Flame Retardant Polycarbonate
- Home /
- Flame Retardant PC Resin
Flame Retardant PC
Flame retardant PC (Polycarbonate) resin is a specialized engineering plastic modified to meet strict fire safety standards, typically achieving UL94 V-0, V-1, or V-2, 5VA, 5VB ratings. It retains the excellent mechanical strength, dimensional stability, and impact resistance of standard PC while preventing the spread of fire. Our FR PC pellets are widely used in electronic components, home appliances, and automotive interiors.
Looking for fire safety? Browse our Flame Retardant PC Resin.
Flame Resistant PC Resin Brands Collection
| Type | Grade No. | Manufacturer | Brand | UL94 Multi-Thickness (mm) | MFR / MVR (300°C/1.2kg) | Notched Izod 23°C / –30°C (kJ/m², ISO 180) | UV / UL 746C f1 |
|---|---|---|---|---|---|---|---|
| PC | PC-6600 | Chi Mei | WONDERLITE® | 1.0 V-0 / 2.0 5VB / 3.0 5VA | MFR 10 ml/10min | 60 / 15 | — / — |
| PC | PC-6600 J01 | Chi Mei | WONDERLITE® | 1.0 V-0 / 2.0 5VB / 3.0 5VA | MFR 10 ml/10min | 60 / 15 | — / — |
| PC | PC-616LS | Chi Mei | WONDERLITE® | 1.0 V-0 / 2.0 5VB / 3.0 5VA | MFR 10 ml/10min | 60 / 15 | — / ✅ UL 746C f1 |
| PC | PC-6610 | Chi Mei | WONDERLITE® | 1.5 V-0 / 3.0 V-0 + 5VA | MFR 10 ml/10min | 60 / 15 | ✅ UV / ✅ UL 746C f1 |
| PC | PC-6710 | Chi Mei | WONDERLITE® | 3.0 V-0 (+ 3.0 5VA) | MFR 10 ml/10min | 60 / 15 | ✅ UV / ✅ UL 746C f1 |
| PC | PC-681U | Chi Mei | WONDERLITE® | 1.5 V-0 / 3.0 5VA | MFR 10 ml/10min | 60 / 45 ⭐ | ✅ UV / ✅ UL 746C f1 |
| PC | PC-6600C | Zhenjiang Chi Mei | WONDERLITE® | 1.5 V-0 | MVR 9 cm³/10min | 55 / 30 @ –40°C | ✅ UV / ✅ UL 746C f1 (E194560) |
| PC | PC-6700 | Chi Mei | WONDERLITE® | 1.5 V-2 / 2.5 V-0 / 3.0 V-0 | MFR 10 ml/10min | 60 / 15 | — / — |
| PC | PC-6710NF | Chi Mei | WONDERLITE® | 3.0 V-0 (PFAS-Free, Provisional) | MFR 10 ml/10min | 60 / n/a | ✅ UV / — |
| PC | PC-6715NF | Chi Mei | WONDERLITE® | 1.5 / 2.0 / 3.0 V-0 (PFAS-Free, Provisional) | MFR 5 ml/10min | 60 / n/a | ✅ UV / — |
| PC | PC-6715VT | Chi Mei | WONDERLITE® | 1.5 V-0 / 3.0 V-0 + 5VA | MFR 6 ml/10min | 60 / 15 | ✅ UV / ✅ UL 746C f1 |
Values from Chimei ISO TDS. UL ratings are color- and thickness-dependent. Please request TDS/SDS/COA and test samples before substitution.
Substitution Checklist (Procurement Review):
Before replacing any grade, verify (1) UL94 rating at the same wall thickness, (2) UL-listed color, (3) halogen-free or PFAS-free declaration, (4) MFR / MVR, (5) notched impact at 23°C and –30°C, (6) UV / UL 746C f1 status, and (7) processing window (barrel temp / mold temp). Typical values are not specifications. Please request current TDS / SDS / COA and test samples before substitution.
