CYCOLOY™ resin PC/ABS blend delivers a balance of impact strength, aesthetic appeal, and low-temperature performance. With excellent moldability and heat resistance, CYCOLOY resin is used in automotive interiors, UL-certified electrical and electronic components, consumer electronics, industrial equipment covers and housings, home appliances, EV charging equipment, and select medical device enclosures.

pc abs resin alloy plastic

CYCOLOY™ PC/ABS for bulk purchase

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
FR PC/ABS AlloyC2800SabicCYCOLOYStandard grade, non-chlorinated/brominated flame retardant, UL V0 & 5VB.Business equipment, monitors, and enclosures.
FR PC/ABS AlloyC2950SabicCYCOLOYHigh heat grade, non-chlorinated/brominated flame retardant, UL V0 & 5VB.Appliances, lighting, and electrical components.
FR PC/ABS AlloyC2950HFSabicCYCOLOYHigh heat grade with improved processability, UL V0 & 5VA/B.Appliances, lighting, and electrical components.
FR PC/ABS AlloyC2951SabicCYCOLOYHigh heat, non-chlorinated/brominated, UL 94 5VA@3.0mm.Demanding electrical applications.
FR PC/ABS AlloyC3650SabicCYCOLOYGeneral purpose, flame retardant, UL V0 & 5VB, suitable for injection molding or sheet forming.Cable channels, meets DIN VDE 0472/815 halogen-free standards.
FR PC/ABS AlloyC6200SabicCYCOLOYBalanced heat, flow, and impact performance, non-chlorinated/brominated flame retardant.Various application needs.
FR PC/ABS AlloyC6600SabicCYCOLOYFlame retardant, balanced flow, impact, hydrolytic stability, UL 94 V0@1.5mm, 5VB@2.0mm.Good chemical resistance, suitable for opaque colors.
FR PC/ABS AlloyC7230PSabicCYCOLOYMineral-filled, flame retardant, good rigidity with balanced flow and impact.Various electrical and industrial applications.
FR PC/ABS AlloyC9210SabicCYCOLOYImpact modified, heat resistant, non-chlorinated/brominated, UL 94 V0.Wide variety of large-sized applications.
FR PC/ABS AlloyCE3510SabicCYCOLOYHigh impact, flame retardant, UL 94 V0@1.5mm, suitable for injection molding and extrusion.Applications without chlorine/bromine.
FR PC/ABS AlloyCM6140SabicCYCOLOYMineral-filled, high modulus, low warpage, UL 94 V0@0.8mm, 5VB@1.5mm.Thin wall applications.
FR PC/ABS AlloyCM6210SabicCYCOLOYHigh impact, mineral-filled, UL 94 V0@1.5mm.Wide range of electrical applications.
FR PC/ABS AlloyCM6220SabicCYCOLOYHigh modulus (6GPa), low warpage, flame resistant for thin walls.Electrical housings and thin wall components.
FR PC/ABS AlloyCM6240SabicCYCOLOYHigh modulus, low warpage, UL 94 V0@0.8mm, 5VB@1.5mm.Thin wall applications.
FR PC/ABS AlloyCY5025SabicCYCOLOYGeneral-purpose thin wall flame retardant, UL V0 & 5VB.Thin wall applications.
FR PC/ABS AlloyCY6025SabicCYCOLOYStandard thin wall flame retardant, UL V0 & 5VB.Thin wall injection molding applications.
FR PC/ABS AlloyCY6110SabicCYCOLOYImpact modified, high flow, UL 94 V0@1.5mm, 5VB@2.5mm.Used extensively in thin wall and large-size components.
FR PC/ABS AlloyCY6120SabicCYCOLOYGood flame retardancy, flow properties, UL 94 V0@1.2mm.Thin wall applications.
FR PC/ABS AlloyCY6310SabicCYCOLOYHigh flow, heat resistant, UL 94 V0@1.5mm, 5VA@2.9mm, 5VB@2.3mm.Large-sized applications.
FR PC/ABS AlloyCY6414SabicCYCOLOYMedium flow, high heat, UL 94 V0@1.2mm, 5VB@2.5mm.Injection molding applications.
PC/ABS AlloyC1200HFSabicCYCOLOYExcellent flow, impact, low-temperature ductility, high heat resistance.General-purpose applications.
PC/ABS AlloyC4210HFSabicCYCOLOY10% glass-filled, high flow, high heat resistance, good strength.Structural applications requiring rigidity.
PC/ABS AlloyC4220SabicCYCOLOY20% glass-filled, excellent heat resistance and strength.High-rigidity applications.
PC/ABS AlloyCM8622SabicCYCOLOYHigh heat, low thermal expansion, good modulus and appearance.Electrical and appearance-focused applications.
PC/ABS AlloyCM8823SabicCYCOLOYHigh heat, low thermal expansion, good modulus and aesthetics.Electrical and appearance-focused applications.
PC/ABS AlloyCP8320SabicCYCOLOYMedium heat, suitable for electroplating.Automotive plating applications.
PC/ABS AlloyCY8630SabicCYCOLOYHeat-resistant PC/ABS for automotive.Automotive applications.
PC/ABS AlloyHC1104HFSabicCYCOLOYHigh heat resistance, excellent flow and impact performance.General heat and impact-resistant applications.
PC/ABS AlloyHC1204HFSabicCYCOLOYHigh heat resistance, biocompatible for medical and pharmaceutical use.Medical devices, pharmaceutical applications.
PC/ABS AlloyLG9000SabicCYCOLOYLow gloss PC/ABS.Automotive interiors or low gloss applications.
PC/ABS AlloyMC1300SabicCYCOLOYHigh impact, excellent flow, plating and painting capable.Plating and painting applications.
PC/ABS AlloyMC8002SabicCYCOLOYLow viscosity, high toughness.General-purpose injection molding.
PC/ABS AlloyMC8100SabicCYCOLOYExtrusion and blow molding grade.Extrusion and blow molding applications.
PC/ABS AlloyMC8800SabicCYCOLOYHigh heat, high impact, low thermal expansion.Structural applications with high heat requirements.
PC/ABS AlloyXCM830SabicCYCOLOY8% talc-filled, high stiffness and impact performance.Applications requiring rigidity and impact resistance.
PC/ABS AlloyXCY620HFSabicCYCOLOYHigh flow and high heat resistance.Electrical components.
PC/ABS AlloyXCY620SabicCYCOLOYExcellent hydrolytic stability.Electrical components and general requirements.
PC/ABS AlloyXCY620SSabicCYCOLOYStandard black and natural colors, excellent hydrolytic stability.Electrical components.
PC/ABS AlloyXCY630SabicCYCOLOYHigh hydrolytic stability.Electrical components.