TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PC1260CovestroMakrolonImpact modified grades / Low viscosity. MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy releaseInjection molding
PC2205CovestroMakrolonGeneral purpose grades.MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding
PC2207CovestroMakrolonGeneral purpose grades / Low viscosity. MVR (300 °C/1.2 kg) 35 cm³/10 min; low viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colorsInjection molding
PC2407CovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colorsInjection molding
PC2605CovestroMakrolonGeneral purpose grades / Medium viscosity. MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding
PC2805CovestroMakrolonGeneral purpose grades. MVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding
PC9425CovestroMakrolon20 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; easy release; available in opaque colors onlyExtrusion; Injection molding
PCAG2677CovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent colors onlyInjection molding; Automotive glazing; Roof modules
PCAL2447CovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colorsInjection molding; Automotive lighting; Headlamp lenses for automotive forward lighting
PCAL2647CovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colorsInjection molding; Automotive lighting; Headlamp lenses for automotive forward lighting
PCAX2677CovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; UV stabilized; available in black colors onlyInjection molding; Automotive exterior roof trim + pillar appliques; High-gloss surfaces with highest requirements; For the use in combination with hard coatings
PCLED2045CovestroMakrolonMVR (250 °C/2.16 kg) 17 cm³/10 min; PC with highest transmission; low viscosity; easy release;available in color code 000000 onlyInjection molding; Light guides
PCLED2245CovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; PC with highest transmission; low viscosity; easy releaseInjection molding; Light guides; optics and lenses
PC2205 RECovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding; General purpose
PC2405 RECovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding; General purpose
PC2407 RECovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colorsInjection molding; General purpose
PC2807 RECovestroMakrolonMVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colorsInjection molding; General purpose
PCAG2677 RECovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent colors only. CQ renewable attributed, Optical qualityInjection molding; Automotive glazing; Roof modules
PCAL2447 RECovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors. CQ renewable attributed, Optical qualityInjection molding; Automotive lighting; Headlamp lenses for automotive forward lighting
PCAX2675 RECovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; available in black colors onlyInjection molding; Automotive exterior roof trim + pillar appliques; High-gloss surfaces with highest requirements; for the use in combination with hard coatings
PCDQ5922 FRCovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; low diffusion; UV stabilizedExtrusion; Injection molding; Light diffusion
PCDQ5942 FRCovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; medium diffusion; UV stabilizedExtrusion; Injection molding; Light diffusion
PCDQ5962 FRCovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; high diffusion; UV stabilizedExtrusion; Injection molding; Light diffusion
PCLED2245 ELCovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy releaseInjection molding; Edge lighting material for light guides and optical parts
PCRW2407 RECovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; UV stabilized; variable content of filler for high reflectance application; CQ renewable attributedAutomotive,Electronics, appliances & telecommunications
PC2407 RE25 CQCovestroMakrolonUV stable, CQ renewable attributed, TransparentAutomotive,Electronics, appliances & telecommunications
PC2805 RE CQCovestroMakrolonCQ renewable attributed, TransparentAutomotive,Electronics, appliances & telecommunications
PCAL2447 RP70 CQCovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; melt temperature 280 – 320 °C; available in clear transparent colors and in various signal colors.automotive lighting; headlamp lenses for automotive forward lighting
PCAL2647 RE CQCovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colorsInjection molding; Automotive lighting; Headlamp lenses for automotive forward lighting
PCAL2647 RP70 CQCovestroMakrolonCQ recycled attributed, UV stable, Transparent, Optical qualityheadlamp lenses for automotive forward lighting
PCLED2245 HP RECovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; high color stability under injection molding conditions; PC with highest transmission; low viscosity; easy releaseInjection molding; Light guides; Optics and lenses
PC2456CovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding; Food contact quality
PC2467CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UL 94V-2/1.5 mm and 3.0 mm; UV stabilized; easy release; available in transparent, translucent and opaque colorsElectronics, appliances & telecommunications
PC2656CovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colors;Food-contact-compliantInjection molding; Food contact quality
PC2856CovestroMakrolonMVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colors. Food-contact-compliant.Injection molding; Food contact quality
PC2865CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 10 cm³/10 min; UL 94V-2/1.5 mm and 3.0 mm; medium viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding
PC3105CovestroMakrolonMVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding; General purpose
PC6455CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 12 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding
PC6457CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 12 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; UV stabilized; easy release; available in transparent and opaque colorsInjection molding