| Type | Grade No. | Manufacturer | Brand | UL94 Multi-Thickness (mm) | MFR / MVR (300°C/1.2kg) | Notched Izod 23°C / –30°C | UV / UL 746C f1 |
|---|---|---|---|---|---|---|---|
| PC | AC3710 | Formosa (FCFC) | TAIRILITE® | V-1 0.45 / V-0 0.6–3.0 / 5VB 1.5–3.0 | MFR 28 g/10min | Izod 685 J/m (23°C, 3.2mm) / n/a | — / — |
| PC | AC3900 | Formosa (FCFC) | TAIRILITE® | V-0 1.5–3.0 | MFR 26 g/10min | Izod 585 J/m (23°C, 3.2mm) / n/a | — / — |
| PC | AC3610-AF | Formosa (FCFC) | TAIRILITE® | V-2 0.6 / V-1 0.8 / V-0 1.0–3.0 / 5VB 2.0–3.0 | MFR 10 g/10min | Izod 735 J/m (23°C, 3.2mm) / n/a | — / — |
| PC | AC3600 | Formosa (FCFC) | TAIRILITE® | V-2 0.6 / V-1 0.8 / V-0 1.0–3.0 / 5VB 2.0–3.0 | MFR 11 g/10min | Izod 735 J/m (23°C, 3.2mm); Charpy 65 kJ/m² / n/a | — / — |
| PC | AC3830 | Formosa (FCFC) | TAIRILITE® | V-0 1.0–3.0 / 5VA 3.0 | MFR 12 g/10min | Charpy 70 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC3839 | Formosa (FCFC) | TAIRILITE® | V-0 1.0–3.0 / 5VA 3.0 | MFR 12 g/10min | Charpy 70 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC3630 | Formosa (FCFC) | TAIRILITE® | V-0 0.8–3.0 / 5VB 1.5–3.0 | MFR 25 g/10min | Izod 635 J/m (23°C, 3.2mm); Charpy 55 kJ/m² / n/a | UL Weather Resist. / ✅ UL 746C f1 |
| PC | AC3843 | Formosa (FCFC) | TAIRILITE® | V-0 3.0–3.3 | MFR 12 g/10min | Charpy 75 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC3853 | Formosa (FCFC) | TAIRILITE® | V-0 2.5–3.0 | MFR 12 g/10min | Charpy 75 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC3854 | Formosa (FCFC) | TAIRILITE® | V-0 2.5–3.0 | MFR 12 g/10min | Charpy 70 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC3832 | Formosa (FCFC) | TAIRILITE® | V-0 1.0–3.0 / 5VA 3.0 | MFR 5 g/10min | Charpy 70 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC3873 | Formosa (FCFC) | TAIRILITE® | V-2 1.2 / V-0 1.5–3.0 | MFR 5 g/10min | Charpy 70 kJ/m² (ISO 179, 23°C) / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AC9830 | Formosa (FCFC) | TAIRILITE® | V-1 0.75 / V-0 1.5–3.0 / 5VA 3.0 | MFR 12 g/10min | Charpy 70 kJ/m² (ISO 179, 23°C); low-temp copolymer / n/a | ✅ UV / — |
Values from Formosa (FCFC) ISO TDS. Formosa TDS reports Charpy (ISO 179) or Izod J/m (ISO 180) rather than Izod kJ/m². UL ratings are color- and thickness-dependent. Please request TDS/SDS/COA before substitution.
Substitution Checklist (Procurement Review):
Before replacing any grade, verify (1) UL94 rating at the same wall thickness, (2) UL-listed color, (3) halogen-free or PFAS-free declaration, (4) MFR / MVR, (5) notched impact at 23°C and –30°C, (6) UV / UL 746C f1 status, and (7) processing window (barrel temp / mold temp). Typical values are not specifications. Please request current TDS / SDS / COA and test samples before substitution.
