TAIRILAC® ABS resins feature a balanced combination of impact strength, rigidity, and surface finish. Known for their excellent mechanical and thermal properties, they are widely used in automotive interiors, electronics housings, home appliances, and consumer products requiring durability and aesthetics.

pc abs resin alloy plastic

Tairilac® ABS available for bulk buy

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
ABSAG15A1-HFormosa (FCFC)TairilacGeneral Purpose Grade. High gloss,Medium impactToys, Caculators, Phone, Clock housing, Stereo housing, Suitcase
ABSANC160Formosa (FCFC)TairilacSelf Extinguishing Grade. Flame retardantFlame retardant materials;Housing of LCD monitor, LCD-TVcomputers & OA machine
ABSAG12A0Formosa (FCFC)TairilacGeneral Purpose Grade. Super high impactHelmets, Shoe heels, Pipe fittings, Products of low-temp usage
ABSAG12A3Formosa (FCFC)TairilacGeneral Purpose Grade. High impactShoe heels, Toys, Clock housing, Stereo housing, Suitcase, The plate-like products
ABSAG15A3Formosa (FCFC)TairilacGeneral Purpose Grade. High gloss, Medium impactToys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
ABSAG15E3Formosa (FCFC)TairilacGeneral Purpose Grade. High gloss, High rigidToys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
ABSAG15E1Formosa (FCFC)TairilacGeneral Purpose Grade. High gloss, High rigidToys, Calculators, Phone,Clock housing,Stereo housing, Suitcase
ABSAG100HFormosa (FCFC)TairilacGeneral Purpose Grade. Super high impactHelmets, Shoe heels, Pipe fittings, Products of low-temp usage
ABSAF3500Formosa (FCFC)TairilacHigh Flow Grade. High impactHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAF3560Formosa (FCFC)TairilacHigh Flow Grade. High impactHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAF3530Formosa (FCFC)TairilacHigh Flow Grade. High impact, Chemical resistantHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAF3535Formosa (FCFC)TairilacHigh Flow Grade. High impactHousing of stereos, Large toys, Chairs, Motorcycles, OA machines
ABSAX4000Formosa (FCFC)TairilacHeat Resistant Grade. Medium high heatParts of cars, Electrical appliances, Hair dryer, Heat resistant parts
ABSAX4300Formosa (FCFC)TairilacHeat Resistant Grade. Medium high heat, Extrusion blow moldingParts of cars, Electrical appliances, Hair dryer, Heat resistant parts
ABSANC100Formosa (FCFC)TairilacHeat Resistant Grade, Flame retardantFlame retardant materials;Housing of LCD monitor, LCD-TV,computers & OA machine
ABSAG23ATFormosa (FCFC)TairilacElectroplating Grade (Mental Plating Grade). High impactWheel cover, Knobs, Tags,Door handle, Plating products
ABSAG10APFormosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products,Crash helmets,Pipes, Shoe heels
ABSAE8000Formosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products,Crash helmets,Pipes, Shoe heels
ABSAG10NPFormosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products,Crash helmets,Pipes, Shoe heels
ABSAE8700Formosa (FCFC)TairilacExtrusion Grade. Extrusion molding, Super high impact, High rigidExtrusion products, Crash helmet, Pipes, Shoe heels
ABSANC120Formosa (FCFC)TairilacSelf Extinguishing Grade. Flame retardantFlame retardant materials;Housing of LCD monitor, LCD-TVcomputers & OA machine
ABSAE10EPFormosa (FCFC)TairilacExtrusion Grade (Jet Black Extrusion Grade). Extrusion molding, Super high impact, High rigidPipes
ABSAX4100Formosa (FCFC)TairilacHeat Resistant Grade. Super high heatParts of cars, Electrical appliances, Hair dryer, Heat resistant parts
ABSAG16A1Formosa (FCFC)TairilacHealth Care Grade. High rigid, Medium impactScalpel shank, Asthma inhaler Meets the requirements of USP Plastic Class VI
ABSAG20GFFormosa (FCFC)Tairilac“20%GF Reinforced Grade. Dimensional stability, High heat resistantPrinter parts