LG Chem ABS Resin

  • Home /
  • LG Chem ABS Plastic Granules

LG ABS Plastic Granules

LG MABS (Methyl Methacrylate Acrylonitrile Butadiene Styrene) is a line of transparent, high-impact thermoplastic resins produced by LG Chem. It combines the exceptional optical clarity and scratch resistance of acrylic (PMMA) with the superior impact strength and processability of standard ABS.

acrylonitrile butadiene styrene abs resin

LG ABS available for bulk purchase

Type Grade No. Manufacturer Brand Grade/Features Use/Applications
ABS AP163 LG Chem / with high antistatic property and high impact strength. injection molding, Semiconductor
ABS HI121H LG Chem / Impact Resistance, General Purpose Electrical/Electronic Products, Miscellaneous Goods
ABS HI121U LG Chem / Injection molding,impact resistance and UV resistance. Electrical/Electronic Products, Miscellaneous Goods
ABS HI121UNS LG Chem / UV Resistance, Antistatic, Impact Resistance Electrical/Electronic Products, Miscellaneous Goods
ABS HI130 LG Chem / Injection molding,very high impact strength and bright white color Motorcycle Interior Parts Refrigerator
ABS HI135 LG Chem / Product for injection molding with high impact strength; High Rubber Content. Safety helmets, Miscellaneous goods
ABS HI140 LG Chem / Injection molding, designed to have super high impact strength and bright white color Safety Helmet Motorcycle Parts.
ABS HP100H LG Chem / with high impact, low temperature resistance and satisfactory spray paint effect. Opaqueness, Hot Stamping, Paintability, Helmets, watches, refrigerators
ABS HP100S LG Chem / Opaqueness, Hot Stamping, Paintability, Multi-axial Impact Strength, High Stiffness Bags, fans, electric toothbrushes
ABS HP171 LG Chem / General purpose injection molding grade with medium flow and high gloss. Router, Ear Phone, remote control, oxygen concentrator.
ABS HP181 LG Chem / Injection molding, with high flow and excellent impact properties. Opaqueness, Hot Stamping, Paintability, Bright White, Colorability, Dimensional Stability Washing machines, air conditioners, air purifiers, sweeping robots
ABS HT550 LG Chem / High Gloss, High Stiffness Electrical/Electronic Products Electric Bike
ABS HT700 LG Chem / High Stiffness Piano Key, Bobbin, Electrical/Electronic Products, Miscellaneous Goods
ABS SG175 LG Chem / Injection molding, designed to have a super gloss level. Refrigerator, Washing Machine, Electrical/Electronic Products
ABS SG175G LG Chem / Injection molding, designed to have extra high gloss and high fluidity. Super Gloss, High Flow. Electrical/Electronic Products
ABS SG175H LG Chem / Super Gloss, UV Resistance. Refrigerator, Washing Machine, Electrical/Electronic Products.
ABS MP220-H LG Chem / Electroplating Grade (Mental Plating Grade).Excellent adhesion and processability Automobiles Radiator Grille, Molding
ABS RS650 LG Chem / Product for extrusion molding with high impact strength. General Extruded Sheet, Pipe, Bathroom Ceiling
ABS RS670 LG Chem / Thermoforming, Chemical Resistance to Cyclopentane, High Impact Strength. Refrigerator
ABS RS681 LG Chem / Extrusion grade, high strength and vacuum blister performance. Hot Stamping, Paintability, Chemical Resistance to Cyclopentane, Multi-axial Impact Strength, Curve Destruction Weight. Extruded Board, refrigerator liners, home profiles.
ABS SH610A LG Chem / Product for extrusion molding with high impact strength. General Extruded Sheet
