FCFC TAIRIPRO® PP Resin

  • Home /
  • FCFC TAIRIPRO® PP Resin

Tairipro® PP Plastic Granules

FORMOSA TAIRIPRO® Polypropylene (PP) resins offer excellent chemical resistance, low density, and good processability. Available in homopolymer, random copolymer, and impact copolymer grades, they are widely used in packaging, automotive parts, consumer goods, and household applications.

polypropylene pp resin

Tairipro® PP available for bulk buy

TypeGrade No.ManufacturerBrandKey FeaturesTypical Applications
PP (Random Copolymer PP)K4535FORMOSA (FCFC)TairiproInjection molding grade.High fluidity, High Clarity, Anti-static, Good resistance to chemical.High transparency container, Transparency housewares, USP Class VI approved
PP (Random Copolymer PP)K4038FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, Anti-static, Good Transparency.Transparency containers,Thin wall products
PP (Random Copolymer PP)K4515FORMOSA (FCFC)TairiproInjection molding grade. High Clarity, Anti-static,Good resistance to chemical.High transparency container, Transparency housewares, USP Class VI approved
PP (Random Copolymer PP)K4650FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, High clarity, anti-static.High transparency container& housewares, meets the requirements of USP Plastic Class VI
PP (Random Copolymer PP)K4715FORMOSA (FCFC)TairiproInjection molding grade. Super High Clarity, Anti-static.Super high transparency container& housewares, meets the requirements of USP Plastic Class VI
PP (Random Copolymer PP)K4750FORMOSA (FCFC)TairiproInjection molding grade. Super High Clarity, Anti-static.Super high transparency container& housewares
PP (Random Copolymer PP)F4006FORMOSA (FCFC)TairiproFilm Grade. Good Transparency.Excellent resistance to whiteness
PP (Random Copolymer PP)F4007FORMOSA (FCFC)TairiproFilm Grade. Good Transparency.Blow Molding, USP CLASS VI Approved
PP (Random Copolymer PP)F4008FORMOSA (FCFC)TairiproFilm Grade. Good transparency,Good slippingCPP,Flexible & Rigid packaging
PP (Random Copolymer PP)T3002FORMOSA (FCFC)TairiproExtrusion Grade. Good transparency, Good resistance to chemical.Blow Molding, USP CLASS VI Approved
PP (Random Copolymer PP)T4002FORMOSA (FCFC)TairiproExtrusion Grade. Good transparency, Good resistance to chemical.Blow molding, sheet
PP (Impact Copolymer PP)K8025FORMOSA (FCFC)TairiproInjection molding grade. High impact strength, High fluidity.Automotive parts, Washing machine parts, Tool boxes,
PP (Impact Copolymer PP)K3029FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, High impact strength.Bumper, Automotive parts, Thin wall products
PP (Impact Copolymer PP)K7005AGFORMOSA (FCFC)TairiproInjection molding grade. High impact strength, High Stiffness, Good light stability.Automotive parts, Furniture,Appliances, Pallet , Crate containers
PP (Impact Copolymer PP)K7005ANFORMOSA (FCFC)TairiproInjection molding grade. High impact strength, High Stiffness.Automotive parts, Furniture,Appliances
PP (Impact Copolymer PP)K7009FORMOSA (FCFC)TairiproInjection molding grade. High stiffness,Good impact strength.Automotive parts, Furniture,Appliances
PP (Impact Copolymer PP)K7009AHFORMOSA (FCFC)TairiproInjection molding grade. Long term thermal aging, High stiffness, Good impact strength.Electric appliance parts, Automotive parts,RTI=125℃
PP (Impact Copolymer PP)K7025FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, High impact strength.Washing machine cylinder, Appliances
PP (Impact Copolymer PP)K8003FORMOSA (FCFC)TairiproInjection molding grade. Hight impact strength, Good Stiffness.Baby-car parts, Paint drum,Sport appliances, Base of Luggage
PP (Impact Copolymer PP)K8003ANFORMOSA (FCFC)TairiproInjection molding grade. Excellent impact strength, High stiffness, Excellent anti-staticPaint drum,Sport appliances, Base of Luggage
PP (Impact Copolymer PP)K8009FORMOSA (FCFC)TairiproInjection molding grade. High impact strength, Good fluidityAutomotive parts, Battery case,Electrical appliances, Furniture
PP (Impact Copolymer PP)K8050FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, Good impact strength, High Stiffness,Low warpageWashing machine,Storage boxes,Thin wall products
PP (Impact Copolymer PP)K8065FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, Good impact strength, High Stiffness,Low warpageWashing machine,Storage boxes,Thin wall products
PP (Impact Copolymer PP)K8095FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, Good impact strength, Good Stiffness.Automotive parts
