Formosa TAIRILITE® PC Resin

  • Home /
  • FCFC TAIRILITE® PC Resin

Tairilite® PC Plastic Granules

TAIRILITE® Polycarbonate (PC) resins, developed by Formosa Chemicals & Fibre Corporation (FCFC), is a premium-grade polycarbonate material known for its outstanding impact strength, optical clarity, and thermal resistance. Designed to meet the needs of demanding industries, TAIRILITE® PC delivers consistent quality, reliable performance, and excellent processability across a wide range of applications.

polycarbonate pc resin

Tairilite® PC available for bulk purchase

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PCAC3710FORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. Halogen free, Flame retardant, High flow, Non-transparencyHousehold appliances, 3C electronic product casings Thin-walled electrical equipment housing such as laptop battery casings, internal components of energy storage devices
PCAC3900FORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. Halogen free, Flame retardant, White color, Non-transparency, High gloss reflectionHome lighting, electronics touch panel module internal accessories such as LED lamp cap, lamp holder, panel white frame
PCAC3610-AFFORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. High flow, Non-transparency, Cl, Br, Sb free, Flame retardantTransformer case, Battery case, Projector housing, Electroomechanical appliance cover
PCAC3600FORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. Halogen free, Flame retardant, High heat resistance, Non-transparencyAdapters, transformers, chargers, batteries, routers casings
PCAC3830FORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. Light diffusion, Mid flow, UV resistance, Halogen freeDiffusion board, Diffusion lamp, Diffusion injection lampshade, Diffusion injection-blow bulb
PCAC3839FORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. Charging shell, battery shell, router shellMid flow, Flame retardant, Low temperature impact property, UV resistance,
PCAC3630FORMOSA (FCFC)TAIRILITESelf Extinguishing Grade. Halogen free, Flame retardant, High flow, Non-transparency,UL weather resistance certificationHousehold appliances, 3C electronic products , outdoor equipment shell, electric bike battery case, Energy storage device
PCAC1115FORMOSA (FCFC)TAIRILITEWeather Resistant Grade. Transparency, Mid-low flow, High clean PC, Low gel.Optical applications, High transparency, PC film, PC sheet.
PCAC3843FORMOSA (FCFC)TAIRILITETransparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free.Transparent flame-retardant injection parts.
PCAC3853FORMOSA (FCFC)TAIRILITETransparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free.Transparent flame-retardant injection parts.
PCAC3854FORMOSA (FCFC)TAIRILITETransparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free.Transparent flame-retardant injection parts.
PCAC3832FORMOSA (FCFC)TAIRILITETransparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free.Transparent flame-retardant sheet and injection parts.
PCAC3873FORMOSA (FCFC)TAIRILITETransparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free.Transparent flame-retardant sheet and injection parts.
PCAC2856FORMOSA (FCFC)TAIRILITEDiffusion Grade. Light diffusion, Mid-high flow, UV resistanceDiffusion injection lampshade, Diffusion injection-blow bulb
PCAC2854FORMOSA (FCFC)TAIRILITEDiffusion Grade. Light diffusion, Mid-high flow, UV resistanceDiffusion board, Diffusion lamp (LED tube shell)
PCAC2820FORMOSA (FCFC)TAIRILITEDiffusion Grade. Light diffusion, Mid-high flow, UV resistanceAutomotive lighting applications, such as DRL, position lights, interior lights
PCAC9140FORMOSA (FCFC)TAIRILITEUltra-low Temp Resistance Copolymer. Transparency, Mid flow, UV resistance,Mobile phone / tablet / laptop / 3C products case, sports equipment / protective gear.
PCAC9144FORMOSA (FCFC)TAIRILITEUltra-low Temp Resistance Copolymer.Mid flow, Low temperature impact property, UV resistance,Mobile phone / tablet / laptop / 3C products case, sports equipment / protective gear.
PCAC9830FORMOSA (FCFC)TAIRILITEUltra-low Temp Resistance Copolymer, Mid flow, Flame retardant, UV resistance,Mobile equipment housing, Connectors, Switches, Outdoor equipment component, Battery pack.
PCAC2916FORMOSA (FCFC)TAIRILITEHigh Transparency Grade. High flowLight guide bar, Daytime running lights for car lamp, LED condenser lens.
PCAC2955FORMOSA (FCFC)TAIRILITEIR Transmittance Grade, Mid-high flowApplications in Information transfer, such as remote control, mobile phone PDA and wireless keyboard ect