ABS AF312A LG Chem / Injection molding, with 1.5mm V-0 flame retardancy and high flow. Hot Stamping, Paintability, imensional Stability. Switch panel, socket, Charge, electric control box
ABS AF312B LG Chem / Fire resistance (2.1mm V-0). Opaqueness, Hot Stamping, Paintability, High Gloss,Dimensional Stability, High Flow. Heater, electric control box, Charge bank, hair dryer.
ABS AF312C LG Chem / Opaqueness, Flame Retardancy, Hot Stamping, Paintability, High Gloss, Dimensional Stability, High Flow. Power switches, alarms, uninterruptible power supplies, security cameras
ABS AF362H LG Chem / fire resistance (3.2mm V-0) Blood pressure monitor, oxygen concentrator, pulse monitor
ABS AF364 LG Chem / High Flame Retardancy, Medium Heat Resistance Hair Dryer, Terminal Box, Electrical/Electronic Products
ABS AF365 LG Chem / Product for injection molding with 2.0mm V-0 flame retardancy. Batter Case, PCB Case, Electrical/Electronic Products
ABS AF365B LG Chem / Flame Retardant ABS product for injection molding, V-0 at 2.0mm. Electrical/ElectronicProducts,IT/OADevices,TV,MonitorHousing
ABS AF365F-L LG Chem / Flame Retardant ABS product for injection molding, V-0 at 2.0mm, high fluidity and good dimensional stability. Television, Bidet, Electrical/Electronic Products
ABS AF365H LG Chem / Opaqueness, Flame Retardancy, Medium Heat Resistance, Hot Stamping, Paintability, High Gloss, Bright White, Thermal Stability, Colorability Control cabinet, fireproof Board, router, Print
ABS AF365HB LG Chem / fire resistance (2.0mm V-0) Special for battery
ABS AF365HF LG Chem / Opaqueness, Medium Heat Resistance, Hot Stamping, Paintability, High Gloss, Bright White, Thermal Stability, Colorability, High Flow. Distribution boxes, medical equipment, speakers, frequency converters.
ABS AF365S LG Chem / Flame Retardant ABS product for extrusion and blow molding, V-0 at 2.0mm Battery Tray
ABS AF366 LG Chem / Flame Retardant ABS product for injection molding, V-0 at 1.5mm. Batter Case, PCB Case, Electrical/Electronic Products
ABS AF366A LG Chem / Product for injection molding with 1.5mm V-0 flame retardancy and high fluidity. Electrical/Electronic Products, IT/OA Devices, TV, Monitor Housing
ABS AF366F LG Chem / Product for injection molding with 1.5mm V-0 flame retardancy and high fluidity. Television, Electrical/Electronic Products
ABS AF366H LG Chem / fire resistance (1.5mm V-0) Speakers, oxygen concentrators, heaters, toilet seats
ABS AF366HF LG Chem / fire resistance (1.5mm V-0).Opaqueness, Bright White. Industrial electronic control boxes, purifiers, heaters.
ABS AF367C LG Chem / Flame Retardancy V-0 at 2.5mm Electrical/Electronic Products, IT/OA Devices, TV, Monitor Housing.
ABS AF367H LG Chem / fire resistance (2.5mm V-0). High thermal resistance, and good Thermal stability. Blood pressure monitor, oxygen concentrator, power supply development, socket.
ABS EF378L LG Chem / Flame Retardancy, Non-Halogen MFP (Multi-Function Printer), Sound Bar, Electrical/Electronic Products
ABS FR500 LG Chem / Flame Retardancy, Imflammability Electrical/Electronic Products
ABS FR500A LG Chem / A TBBA Flame Retardant ABS product for injection molding, V-0 at 1.5mm Electrical/Electronic Products
ABS FR500H LG Chem / A TBBA Flame Retardant ABS product for injection molding, V-0 at 2.5mm. Electrical/Electronic Products.