PC6485CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 9.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; medium viscosity; easy release; available in opaque colors onlyInjection molding
PC6487CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 9.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; medium viscosity; UV stabilized; easy release; available in opaque colors onlyInjection molding
PC6555CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 10 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding
PC6557CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 10 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors.Injection molding
PC6717CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 3.0 cm³/10 min; V-0 at 2.0 mm (UL 94); high viscosity; branched; UV stabilized; easy release; available in transparent, translucent and opaque colors 
PC8025CovestroMakrolon20 % glass fiber reinforced; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; milled fiber; high viscosity; easy release; available in opaque colors only;Dimensionally stableExtrusion; Injection molding; Precision parts
PC8325CovestroMakrolon20 % glass fiber reinforced; MVR (300 °C/1.2 kg) 4.0 cm³/10 min; high viscosity; easy release; available in opaque colors only; Dimensionally stableExtrusion; Injection molding
PC9125CovestroMakrolon20 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 8.0 cm³/10 min; UL 94V-0/1.5 mm; medium viscosity; easy release; available in opaque colors only; Dimensionally stable.Injection molding
PC9415CovestroMakrolon10 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; easy release; available in opaque colors only; Dimensionally stable.Injection molding
PC9417CovestroMakrolon10 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; UV stabilized; easy release; available in opaque colors onlyInjection Molding
PCET3113CovestroMakrolonMVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; UV stabilized; available in transparent colors only; Impact resistant.Extrusion;Solid sheet; Corrugated sheet
PCFR6002CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 18 cm³/10 min; low viscosity; easy releaseInjection molding
PCFR7087CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 12 cm³/10 min; UL 94V-0/2.2 mm and 5VA/3.0 mm; medium viscosity; UV stabilized; easy release; available in transparent and translucent colorsInjection molding; Electrical/electronic
PCGF9002CovestroMakrolon10 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 15 cm³/10 min; UL 94V-0/1.2 mm; low viscosity; easy release; available in opaque colors onlyInjection molding; Electrical/electronic; Housing parts with low wall thickness
PCXT5010CovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; easy processing; low viscosity; easy release; Vicat softening temperature 50 N, 50 °C/h = 110 °C; available in transparent colors onlyInjection molding; LCD TV frame
PC6265 XCovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; UL 94V-0/1.5 mm; low viscosity; easy release; available in opaque colors onlyInjection molding
PC6267 XCovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; UL 94V-0/1.5 mm; low viscosity; UV stabilized; easy release; available in opaque colors onlyInjection molding
PC6487 RECovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 9.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; medium viscosity; UV stabilized; easy release; available in opaque colors onlyInjection molding
PC6557 RECovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors; Food-contact-compliant, CQ renewable attributedInjection molding; Food contact quality
PC2456 RE CQCovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colorsInjection molding; Food contact quality
PC2856 RE CQCovestroMakrolonMVR (300 °C/1.2 kg) 9.0 cm³/10 min; food contact quality; medium viscosity; easy release; melt temperature 280 – 320 °C; available in transparent, translucent and opaque colorinjection molding
PC6555 RE CQCovestroMakrolonMVR (300 °C/1.2 kg) 10 cm³/10 min; flame retardant; UL 94V-0/3.0 mm; medium viscosity; easy release; melt temperature 280 – 320 °C; available in transparent, translucent and opaque colorsinjection molding
PC6265 X RE25 CQCovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; flame retardant; UL 94V-0/1.5 mm; low viscosity; easy release; melt temperature 280 – 320 °C; available in opaque colors onlyinjection molding
PC6265 X RE CQCovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; flame retardant; UL 94V-0/1.5 mm; low viscosity; easy release; melt temperature 280 – 320 °C; available in opaque colors onlyInjection molding
PC6267 X RE CQCovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; flame retardant; UL 94V-0/1.5 mm; low viscosity; UV stabilized; easy release; injection molding – melt temperature 280 – 320 °C; available in opaque colors onlyInjection molding
PC2258CovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colorsInjection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C
PC2558CovestroMakrolonMVR (300 °C/1.2 kg) 14 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors; Medical.Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C
PC2658CovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors; Medical.Injection molding; Medical devices; suitable for ETO and steam sterilization at 121 °C
PC3158CovestroMakrolonMVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colorsInjection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C
PCRx1452CovestroMakrolonMVR (300 °C/1.2 kg) 16 cm³/10 min; low viscosity; easy release; Medical, TransparentInjection molding; Medical devices
PCRx1805CovestroMakrolonMVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; high lipid resistance; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirementsInjection molding; Medical devices; Transparent parts for medical devices
PCRx1851CovestroMakrolonMVR (300 °C/1.2 kg) 23 cm³/10 min; low viscosity; easy release; Medical, TransparentInjection molding; Medical devices
PCRx2530CovestroMakrolonMVR (300 °C/1.2 kg) 15 cm³/10 min; medium viscosity; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements; Medical, Transparent.Injection molding; Medical devices; Transparent parts for medical devices.
