LEXAN™ Resin PC

LEXAN™ Polycarbonate (PC)

Lexan™ polycarbonate is a high-performance thermoplastic that offers exceptional strength, impact resistance, and transparency. It is widely used in various industries, including automotive, construction, electrical and electronics, and safety equipment, due to its outstanding properties.

polycarbonate pc resin

Lexan PC available for bulk purchase

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PC101SabicLEXAN7 MFR polycarbonate, MVR of 6. UL94 HB rated.Suitable for extrusion and injection molding applications.
PC101RSabicLEXANUL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR.for thicker sections without sinks. Internal mold release
PC102LSabicLEXANhigh viscosity linear polycarbonate resin granulate.be used as a base material for production of transparent and opaque products
PC103SabicLEXAN7 MFR polycarbonate, MVR of 6. UV stabilized. UL94 HB rated. UL746C f1 rated.for extrusion and injection molding applications
PC103RSabicLEXAN7 MFR polycarbonate, MVR of 6. UV Stabilized. Mold release. UL94 HB rated. UL746C f1 rated.for extrusion and injection molding applications
PC104SabicLEXAN7 MFR polycarbonate, MVR of 6. Grade designed for food contact. UL94 HB ratedfor extrusion and injection molding applications
PC104RSabicLEXAN7 MFR polycarbonate, MVR of 6. Mold release. UL94 HB rated.for extrusion and injection molding applications
PC121MSabicLEXAN18 MFR polycarbonate. Improved internal mold release. UL94 HB rated. 
PC121RSabicLEXAN18 MFR polycarbonate, MVR of 21. Mold release. UL94 HB rated. 
PC121SRMSabicLEXANEasy flow, impact modified, super release grade polycarbonate. 
PC123SabicLEXANUL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. 
PC123MSabicLEXAN18 MFR polycarbonate. UV Stabilized. Improved internal mold release. UL94 HB rated. 
PC123RSabicLEXAN18 MFR polycarbonate, MVR of 21. UV Stabilized. Mold release. UL746C f1 rated. UL94 HB rated 
PC123SRMSabicLEXANEasy flow, uv stabilised, impact modified, super release grade 
PC124RSabicLEXAN18 MFR polycarbonate. 21 MVR. Mold release. UL94 HB rated. 
PC131SabicLEXAN3.5 MFR polycarbonate. UL94 HB rated. For blow molding or extrusion.Suitable for injection molding.
PC133RSabicLEXAN3.5 MFR polycarbonate, MVR of 3. UV Stabilized. Mold release. UL94 HB rated.designed for blow molding or extrusion. Suitable for injection molding.
PC134RSabicLEXAN3.5 MFR polycarbonate, MVR of 3. Grade intended for food contact. Mold release. UL94 HB rated.Designed for blow molding or extrusion. Suitable for injection molding.
PC141SabicLEXAN11 MFR polycarbonate. UL94 HB rated. 
PC141RSabicLEXAN11 MFR polycarbonate, MVR of 12. Mold release. UL94 HB rated. 
PC143SabicLEXANUL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. 
PC143RSabicLEXAN11 MFR polycarbonate, MVR of 12. UV Stabilized. Mold release. UL94 HB rated. UL746C f1 rated. 
PC144RSabicLEXAN11 MFR polycarbonate, MVR of 12. Mold release. UL94 HB rated. This material is food contact compliant in most jurisdictions 
PC153RSabicLEXAN2.5 MFR Branched polycarbonate. UV Stabilized. Mold release. UL94 HB rated. 
PC161RSabicLEXANa medium viscosity multi purpose grade and contains a release agent to ensure easy processing. 
PC163RSabicLEXANmedium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. 
PC164RSabicLEXANMedium viscosity, multi purpose polycarbonate resin with added release agentdesigned for blow molding or extrusion.
PC172LSabicLEXANlow viscosity linear polycarbonate resin granulatebe used as a base material for production of transparent and opaque products.
PC191SabicLEXAN9 MFR polycarbonate. UL94 HB rated. Improved chemical resistance. Available only in opaque colors. 
PC201RSabicLEXAN7 MFR polycarbonate. Mold release. Flame retardant grade, UL94 V2 rated.For extrusion and injection molding.