ABS FR530 LG Chem / Flame Retardancy, Thermal Stability, Colorability,Imflammability. Electrical/Electronic Products Medical Equipment Housing.
ABS BM662 LG Chem / Standard Purpose, High Heat Resistance, Paintability Spoiler
ABS ER232 LG Chem / High Heat Resistance, Metal Plating, Thermal Stability, Superior Surface Quality, High Flow. Bumper, Cockpit, Door Trim, Exterior ETC, Interior ETC, Outside Mirror, Rear Combination Lamp.
ABS ER400 LG Chem / Medium Heat Resistance, High Impact Strength Automotive Interior Parts, Automotive Exterior Parts, Sheet
ABS ER400-C LG Chem / Medium Heat Resistance, Low TVOC, Low Gloss General Extruded Sheet, Edge Band
ABS ER400-M LG Chem / Medium Heat Resistance, Non Painting, Low TVOC, Low Gloss Cockpit, Door Trim, Edge Band, Interior ETC
ABS ER460 LG Chem / Medium Heat Resistance Motorcycle, Vacuum Cleaner, Electrical/Electronic Products, Miscellaneous Goods
ABS ER468 LG Chem / Medium Heat Resistance, High Flow Electrical/Electronic Products, Miscellaneous Goods.
ABS NF424 LG Chem / High Heat Resistance, Low TVOC Automotive Interior Components (e.g., vents, control panels); Consumer Electronics Housings; Household Appliances and Kitchenware; Office Equipment Parts.
ABS XR401 LG Chem / Standard Purpose, High Heat Resistance, Paintability, High Impact Strength Air Conditioner, Air Purifier, Battery, Bumper, Cockpit, Coffee Machine, Consent, Dehumidifier, Delivery Robot, Door Trim, Drone, Electric Bike, Exterior ETC, Fan, Fan Heater, Fire Alarm, Food Serving Robot, Interior ETC, Microwave Oven, Motorcycle, Multi Tap, Outside Mirror, PCB (Printed Circuit Board), Power Tool, Security Alarm, Set-Top Box, Switch, Terminal Box, Tractor, UPS (Uninterruptible Power Supply System), Water Purifier, Wireless Router.
ABS XR401B LG Chem / High Heat Resistance, Paintability, Chemical Resistance /
ABS XR404 LG Chem / Standard Purpose, High Heat Resistance, Paintability, High Stiffness Air Conditioner, Battery, Bumper, Cockpit, Coffee Machine, Consent, Delivery Robot, Electric Bike, Electric Rice Cooker, Fan, Fan Heater, Fire Alarm, Food Serving Robot, Hair Dryer, Microwave Oven, Motorcycle, Multi Tap, Others, Outside Mirror, PCB (Printed Circuit Board), Power Tool, Rear Combination Lamp, Security Alarm, Set-Top Box, Spoiler, Switch, Terminal Box, Tractor, UPS, Water Purifier, Wireless Router.
ABS XR404T LG Chem / High Heat Resistance, Welding, Superior Surface Quality, Welding Strength Rear Combination Lamp
ABS XR409H LG Chem / Standard Purpose, Ultra High Heat Resistance, Non Painting Cockpit, Door Trim, Fire Alarm, Hair Dryer, Interior ETC, Microwave Oven, Rear Combination Lamp, Set-Top Box, Tractor, Wireless Router.
ABS XR410 LG Chem / High Heat Resistance, Non Painting, Low TVOC, Low Gloss Cockpit, Door Trim, Interior ETC
ABS XR438 LG Chem / Ultra High Heat Resistance, Paintability, Chemical Resistance, Dimensional Stability. /
ABS XR440 LG Chem / High Heat Resistance, Non Painting, Low TVOC, Low Gloss Cockpit, Door Trim, Interior ETC
ABS XR470 LG Chem / Ultra High Heat Resistance, Low TVOC Cockpit, Door Trim, Others
ABS XR474 LG Chem / Ultra High Heat Resistance, Non Painting, Low TVOC /
ABS XR490 LG Chem / Ultra High Heat Resistance, Non Painting, Low TVOC, Low Gloss Cockpit, Door Trim, Others
ABS XR630 LG Chem / High Heat Resistance, Chemical Resistance Window Profile Insulation Bar

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.