| Type | Grade No. | Manufacturer | Brand | UL94 Multi-Thickness (mm) | MFR / MVR (300°C/1.2kg) | Notched Izod 23°C / –30°C | UV / UL 746C f1 |
|---|---|---|---|---|---|---|---|
| PC | 9425 | Covestro | Makrolon® | V-0 1.5 / 5VA 3.0 (20% GF) | MVR 5.0 cm³/10min | n/a (not stated in TDS) / n/a | — / — |
| PC | DQ5922 FR | Covestro | Makrolon® | FR (light-diffusion, low) | MVR 5.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | DQ5942 FR | Covestro | Makrolon® | FR (light-diffusion, medium) | MVR 5.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | DQ5962 FR | Covestro | Makrolon® | FR (light-diffusion, high) | MVR 5.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 2467 | Covestro | Makrolon® | V-2 1.5 / V-2 3.0 | MVR 19 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 2865 | Covestro | Makrolon® | V-2 1.5 / V-2 3.0 | MVR 10 cm³/10min | n/a / n/a | — / — |
| PC | 6455 | Covestro | Makrolon® | V-0 3.0 | MVR 12 cm³/10min | n/a / n/a | — / — |
| PC | 6457 | Covestro | Makrolon® | V-0 3.0 | MVR 12 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 6485 | Covestro | Makrolon® | V-0 1.5 / 5VA 3.0 | MVR 9.0 cm³/10min | n/a / n/a | — / — |
| PC | 6487 | Covestro | Makrolon® | V-0 1.5 / 5VA 3.0 | MVR 9.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 6555 | Covestro | Makrolon® | V-0 3.0 | MVR 10 cm³/10min | n/a / n/a | — / — |
| PC | 6557 | Covestro | Makrolon® | V-0 3.0 | MVR 10 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 6717 | Covestro | Makrolon® | V-0 2.0 | MVR 3.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 9125 | Covestro | Makrolon® | V-0 1.5 (20% GF) | MVR 8.0 cm³/10min | n/a / n/a | — / — |
| PC | 9415 | Covestro | Makrolon® | V-0 1.5 / 5VA 3.0 (10% GF) | MVR 6.0 cm³/10min | n/a / n/a | — / — |
| PC | 9417 | Covestro | Makrolon® | V-0 1.5 / 5VA 3.0 (10% GF) | MVR 6.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | FR6002 | Covestro | Makrolon® | FR (grade stated) | MVR 18 cm³/10min | n/a / n/a | — / — |
| PC | FR7087 | Covestro | Makrolon® | V-0 2.2 / 5VA 3.0 | MVR 12 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | GF9002 | Covestro | Makrolon® | V-0 1.2 (10% GF) | MVR 15 cm³/10min | n/a / n/a | — / — |
| PC | 6265 X | Covestro | Makrolon® | V-0 1.5 | MVR 19 cm³/10min | n/a / n/a | — / — |
| PC | 6267 X | Covestro | Makrolon® | V-0 1.5 | MVR 19 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 6487 RE | Covestro | Makrolon® | V-0 1.5 / 5VA 3.0 | MVR 9.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 6555 RE CQ | Covestro | Makrolon® | V-0 3.0 | MVR 10 cm³/10min | n/a / n/a | — / — |
| PC | 6265 X RE25 CQ | Covestro | Makrolon® | V-0 1.5 | MVR 19 cm³/10min | n/a / n/a | — / — |
| PC | 6265 X RE CQ | Covestro | Makrolon® | V-0 1.5 | MVR 19 cm³/10min | n/a / n/a | — / — |
| PC | 6267 X RE CQ | Covestro | Makrolon® | V-0 1.5 | MVR 19 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | 1804 | Covestro | Makrolon® | V-2 1.5 / V-2 3.0 (extrusion) | MVR 6.0 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | FR1897 | Covestro | Apec® (high-heat copolymer) | V-2 1.5 / V-0 3.0 (VST/B120 = 182°C) | MVR 18 cm³/10min (330°C/2.16kg) | n/a / n/a | ✅ UV (EN 170) / — |
Covestro ISO TDS commonly reports flow as MVR (cm³/10min) and does not list Izod kJ/m² in the way Chimei does; impact data available in the full TDS on request. UL ratings are color- and thickness-dependent.
Substitution Checklist (Procurement Review):
Before replacing any grade, verify (1) UL94 rating at the same wall thickness, (2) UL-listed color, (3) halogen-free or PFAS-free declaration, (4) MFR / MVR, (5) notched impact at 23°C and –30°C, (6) UV / UL 746C f1 status, and (7) processing window (barrel temp / mold temp). Typical values are not specifications. Please request current TDS / SDS / COA and test samples before substitution.
