High-Performance PEN Resin

TEIJIN PEN Resin for Demanding Transparent Applications

PEN, Polyethylene Naphthalate, is a high-performance polyester resin. It provides stronger heat resistance, gas barrier performance, chemical resistance, and low adsorption compared with many common transparent plastics.

teijin chemicals pen plastic raw material granules

Supply Grades of PEN pellets

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PENTN-8065STEIJIN CHEMICALS General injection molding grade, low oxygen permeability, good barrier performance, 80 MPa tensile strength, No Break unnotched Charpy impactBarrier packaging parts; precision injection molded parts; electronic housings; heat-resistant functional parts; medical/healthcare packaging components

Features Overview

Gas Barrier Performance

Suitable for containers and molded parts requiring reduced oxygen and vapor transmission.

Chemical Resistance

Designed for applications where PC, PET, or COC may not provide enough chemical resistance.

Low Adsorption

Useful for pharmaceutical and medical container applications requiring reduced material interaction.

Higher Heat Resistance

Heat-resistant PEN development grades provide HDT up to 147°C at 0.45 MPa.

Transparent Molding

Suitable for transparent medical containers and inspection-friendly precision parts.

Dimensional Stability

YJ-0157 and YJ-0158 show 0% dimensional change rate under listed test conditions.

Available PEN Resin Grades

Grade selection depends on heat resistance, flow, transparency requirement, barrier performance, and final application validation.


Standard Transparent PEN
TN-8065S
Density 1,330 kg/m³
MVR 15 cm³/10 min
HDT, 0.45 MPa 107°C
Oxygen Barrier 12
Water Vapor Barrier 0.3

High Heat-Resistant Grade
YJ-0157
Density 1,320 kg/m³
MVR 11 cm³/10 min
HDT, 0.45 MPa 138°C
Tensile Strength 97 Mpa
Dimensional Change 0%

Higher Heat-Resistant Grade
YJ-0158
Density1,310 kg/m³
MVR7 cm³/10 min
HDT, 0.45 MPa147°C
Tensile Strength100 Mpa
Dimensional Change0 %

Application for High-Performance PEN

PEN is suitable for transparent and barrier-related applications requiring stronger performance than standard PET.

Medical Containers

Transparent containers requiring chemical resistance and barrier performance.

Pharmaceutical Packaging

Packaging applications requiring low adsorption and stable barrier properties.

Barrier Parts

Molded components where oxygen and vapor transmission need to be reduced.

Diagnostic Components

Transparent precision molded parts for inspection-friendly medical device design.

Heat-Resistant Parts

Applications requiring higher HDT than standard PET materials.

Chemical-Resistant Parts

Parts exposed to selected chemical environments after validation testing.

Low-Adsorption Containers

Useful for material-contact applications requiring reduced adsorption risk.

Precision Molding

Suitable for transparent and dimensionally controlled molded components.

High-Performance PEN Resin FAQ

Is PEN resin an engineering plastic?

Yes. PEN can be positioned as an engineering plastic or high-performance polyester resin. It provides stronger heat resistance, gas barrier performance, chemical resistance, and dimensional stability than standard PET.

What is TEIJIN TN-8065S?

TN-8065S is a standard transparent PEN resin grade. It provides chemical resistance, gas barrier performance, low adsorption, and an HDT of 107°C at 0.45 MPa.

What are YJ-0157 and YJ-0158?

YJ-0157 and YJ-0158 are TEIJIN high heat-resistant PEN development grades. They provide HDT values of 138°C and 147°C at 0.45 MPa respectively.

Is PEN better than PET?

PEN is preferred when better heat resistance, gas barrier performance, chemical resistance, and low adsorption are required. PET is still more common for general packaging.

Send Us a Message