PC203RSabicLEXAN7 MFR polycarbonate, MVR of 6. UV stabilized. Mold release. Flame retardant grade, UL94 V2 rated. UL746C f1 ratedFor extrusion and injection molding.
PC221RSabicLEXAN18 MFR polycarbonate. Mold release. Flame retardant grade, UL94 V2 rated. 
PC223MSabicLEXAN18 MFR polycarbonate. UV Stabilized. Improved mold release. Flame retardant grade, UL94 V2 rated. 
PC223RSabicLEXAN18 MFR polycarbonate, MVR of 21. UV stabilized. Mold release. Flame retardant grade, UL94 V2 rated. UL746C f1 rated. 
PC223SSabicLEXAN17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. 
PC241RSabicLEXAN  
PC241SSabicLEXAN10.5 MFR. Improved flame retardance. Super mold release. 
PC243RSabicLEXAN11 MFR polycarbonate, MVR of 12. UV stabilized. Mold release. Flame retardant grade, UL94 V2 rated. UL746C f1 rated. 
PC244RSabicLEXAN10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. 
PC244RFSabicLEXANa medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors 
PC263RSabicLEXANmedium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. 
PCAD143SabicLEXANmedium viscosity, injection molding grade exhibiting low dust attraction. 
PCAT1230RSabicLEXAN  
PCAT2030RSabicLEXAN  
PCAVP KLL10FRSabicLEXAN10% glass fiber filled polycarbonate. UL94 V0 and 5VA rated. 
PCAVP TLL12CUSabicLEXANAVP TLL12CU resin is a wide specification polycarbonate. 12 MFR targeted. UV stabilized. UL94 V2 rated. Injection moldable. Available in clear and in opaque colorsdesigned for applications with high optical requirements in terms of clarity and light transmission
PCAVP TLL80CUSabicLEXANwide specification polycarbonate. 20 MFR targeted. UV stabilized. UL94 V2 rated. Injection moldable. Available in clear. 
PCAVP ZLL12CPSabicLEXANwide specification polycarbonate. 12 MFR targeted. UL94 V2 rated. Available in limited opaque colors. 
PCAVP ZLL19CUSabicLEXANwide specification polycarbonate. 19 MFR targeted. UV stabilized. Available in limited opaque colors. 
PCEM1210SabicLEXANExcellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditionsAutomotive interiors.
PCEM3110SabicLEXAN20 MFR polycarbonate. Impact resistant at -20oC. UL94 HB rated. Optimized flow and processability for cost effective thinner wall designs.for automotive interiors.
PCEX1332TSabicLEXAN3 MFR polycarbonate, MVR of 3. UV stabilized. Release agent. UL94 HB rated.Designed for use in multi-wall sheet or profile extrusion applications.
PCEX1632TSabicLEXAN6 MFR polycarbonate, MVR of 6. UV stabilized. Release agent. UL94 HB rated.Designed for use in multi-wall sheet or profile extrusion applications.
PCEX5681TSabicLEXANcoextrusion product which is UV stabilized for improved outdoor weathering of LEXAN™ sheet and improved processing. 
PCEX6681TSabicLEXANcoextrusion product which is UV stabilized for good outdoor weathering of LEXAN™ sheet and excellent processing. 
PCEX7631TSabicLEXANhighly UV stabilized, 10 MFR polycarbonate. Release agent.Suitable for co-extrusion / cap layers. Exhibits low plate out and improved outdoor weathering on PC sheets.
PCEX7681TSabicLEXANhighly UV stabilized 10 MFR polycarbonate, MVR of 10.Suitable for co-extrusion / cap layers. Exhibits low plate out and improved outdoor weathering on PC sheets.
PCEX8681TSabicLEXANcoextrusion product which is highly UV stabilizedfor improved outdoor weathering of LEXAN™ sheet and excellent processing.
PCEX9332TSabicLEXANMVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retadant, mold release, UV stabilized, transparent, translucent and opaque colors.Material typically used in railway applications and building & construction. Multiwall sheet, solid sheet, pipe, profiles
PCGLX143SabicLEXANwith MVR of 12. Medium viscosity grade. Excellent candidate. Available in transparent and translucent colors.for applications with high optical quality requirements such as automotive glazing (vehicle windows).