PP (Impact Copolymer PP)K8802FORMOSA (FCFC)TairiproInjection molding grade. Hight impact strength,Excellent resistance to low temp. Brittleness, Good luster.Suitcase Parts
PP (Impact Copolymer PP)K9010FORMOSA (FCFC)TairiproInjection molding grade. High impact strength, Good fluidityAutomotive parts
PP (Impact Copolymer PP)K9017FORMOSA (FCFC)TairiproInjection molding grade. High impact strength, Good fluidity, Anti-UV addedAutomotive parts
PP (Impact Copolymer PP)K9030FORMOSA (FCFC)TairiproInjection molding grade. High fluidity, Hight impact strengthBumper,Automotive parts, Thin wall products
PP (Impact Copolymer PP)KP03BFORMOSA (FCFC)TairiproInjection molding grade. High fluidity, Good impact strengthAutomotive parts, Storage boxes, Thin wall products
PP (Impact Copolymer PP)B8001FORMOSA (FCFC)TairiproExtrusion grade. High impact strength, Excellent resistance to low temp. Brittleness,Good lusterPP Pipe, Thermoforming sheet, Blow molding
PP (Impact Copolymer PP)B8001A3FORMOSA (FCFC)TairiproExtrusion grade. Excellent impact strength, Excellent resistance to low temp. brittlenessPP-B pipe, Thermoforming sheet,Blow molding
PP (Impact Copolymer PP)T8002FORMOSA (FCFC)TairiproExtrusion grade. Hight impact strength, Excellent resistance to low temp. Brittleness,Good lusterCorrugated sheet, Bottles, Thermo-forming sheet
PP (Homopolymer PP)K1080FORMOSA (FCFC)TairiproInjection molding grade, Ultra high fluidity, Good stiffness, Good lusterThin wall parts, Housewares, Toys
PP (Homopolymer PP)K1108FORMOSA (FCFC)TairiproInjection molding grade, Good stiffness, Good lusterGeneral purpose, Foodcontainers, Electrical appliances, Housewares
PP (Homopolymer PP)K1525FORMOSA (FCFC)TairiproInjection molding grade, High fluidity, High Stiffness, Good luster, Good Transparencymicrowave containers, Food containers
PP (Homopolymer PP)K2051FORMOSA (FCFC)TairiproInjection molding grade, Super high fluidity, High stiffness, Good luster, Nucleating Agent, Low warpageThinner Wall Parts, Microwave containers, House wares,Toys
PP (Homopolymer PP)K1011FORMOSA (FCFC)TairiproInjection molding grade, Good stiffness, Good lusterGeneral purpose, Foodcontainers, Electrical appliances, Housewares meets the requirements of USP Plastic Class VI
PP (Homopolymer PP)K1011AGFORMOSA (FCFC)TairiproInjection molding grade, Long term heat resistance,High stiffness,Good lusterElectric appliance parts,RTI=125℃
PP (Homopolymer PP)K1023FORMOSA (FCFC)TairiproInjection molding grade, High fluidity, Good Stiffness, Good lusterThin wall parts,Housewares,Toys,meets the requirements of USP Plastic Class VI
PP (Homopolymer PP)K1035FORMOSA (FCFC)TairiproInjection molding grade,High fluidity, Good Stiffness, Good lusterThin wall parts, Housewares, Toys
PP (Homopolymer PP)S1019FORMOSA (FCFC)TairiproMulti-Filament Grade, Controlled rheology, Good softness, Anti gas fadingStaple fiber, ES fiber & PP staple fiber
PP (Homopolymer PP)S1040FORMOSA (FCFC)TairiproMulti-Filament Grade, Controlled rheology, Compact Spinning, Anti gas fadingNonwoven, Fine Denier staple fiber
PP (Homopolymer PP)F1611FORMOSA (FCFC)TairiproBlown Film Grade, High slip, Anti-blockpackaging in General
PP (Homopolymer PP)S1003FORMOSA (FCFC)TairiproFlat Yarn Grade. Good stretchabilityPortfolio, Yarn: Woven bag, Carpet, Backing, Ropes, Monofilament: Brushes, Ropes, Nettings
PP (Homopolymer PP)S1005FORMOSA (FCFC)TairiproFlat Yarn Grade. Good stretchability, Good processabilityPortfolio, Straw
PP (Homopolymer PP)S1803FORMOSA (FCFC)TairiproFlat Yarn Grade. UV, Flat yarnPortfolio, Yarn: Woven bag, Carpet, Backing, Ropes, Monofilament: Brushes, Ropes, Nettings
PP (Homopolymer PP)F2011FORMOSA (FCFC)TairiproFilm Grade. Middle slipping, Good clarityCPP usage, Flexible & Rigid packaging
PP (Homopolymer PP)F2003FORMOSA (FCFC)TairiproBOPP Grade. High stiffness, High clarityFlexible & Rigid packaging, Cigarette wraps, Adhesive tape, House wares, labels
PP (Homopolymer PP)B1101FORMOSA (FCFC)TairiproExtrusion Grade. Excellent melt strength,Deep drawingThermoforming Sheet, PP-H pipe, Tray, Blow molding
PP (Homopolymer PP)T1002FORMOSA (FCFC)TairiproExtrusion Grade. Excellent tensile strengthCorrugated sheet, Strapping, Bottles
PP (Homopolymer PP)T1202FORMOSA (FCFC)TairiproExtrusion Grade. Blow moldinghigh stiffness, heat resistance, clarity
PP (Homopolymer PP)T2502FORMOSA (FCFC)TairiproExtrusion Grade. High stiffiness, Good transparency, Good heat resistanceTransparency pressure forming sheet,Portfolio, Bottles

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.