| Type | Grade No. | Manufacturer | Brand | UL94 Multi-Thickness (mm) | MFR / MVR (300°C/1.2kg) | Notched Izod 23°C / –30°C | UV / UL 746C f1 |
|---|---|---|---|---|---|---|---|
| PC | 201R | Sabic | LEXAN® | V-2 1.09 / V-0 5.99 | MFR 7 g/10min | n/a / n/a | — / — |
| PC | 203R | Sabic | LEXAN® | V-2 | MFR 7 g/10min; MVR 6 | n/a / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | 221R | Sabic | LEXAN® | V-2 | MFR 18 g/10min | n/a / n/a | — / — |
| PC | 223M | Sabic | LEXAN® | V-2 | MFR 18 g/10min | n/a / n/a | ✅ UV / — |
| PC | 223R | Sabic | LEXAN® | V-2 | MFR 18 g/10min; MVR 21 | n/a / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | 223S | Sabic | LEXAN® | FR (improved; small/intricate parts) | MFR 17.5 g/10min | n/a / n/a | ✅ UV / — |
| PC | 241S | Sabic | LEXAN® | FR (improved; super release) | MFR 10.5 g/10min | n/a / n/a | — / — |
| PC | 243R | Sabic | LEXAN® | V-2 | MFR 11 g/10min; MVR 12 | n/a / n/a | ✅ UV / ✅ UL 746C f1 |
| PC | AVP KLL10FR | Sabic | LEXAN® | V-0 / 5VA (10% GF) | n/a (TDS not disclosed here) | n/a / n/a | — / — |
| PC | AVP TLL12CU | Sabic | LEXAN® | V-2 | MFR 12 g/10min (target) | n/a / n/a | ✅ UV / — |
| PC | AVP TLL80CU | Sabic | LEXAN® | V-2 | MFR 20 g/10min (target) | n/a / n/a | ✅ UV / — |
| PC | AVP ZLL12CP | Sabic | LEXAN® | V-2 | MFR 12 g/10min (target) | n/a / n/a | — / — |
| PC | HF1110 | Sabic | LEXAN® | V-2 | MFR 25 g/10min | n/a / n/a | — / — |
| PC | HF1110R | Sabic | LEXAN® | V-2 | MFR 25 g/10min; MVR 26 | n/a / n/a | — / — |
| PC | HF1130 | Sabic | LEXAN® | V-2 | MFR 25 g/10min | n/a / n/a | ✅ UV / — |
| PC | HF1130R | Sabic | LEXAN® | V-2 | MFR 25 g/10min; MVR 26 | n/a / n/a | ✅ UV / — |
| PC | HF1140R | Sabic | LEXAN® | V-2 | MFR 25 g/10min; MVR 26 | n/a / n/a | — / — |
| PC | HFR1723 | Sabic | LEXAN® | V-2 | MFR 25 g/10min | n/a / n/a | ✅ UV / — |
| PC | LUX2114 | Sabic | LEXAN® | FR (improved) | MFR 18 g/10min | n/a / n/a | ✅ UV / — |
| PC | LUX2114G | Sabic | LEXAN® | FR (improved) | MFR 18 g/10min | n/a / n/a | ✅ UV / — |
| PC | LUX2289 | Sabic | LEXAN® | V-2 | MFR 17 g/10min; MVR 16 | n/a / n/a | ✅ UV / — |
| PC | LUX2614G | Sabic | LEXAN® | FR (LED diffusion) | n/a (high-viscosity) | n/a / n/a | ✅ UV / — |
| PC | LUX2619 | Sabic | LEXAN® | V-2 1.5 (extrusion) | n/a (extrusion grade) | n/a / n/a | — / — |
| PC | ML3729 | Sabic | LEXAN® | V-2 | MVR 36 cm³/10min | n/a / n/a | ✅ UV / — |
| PC | ML3729R | Sabic | LEXAN® | V-2 (US) | MFR 39 g/10min; MVR 36 | n/a / n/a | ✅ UV / — |
Sabic LEXAN® TDS commonly reports Izod in ft·lb/in rather than kJ/m²; impact data available in the full TDS on request. UL ratings are color- and thickness-dependent.
Substitution Checklist (Procurement Review):
Before replacing any grade, verify (1) UL94 rating at the same wall thickness, (2) UL-listed color, (3) halogen-free or PFAS-free declaration, (4) MFR / MVR, (5) notched impact at 23°C and –30°C, (6) UV / UL 746C f1 status, and (7) processing window (barrel temp / mold temp). Typical values are not specifications. Please request current TDS / SDS / COA and test samples before substitution.
Frequently Asked Questions (FAQ)
V-0 is the highest rating, where the material extinguishes within 10 seconds without dripping. V-1 allows extinguishing within 30 seconds without dripping, while V-2 allows extinguishing within 30 seconds but permits dripping of flaming particles.
Yes, due to the addition of flame retardant additives and more complex production processes, FR PC is generally 10-30% more expensive than standard PC.
Absolutely. For any product listed on this page, please contact us or click the product link to request the Technical Data Sheet (TDS) and UL Yellow Card.
Explore Resources
- General Purpose Grade PC
- Optical Grade PC
- Weather Resistant Grade PC
- Food Contact Grade PC
- Medical Grade PC