Covestro Flame Retardant PC Resin

  • Home /
  • Covestro Flame Retardant PC Resin

Covestro Makrolon® FR PC Full Grade Portfolio

Covestro Makrolon® FR PC resin delivers 27+ datasheet-matched grades covering V-0 at 0.75–6.0 mm, 5VA at 3.0 mm, transparent/translucent/opaque colors, UV-stabilized variants, 10–20% glass-fiber reinforcement, and ISCC PLUS bio-circular options. Suke Plastics supplies the full portfolio with ISO TDS, SDS, and UL Yellow Card verification support.

🔹 Light Diffusion FR, UV-Stabilized (Injection/Extrusion)
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
DQ5922 FRLow diffusionV-0 @0.8mm; 5VA @3.0mm5.0121°CIzod 9CYes
DQ5942 FRMedium diffusionV-0 @0.8mm; 5VA @3.0mm5.0120°CIzod 7CYes
DQ5962 FRHigh diffusionV-0 @0.8mm; 5VA @3.0mm5.0123°CIzod 12CYes
🔹 Transparent / Translucent FR (Medium & Low Viscosity)
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
2467Low viscosity; UVV-2 @0.75mm; V-0 @6.4mm19124°CCharpy 65P(C); Izod 60PYes
2865Medium viscosityV-2 @0.75mm; V-0 @6.0mm10125°CCharpy 75P; Izod 65PNo
6455Medium viscosityV-2 @1.5mm; V-0 @3.0mm12124°CCharpy 70P; Izod 65PNo
6457Medium viscosity; UVV-2 @1.5mm; V-0 @3.0mm12123°CCharpy 70P(C); Izod 65PYes
6555Medium viscosityV-0 @3.0mm; V-2 @1.0mm10125°CCharpy 70P; Izod 65PNo
6557Medium viscosity; UVV-2 @1.5mm; V-0 @3.0mm10124°CCharpy 70P(C); Izod 65PYes
6717High viscosity, branched; UVV-0 @2.0mm3.0127°CCharpy 70P; Izod 60PYes
🔹 Opaque 5VA Medium Viscosity (E/E Housings)
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
6485Medium viscosity; 5VAV-0 @1.5mm; 5VA @3.0mm9.0124°CCharpy 70P(C); Izod 65P(C)No
6487Medium viscosity; 5VA; UVV-0 @1.5mm; 5VA @3.0mm9.0122°CCharpy 70P(C); Izod 70P(C)Yes
🔹 Opaque Low Viscosity (Fast-Flow Connectors)
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
6265 XLow viscosityV-0 @1.5mm19124°CCharpy 65P(C); Izod 50P(C)No
6267 XLow viscosity; UVV-0 @1.5mm19122°CCharpy 60P(C); Izod 15P(C)Yes
FR6002Low viscosity; WT/GY/BKV-0 @0.75/1.5/3.0mm18124°CIzod 15P(C)No
🔹 Glass-Fiber Reinforced FR (Structural Opaque)
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
GF900210% GF; low viscosityV-0 @1.2mm; V-1 @0.75mm15132°CCharpy 8CNo
912520% GF; medium viscosityV-0 @1.5mm; V-2 @0.36mm8.0138°CCharpy 8C; Izod 8CNo
941510% GF; high viscosity; 5VAV-0 @1.5mm; 5VA @3.0mm6.0136°CCharpy 10C; Izod 10CNo
941710% GF; UV; 5VAV-0 @1.5mm; 5VA @3.0mm6.0135°CCharpy 10C; Izod 10CYes
942520% GF; high viscosity; 5VAV-0 @1.5mm; 5VA @3.0mm5.0138°CCharpy 8C; Izod 8CNo
🔹 Bio-Circular (ISCC PLUS) & RE CQ Grades
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
6265 X RE25 CQBio-circular; low viscosityV-0 @1.5mm19124°CCharpy 65P(C); Izod 50P(C)No
6265 X RE CQBio-circular; low viscosityV-0 @1.5mm19124°CCharpy 65P(C); Izod 50P(C)No
6267 X RE CQBio-circular; low viscosity; UVV-0 @1.5mm19122°CCharpy 60P(C); Izod 15P(C)Yes
6487 REBio-circular; 5VA; UVV-0 @1.5mm; 5VA @3.0mm9.0122°CCharpy 70P(C); Izod 70P(C)Yes
6555 RE CQRE CQ; medium viscosityV-0 @3.0mm; V-2 @1.0mm10125°CCharpy 70P; Izod 65PN/A
🔹 Extrusion FR Sheet & Special E/E
GradePositioningUL94 (ISO TDS)MVRHDT (1.80 MPa)Notched ImpactUV
1804Extrusion; high viscosity; sheetV-2 @1.5mm; V-0 @6.0mm6.0127°CCharpy 80P; Izod 70PYes
FR7087Medium viscosity; UV; E/EV-2 @1.5mm; V-0 @2.2mm; 5VA @3.0mm12106°CIzod 8C; 8C @-30°CYes

Send Us a Message