PC2258 RECovestroMakrolonMVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colorsInjection molding; Medical devices; suitable for ETO and steam sterilization at 121 °C
PC2458 RECovestroMakrolonMVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors.Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C
PC2658 RECovestroMakrolonMVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors. CQ renewable attributed.Injection molding; Medical devices; suitable for ETO and steam sterilization at 121 °C
PC2858 RECovestroMakrolonMVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colorsInjection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C
PCRx1805 RECovestroMakrolonMVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; high lipid resistance; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirementsInjection molding; Medical devices; Transparent parts for medical devices
PCRx2530 RECovestroMakrolonMVR (300 °C/1.2 kg) 15 cm³/10 min; medium viscosity; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements; Medical, CQ renewable attributedInjection molding; Medical devices; Transparent parts for medical devices
PC1804CovestroMakrolonflame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-2/1.5 mm and 3.0 mm; high viscosity; UV stabilized; optimized for low plate-out; TransparentExtrusion; Solid sheet; Aircraft construction; Automotive construction; Railway construction
PC1603CovestroApecHeat Resistant Grade. MVR (330°C/2.16 kg) 25 cm³/10 min; high viscosity; UV stabilized; softening temperature (VST/B 120) = 159 °CInjection molding
PC1695CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330°C/2.16 kg) 45 cm³/10 min; easy release; softening temperature (VST/B 120) = 158°CInjection molding; Covers for brake lights and indicator lights; Headlamp reflectors/bezels
PC1745CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 17 cm³/10 min; easy release; for superheated steam sterilization up to 143 °C; meets criteria of US Pharmacopeia (USP) Class VI; biocompatible according to many ISO 10993-1 test requirements; softening temperature (VST/B 120) = 170 °CInjection molding; Films for medical packaging; Contact lens holders; Medical vessels; Safety valve for respiration aids; Syringe tops
PC1795CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 30 cm³/10 min; easy release; low viscosity; softening temperature (VST/B 120) = 173°CInjection molding; Covers for brake lights and indicator lights; Headlamp reflectors/bezels
PC1803CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 10 cm³/10 min; high viscosity; UV stabilized; softening temperature (VST/B 120) = 184 °CInjection molding; Covers for brake lights and indicator lights; Car interior light covers; Domestic lamp covers; Headlamp lenses; Covers for ships’ lights; Connector pieces for halogen systems
PC1895CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 18 cm³/10 min; easy release; softening temperature (VST/B 120) = 183°CInjection molding; Covers for brake lights and indicator lights; Recessed light fixtures/reflectors; Raised brake lights; Headlamp reflectors/bezels
PC1897CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 18 cm³/10 min; easy release; UV stabilized; softening temperature (VST/B 120) = 182 °CInjection molding; Lamp covers; Headlamp lenses
PC2095CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 8 cm³/10 min; high viscosity; easy release; softening temperature (VST/B 120) = 203 °CInjection molding; Covers for brake lights and indicator lights; Recessed light fixtures/reflectors; Blade-type fuses; Headlamp reflectors/bezels
PC2097CovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 8 cm³/10 min; high viscosity; easy release; UV stabilized; softening temperature (VST/B 120) = 202 °CInjection molding; Lamp covers; Headlamp lenses
PCFR1897CovestroApecHeat Resistant Grade. Copolycarbonate; flame retardant, MVR (330°C/2.16 kg) 18 cm³/10 min; low viscosity; easy release; UV stabilized (fulfills the requirements according to EN 170); V-2/1.5mm (UL 94); V-0/3.0mm (UL 94); softening temperature (VST/B 120) = 182°C; available in transparent and opaque colorsInjection molding; Visors for firemen’s helmets
PC1745 RECovestroApecHeat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 17 cm³/10 min; easy release; for superheated steam sterilization up to 143 °C; meets criteria of US Pharmacopeia (USP) Class VI; biocompatible according to many ISO 10993-1 test requirements; softening temperature (VST/B 120) = 170 °C; Medical, CQ renewable attributedInjection molding; Films for medical packaging; Contact lens holders; Medical vessels; Safety valve for respiration aids; Syringe tops

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.