MABS Resin Plastic Pellets
- Home /
- MABS Resin



Supply Various Grades of MABS pellets
| Type | Grade No. | Manufacturer | Brand | Grade/Features | Use/Applications |
|---|---|---|---|---|---|
| MABS | PA-758 | Chi Mei | Polylac | Transparent Grade. Good transparency, high flowability | Air conditioning panels, washing machine covers, vacuum cleaner casings, 3C product casings, household appliances, stationery |
| MABS | PA-758R | Chi Mei | Polylac | Transparent Grade. Transparency with blue tint, high rigidity, chemical resistance | Air conditioning panels, washing machine covers, vacuum cleaner casings, 3C product casings, household appliances, stationery |
| MABS | PA-703 TRP | Chi Mei | Polylac | Transparent Grade. Transparency with blue tint, chemical resistance, comply with Bio-compatibility test (ISO10993) | Medical application |
| MABS | PA-702 TRP | Chi Mei | Polylac | Transparent Grade. Good transparency, well-balanced mechanical properties, comply with biocompatibility test (ISO 10993) | Medical application |
| MABS | PA-758 L125 | Chi Mei | Polylac | Transparent Grade. Transparency with blue tint, high flowability | Air conditioning panels, washing machine covers, vacuum cleaner casings, 3C product casings, household appliances, stationery |
| Type | Grade No. | Manufacturer | Brand | Grade/Features | Use/Applications |
|---|---|---|---|---|---|
| MABS | AT553 | LG Chem | / | Transparency, Permanent Antistatic. | Electrical/Electronic Products. |
| MABS | TR530F | LG Chem | / | Transparency, High Impact Strength, Softness | Artificial Nail |
| MABS | TR551 | LG Chem | / | Product for injection molding with transparency. Transparency, High Hardness, High Stiffness | Washing Machine, Refrigerator, Electrical/Electronic Products,Miscellaneous Goods |
| MABS | TR552 | LG Chem | / | Product for injection molding with transparency and high impact strength. Transparency, Chemical Resistance, High Impact Strength | Electrical/Electronic Products, Miscellaneous Goods |
| MABS | TR552F | LG Chem | / | High Transparency, Whitening Resistance, Softness | Artificial Nail, Edge Band. |
| MABS | TR556 | LG Chem | / | Transparency, Chemical Resistance, High Impact Strength | Electrical/Electronic Products, Miscellaneous Goods |
| MABS | TR557 | LG Chem | / | Transparency, High Impact Strength | Washing Machine, Refrigerator, Electrical/Electronic Products, Miscellaneous Goods. |
| MABS | TR558A | LG Chem | / | Transparency, General Purpose | Washing Machine, Refrigerator, Electrical/Electronic Products,Miscellaneous Goods |
| MABS | TR558A-L | LG Chem | / | Transparency | Medical equipment |
| MABS | XG569C | LG Chem | / | Transparency, Scratch Resistance, High Hardness, High Stiffness | Television, Sound Bar, Remote Control, Electrical/Electronic Products |
| MABS | XG571 | LG Chem | / | Translucency, High Gloss, High Flow. | Air Conditioner, Water Purifier, Air Purifier, Electrical/Electronic Products |
| MABS | XG571-G | LG Chem | / | Translucency, High Gloss, Scratch Resistance, High Flow | Electrical/Electronic Products |
| Type | Grade No. | Manufacturer | Brand | Grade/Features | Use/Applications |
|---|---|---|---|---|---|
| MABS | 900 352 U | TORAY | Toyolac | Transparent Grade, Middle Impact Strength | E&E Products, Household and Office Appliances, Toys |
| MABS | 900 352A U | TORAY | Toyolac | Transparent Grade, Middle Impact Strength | E&E Products, Household and Office Appliances, Toys |
| MABS | 912 X01 U | TORAY | Toyolac | Transparent Grade, High Scratch Resistant | E&E Products, Office Appliances, Toys |
| MABS | 920 555 U | TORAY | Toyolac | Transparent Grade, High Rigidity | E&E Products, Household and Office Appliances, Toys |
| MABS | 990 X88 | TORAY | Toyolac | Transparent Grade, High Impact Strength, High Flow | E&E Products, Household and Office Appliances, Toys |
What is MABS Resin?