PCHF1110SabicLEXAN25 MFR polycarbonate. UL94 V2 rated. 
PCHF1110RSabicLEXAN25 MFR polycarbonate, MVR of 26. Mold release. UL94 V2 rated. 
PCHF1130SabicLEXAN25 MFR polycarbonate. UV stabilized. UL94 V2 rated. 
PCHF1130RSabicLEXAN25 MFR polycarbonate, MVR of 26. UV stabilized. Mold release. UL94 V2 rated. 
PCHF1140SabicLEXAN25 MFR polycarbonate, MVR of 26. Grade designed for food contact. UL94 V2 rated. 
PCHF1140RSabicLEXAN25 MFR polycarbonate, MVR of 26. Mold release. UL94 V2 rated. 
PCHF1840RSabicLEXANMVR (300°C/1.2kg) 36 cm3/10min, extreme low viscosity, injection molding, mold release, transparent.This material is food contact compliant in most jurisdictions – exceptions may exist, request a declaration for details.
PCHF3510RSabicLEXAN39 MFR polycarbonate, MVR of 34. Mold release. Easy processing. Available only in opaque colors.Suitable for automotive applications, including bezels
PCHF4010SRSabicLEXANexcellent flow 42 MFR polycarbonate, MVR of 40. Superior release. High gloss. Available in opaque colors.Suitable for large parts and thin wall molding.
PCHFR1723SabicLEXAN25 MFR polycarbonate. UV stabilized. Mold release. UL94 V2 rated.Available in transparent, limited package types, and must meet minimum order quantity requirements.
PCHFR1724SabicLEXAN25 MFR polycarbonate. Grade designed for food contact. Mold release. UL94 V2 rated.Available in transparent, limited package types, and must meet minimum order quantity requirements.
PCIR1810SabicLEXANhigh flow (MFR = 22 at 300°C/1.2kg), heat stabilizedfor use in the custom compounding market.
PCIR1840SabicLEXANhigh flow (MFR = 22 at 300°C/1.2kg), heat stabilizedfor use in the general purpose molding market.
PCIR2040SabicLEXAN18 MFR polycarbonate, MVR of 21. Grade designed for food contact. Mold release.Available in transparent, limited package types, and must meet minimum order quantity requirements.
PCIR2110SabicLEXANmedium-high flow (MFR = 15 at 300°C/1.2kg), heat stabilizedfor use in the custom compounding market.
PCIR2210SabicLEXANmedium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilizedfor use in the custom compounding market.
PCIR2240SabicLEXAN11 MFR polycarbonate, MVR of 9. Grade designed for food contact. Mold release.Available in transparent, limited package types, and must meet minimum order quantity requirements.
PCIR2840SabicLEXAN7 MFR polycarbonate, MVR of 6. Grade designed for food contact. Mold release. Injection moldable.Available in transparent, limited package types, and must meet minimum order quantity requirements.
PCLS1SabicLEXAN20 MFR polycarbonate, MVR of 21. UV stabilized. UL94 HB rated. UL746C f1 rated. Low viscosity.For automotive lens applications. AMECA listed.
PCLS2SabicLEXAN11 MFR polycarbonate, MVR of 12. UV stabilized. UL94 HB rated. UL746C f1 rated. Medium viscosity.For Automotive lens applications. AMECA listed.
PCLSHFSabicLEXAN25 MFR polycarbonate, MVR of 24. UV stabilized.For Automotive lens applications. AMECA listed.
PCLUX1619SabicLEXAN7.5 MFR polycarbonate. UL94 HB rated.For high light reflectance. Extrudable and injection moldable.
PCLUX2010TSabicLEXANInjection moulding grade. Excellent flow properties combined with very high transmission and color stability.especially designed for manufacturing optical parts
PCLUX2110TSabicLEXANInjection moulding grade. Easy flow properties combined with very high transmission and color stability.especially designed for manufacturing optical parts
PCLUX2114SabicLEXAN18 MFR. Improved flame retardance. Internal mold release. UV stabilized. 
PCLUX2114GSabicLEXAN18 MFR. Improved flame retardance. Internal mold release. UV stabilized. 
PCLUX2289SabicLEXAN17 MFR polycarbonate, MVR of 16. UV stabilized. UL94 V2 rated. High light reflectance. Injection moldable. 
