiang)PolylacGeneral Grade. High rigidity, high gloss, medium impact strength.TV front bezels, photocopier housings, telephone casings, cosmetic containers, wheel covers, etc.
ABSPA-749KChi Mei (Zhenjiang)PolylacGeneral Grade. Ultra-high impact strength.Safety helmets, motorcycle fenders, shoe heels, snow sports equipment, water filter housings, etc.
ABSD-180Chi Mei (Zhenjiang)PolylacGeneral Grade. High rigidity, high gloss, medium impact strength.TV front bezels, photocopier housings, telephone casings, cosmetic containers, wheel covers, etc.
ABSD-190Chi Mei (Zhenjiang)PolylacGeneral Purpose Grade. High gloss, high rigidity, excellent flexural strength.Telephone housings, lamp holders, toys, office supplies, clock casings, small home appliances, etc.
ABSPA-749SKChi Mei (Zhenjiang)PolylacExtrusion Grade. High impact strength; suitable for both extrusion and injection molding.Tubing, luggage, helmets, refrigerator components, etc.
ABSD-120Chi Mei (Zhenjiang)PolylacExtrusion Grade. High impact strength; suitable for both extrusion and injection molding.Tubing, luggage, helmets, refrigerator components, etc.
ABSD-1000Chi Mei (Zhenjiang)PolylacFlame Retardant Grade. Standard flow; 1.5mm V-0, 2.5mm 5VB, 3.0mm 5VA (TBBA-based).Set-top boxes, power switch panels, power sockets, car batteries, cash register housings, light boxes, DVD players, car audio control panels, etc.
ABSD-1200Chi Mei (Zhenjiang)PolylacFlame Retardant Grade. Standard flow; 1.5mm V-2, 2.5mm V-0, 2.5mm 5VB, 3.0mm 5VA (TBBA-based).Set-top boxes, power switch panels, power sockets, car batteries, cash register housings, light boxes, DVD players, car audio control panels, etc.
ABSD-1400Chi Mei (Zhenjiang)PolylacFlame Retardant Grade: 3.0mm V0 (TBBA Series)Set-top boxes, power switch panels, power outlets, car batteries, cash register housings, light boxes, DVD players, car audio control panels, etc.
ABSD-2200Chi Mei (Zhenjiang)PolylacHeat-Resistant Grade: High Impact StrengthAutomotive-related products, electronics, electrical appliances, etc.
ABSD-2400Chi Mei (Zhenjiang)PolylacHigh Heat-Resistant GradeAutomotive-related products, electronics, electrical appliances, etc.
ABSPA-757KFChi Mei (Zhenjiang)PolylacLow Residual Monomer Grade: Food Contact Compliant (Passed GB4806); Low Residual Monomer ContentFood containers, small household appliances.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.