MABS Resin (Methyl Methacrylate Acrylonitrile Butadiene Styrene) is a transparent engineering-grade thermoplastic. As a “clarity polymer,” MABS combines the impact resistance of ABS with the optical properties of PMMA, offering a unique balance of transparency, gloss, and toughness. It is widely referred to as MABS plastic due to its versatile applications.
Key Properties of MABS
- High transparency and glossy surface
- Outstanding impact resistance, even at low temperatures
- Good dimensional stability and rigidity
- Excellent colorability and printability
- Easy to process by injection molding and extrusion
- Resistant to environmental stress cracking
- Available in natural and customized colors
Applications of MABS
MABS resin is the ideal clarity polymer for many industries. Common uses include:
- Electronics: Transparent housings for LED displays and control panels.
- Cosmetic Packaging: High-gloss and durable cases for luxury products.
- Medical Devices: Diagnostic equipment and housings requiring visibility and sterility.
- Automotive Parts: Interior trims and illuminated control panels.
Other Names
- Transparent ABS
- MABS Copolymer
- Clear ABS Plastic
- MABS Pellets
- MABS Granules
Packaging
- 25kg bags or jumbo bags
- Palletized units available upon request
Appearance
- Transparent
- Translucent
- High-gloss surface
HS Code
- 39033000
MABS VS PC VS PMMA
| Property | MABS Resin | Polycarbonate (PC) | Acrylic (PMMA) |
|---|---|---|---|
| Transparency | 85–92% | 85–90% | 92% |
| Impact Resistance | High | Very High | Moderate |
| UV Resistance | Moderate | High | High |
| Application Examples | Electronics, Medical | Automotive, Aviation | Display Cases, Lighting |
What Makes ABS Clear: Modifications to Standard ABS
1. Chemical Composition Adjustments
Manufacturers create transparent ABS or MABS Resin by altering the traditional ABS formulation, focusing on the following:
- Reducing Butadiene Content: By decreasing the ratio of butadiene rubber, light scattering is minimized without compromising impact resistance.
- Incorporation of Methyl Methacrylate (MMA): Adding MMA aligns refractive indices between the rubber and SAN (Styrene-Acrylonitrile) phases, which enhances clarity and creates a hybrid “clarity polymer.”
- Optimizing Particle Size: The butadiene rubber particles are reduced in size to ensure minimal disruption of light transmission—a key factor in achieving transparency in MABS plastic.
2. Processing Techniques
Even beyond chemical adjustments, manufacturing techniques play a crucial role in enhancing the optical clarity of MABS plastic:
- Controlled Cooling Rates: During injection molding, carefully calibrated cooling methods prevent crystallization that could cause hazy or cloudy results.
- Nucleating Agents: These are added to promote smaller and more uniform crystal structures, allowing for greater transparency.
- Additives for Refractive Alignment: Proprietary refractive index modifiers are used to maximize the optical performance of the final polymer matrix.
Frequently Ask Questions
Find answers to the most common questions about MABS resin, including its composition, processing methods, certifications, and handling guidelines. Our expert responses help you make informed sourcing and application decisions.
Our MABS Resin offers exceptional impact resistance (inherited from ABS) combined with glass-like clarity (similar to PMMA), making it ideal for dashboard trims, light covers, and touchscreens. Unlike PC, it’s more cost-effective and resists stress cracking, while outperforming ABS in aesthetics and surface hardness. It’s UV-stabilized for long-term color retention, critical for automotive interiors exposed to sunlight.
Absolutely. We offer medical-grade MABS Resin with FDA, ISO 10993, and EU 10/2011 compliance. These grades are optimized for sterilizability (autoclave/ETO/Gamma) and chemical resistance, ensuring safety for surgical tool housings, diagnostic devices, and drug-delivery systems. Customization for color, rigidity, or flame retardancy is available.
Our ISO 9001-certified facilities employ rigorous quality control protocols, including real-time MFI (Melt Flow Index) tracking, spectroscopic analysis, and impact/thermal testing. We provide certificates of analysis (CoA) with every shipment and allow third-party lab verification.
Yes. Our UL94 V0/V2 grades meet IEC 62368 standards, with halogen-free options available. They maintain clarity (<5% haze) and withstand 85°C/85% RH aging tests, making them perfect for smart device housings or transparent protective covers..
Our MABS Resin is 100% recyclable (compatible with standard ABS/PMMA streams) and produced via energy-efficient processes (30% lower CO2 emissions vs. industry averages). We also offer bio-based filler options and certify compliance with REACH, RoHS, and TSCA.