PCLUX2614GSabicLEXANdiffusive, high viscosity, uv stabilized, flame retardantDeveloped for injection molding LED applications
PCLUX2619SabicLEXANextrusion grade. It is UL94 V-2 rated at 1.5 mm.designed for high light reflectance.
PCML3729SabicLEXANan excellent flow polycarbonate with MVR of 36. UV stabilized. UL94 V2 rated. Easy processing. Available in transparent, translucent and opaque colors. 
PCML3729RSabicLEXAN39 MFR polycarbonate, MVR of 36. UV stabilized. Mold release. UL94 V2 rated (US). Easy processing. 
PCOQ1022SabicLEXANan optical quality polycarbonate. High purity resin. Produced in dedicated equipment with stringent production control conditions.for CD, DVD and BD applications at short cycle times (not UV stabilized).
PCOQ1028SabicLEXANan optical quality polycarbonate. High purity resin. Produced in dedicated equipment with stringent production control conditions.for CD, DVD and BD applications at short cycle times (not UV stabilized).
PCOQ2720SabicLEXAN7.5 MFR polycarbonate. UV stabilized. Produced in dedicated equipment with stringent production control conditions. Available in transparent and translucent colors.For ophthalmic or safety lens market.
PCOQ3420SabicLEXAN11 MFR polycarbonate. UV stabilized. Medium viscosity.Designed for ophthalmic lenses.
PCOQ3820SabicLEXAN7.4 MFR polycarbonate, MVR of 6. UV stabilized. High viscosity.Designed for ophthalmic lenses.
PCOQ4005SabicLEXANMVR of 8, UV-stabilized PC. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades.Suitable for sunglass and sunvisor markets.
PCOQ4120RSabicLEXAN25 MFR polycarbonate, MVR of 21. UV stabilized. Mold release. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades.Suitable for sunglass and sunvisor markets.
PCOQ4320RSabicLEXAN13 MFR polycarbonate. UV stabilized. Mold release. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades.Suitable for sunglass and sunvisor markets.
PCOQ4820SabicLEXANpolycarbonate with MVR 6. UV stabilized. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades.Suitable for sunglass and sunvisor markets.
PCPK2870SabicLEXAN2.5 MFR branched polycarbonate, MVR of 2. High viscosity. For blow molding, with high melt strength and high impact resistance.Excellent candidate for water bottle applications. Available in transparent colors only.
PCPU1230RSabicLEXAN11 MFR polycarbonate, MVR of 12. UV stabilized. Medium viscosity.Designed for Automotive trim applications, excellent PUR coating adhesion.
PCPU2030RSabicLEXAN17 MFR polycarbonate, MVR of 18. UV stabilized. Low viscosity.Designed for Automotive trim applications, excellent PUR coating adhesion.
PCT5R141RCSabicLEXANETP compound, which is formulated with 50wt% post-consumer recycled plastics. 
PCVR1820SabicLEXANhigh flow (MFR = 22 at 300°C/1.2kg), heat and UV stabilized, polycarbonate product with mold releasedesigned for use in the general purpose molding market.
PCVR2020SabicLEXAN18 MFR polycarbonate, MVR of 17. UV stabilized. Mold release. UL746C f1 rated. Available in transparent, limited package types, and must meet minimum order quantity requirements. 
PCVR2220SabicLEXAN12 MFR polycarbonate, MVR of 11. UV stabilized. Mold release. UL746C f1 rated. Available in transparent, limited package types, and must meet minimum order quantity requirements. 
PCVR2820SabicLEXAN7 MFR polycarbonate, MVR of 6. UV stabilized. Mold release. Injection moldable.Available in transparent, limited package types, and must meet minimum order quantity requirements.
PCXLS1110SabicLEXAN35 MVR polycarbonate.Designed for automotive optical parts requiring excellent flow properties, very high transmission and color stability. AMECA listed for protected applications only.
PCXLS1110TSabicLEXAN35 MVR polycarbonate.Designed for automotive optical parts requiring excellent flow properties, very high transmission and color stability. AMECA listed for protected applications only.
PCXLS1210SabicLEXAN18 MVR polycarbonate.Designed for automotive optical parts requiring very high transmission and color stability. AMECA listed for protected applications only.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.