FCFC Flame Retardant PC Resin

  • Home /
  • FCFC Flame Retardant PC Resin

FORMOSA (FCFC) Flame Resistant PC Collection

FCFC TAIRILITE® flame retardant PC resin covers 13 halogen-free grades across 3 series: Universal FR baseline (V-0 at 1.5–3.0mm), UL 746C f1 outdoor UV opaque, and transparent FR with >87% light transmission. Non-halogen phosphorus-based FR. Fits electronics housings, EV charging, LED fixtures, sheet extrusion.

🔹 Universal FR Baseline (Opaque, Halogen-Free)

GradeCore PositioningUL94 Multi-Thickness RatingAppearanceKey Property SnapshotUV / f1Key FeatureRecommended Applications
AC3710High-flow FR baseline, thin-wall injection1.5 V-0OpaqueHigh MFI, halogen-free FR—Easy filling for thin-wall housingsConsumer electronics covers, adapter housings
AC3610-AFStandard FR injection, halogen-free1.5 V-0OpaqueTensile 51 MPa, FM 3330 MPa—Rigid FR for structural partsBusiness machine housings, printer frames
AC3600FR injection baseline, mid-flow1.5 V-0OpaqueHalogen-free phosphorus FR—Balanced flow + flame resistanceBattery housings, small appliance parts
AC3900V-0 benchmark, mid-flow1.5 V-0 / 3.0 V-0OpaqueDTUL 124°C, Vicat 146°C—Multi-thickness V-0 reliabilityStandard electrical enclosures, connectors

 

🔹 Outdoor UV & UL 746C f1 (Opaque + Low-Temp Impact)

GradeCore PositioningUL94 Multi-Thickness RatingAppearanceKey Property SnapshotUV / f1Key FeatureRecommended Applications
AC3630Weather-resistant FR opaque1.5 V-0OpaqueUV stabilized, halogen-free✅ UVOutdoor UV durabilityOutdoor electrical boxes, utility covers
AC3830Outdoor opaque, f1 certified1.5 V-0OpaqueUL E162823 listed✅ UL 746C f1Outdoor UV + water-exposure certifiedEV charging stations, outdoor terminals
AC3839Outdoor opaque, injection & extrusion1.5 V-0OpaqueSoftening 130°C, SG 1.18–1.20✅ UL 746C f1Dual-process compatibilityOutdoor equipment housings, meter boxes
AC9830Low-temp impact FR flagship1.5 V-0 / 3.0 5VAOpaqueIzod 687 J/m @23°C, 392 J/m @-40°C ⭐✅ UL 746C f1-40°C impact 392 J/m, DTUL 122°CCold-climate outdoor equipment, northern EV chargers

 

🔹 Transparent FR + UV + UL 746C f1 (Halogen-Free)

GradeCore PositioningUL94 Multi-Thickness RatingAppearanceKey Property SnapshotUV / f1Key FeatureRecommended Applications
AC3843Transparent FR, mid-low flow3.0 V-0TransparentTrans >87%, Haze <1, MFI 12✅ UL 746C f1High clarity + halogen-free FRTransparent housings, light guides
AC3853Transparent FR, mid-low flow2.5 V-0 / 3.0 V-0TransparentHalogen-free phosphorus FR✅ UL 746C f1Multi-thickness transparent V-0Lamp lenses, display covers
AC3854Transparent FR, higher flow3.0 V-0TransparentMFI 13, Trans 88%, Haze 2%✅ UL 746C f1Easier filling for thin transparent partsThin-wall transparent covers, light panels
AC3832Transparent FR, low flow (sheet)3.0 V-0TransparentLow flow, high molecular weight✅ UVSheet extrusion + injection dual-useFR transparent sheets, safety glazing
AC3873Transparent FR, low flow (sheet)3.0 V-0TransparentLow flow, halogen-free✅ UVExtrusion-grade transparent FRFR glazing sheets, machine guards