PA66 Resin (Nylon 66 Resin)
- Home /
- Nylon PA66 Resin
PA66 Pellets
At Suke Plastics, we mainly supply:
- BASF Ultramid® PA66
- Shen Ma PA66
- Celanese Zytel® PA66




Supply Various Grades of PA66 pellets
| Type | Grade No. | Manufacturer | Brand | Grade/Features |
|---|---|---|---|---|
| PA66 | A3EG3 | Basf | ULTRAMID® | 15% glass fiber reinforced, good stiffness, oil-resistant. |
| PA66 | A3EG10 | Basf | ULTRAMID® | 50% glass fiber reinforced, high rigidity, oil-resistant. |
| PA66 | A3EG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, injection molding grade, high rigidity, excellent dimensional stability, oil-resistant. |
| PA66 | A3EG6 | Basf | ULTRAMID® | 30% glass fiber reinforced, high dimensional stability, high rigidity, oil-resistant. |
| PA66 | A3EG7 | Basf | ULTRAMID® | 35% glass fiber reinforced, high dimensional stability, high rigidity, oil-resistant. |
| PA66 | A3HG2 | Basf | ULTRAMID® | 10% glass fiber reinforced, injection molding grade, good electrical insulation properties, medium stiffness. |
| PA66 | A3SK | Basf | ULTRAMID® | Injection molding grade, short cycle time, excellent flowability, oil-resistant. |
| PA66 | A3UG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, halogen-free, low phosphorus content (approaching zero), oil-resistant. |
| PA66 | A3WG3 | Basf | ULTRAMID® | 15% glass fiber reinforced, injection molding grade, good stiffness, heat aging resistance, oil resistance. |
| PA66 | A3WG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, injection molding grade, excellent heat resistance, high stiffness, high dimensional stability, oil resistance. |
| PA66 | A3WG7 | Basf | ULTRAMID® | 35% glass fiber reinforced, injection molding grade, excellent heat resistance, oil resistance. |
| PA66 | A3Z | Basf | ULTRAMID® | Injection molding grade, excellent low-temperature impact resistance, oil resistance. |
| PA66 | A3HG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, injection molding grade, high dimensional stability, high stiffness. |
| PA66 | A3HG7 | Basf | ULTRAMID® | 35% glass fiber reinforced, injection molding grade, electrical insulation, high dimensional stability, high stiffness. |
| PA66 | A3K | Basf | ULTRAMID® | Injection molding grade, fast molding cycle, excellent flow, oil resistance. |
| PA66 | A3K R01 | Basf | ULTRAMID® | Good flowability, injection molding grade, electrical insulation, fast molding cycle. |
| PA66 | A3W2G10 BK20560 | Basf | ULTRAMID® | 50% glass fiber reinforced, injection molding grade, oil resistance. |
| PA66+PA6 | A3W2G6 BK20560 | Basf | ULTRAMID® | 30% glass fiber reinforced, injection molding grade, heat aging resistance, oil resistance. |
| PA66 | A3W | Basf | ULTRAMID® | Fast molding cycle, excellent flowability, heat aging resistance, oil resistance. |
| PA66 | A3WG10 | Basf | ULTRAMID® | 50% glass fiber reinforced, heat aging resistant, high stiffness, oil resistance. |
| PA66 | A3WG8 BK20560 | Basf | ULTRAMID® | 40% glass fiber reinforced, high heat resistance, high stiffness, high strength, oil resistance. |
| PA66 | A3WGM53 BK20560 | Basf | ULTRAMID® | 40% glass fiber/mineral reinforced, good dimensional stability, excellent surface finish, high stiffness, oil resistance. |
| PA66 | A3W Q601 | Basf | ULTRAMID® | Fast molding cycle, good flowability, heat aging resistance, oil resistance. |
| PA66 | A3X2G10 | Basf | ULTRAMID® | 50% glass fiber reinforced, flame retardant, excellent electrical properties, high stiffness, high strength, oil resistance. |
| PA66 | A3XZG5 | Basf | ULTRAMID® | 25% glass fiber reinforced, flame retardant, excellent impact strength, high dimensional stability, high stiffness, impact-modified, oil resistance. |
| PA66 | A3Z HP BK20465 | Basf | ULTRAMID® | Outstanding processability, heat stabilized, high flowability, high impact strength, oil resistance, ultra-high toughness. |
| PA66 | A4H | Basf | ULTRAMID® | Heat aging resistant, medium viscosity, oil resistance. |
| PA66 | A3EG6 EQ BK23189 | Basf | ULTRAMID® | 30% glass fiber reinforced, injection molding grade, electronics-grade, laser-sensitive. |
| PA66 | A3EG7 FC AQUA UN | Basf | ULTRAMID® | 35% glass fiber reinforced, food-contact grade. |
| PA66+PA610 | A3HG6 BALANCE R01 BK 23591 | Basf | ULTRAMID® | 30% glass fiber reinforced, calcium chloride resistant, hydrolysis resistant, stress cracking resistant. |
| PA66 | A3HG6 HR BK23591 | Basf | ULTRAMID® | 30% glass fiber reinforced, hydrolysis resistant, oil resistant. |
| PA66 | A3U42G6 | Basf | ULTRAMID® | 30% glass fiber reinforced, injection molding grade, halogen-free flame retardant, easy to color. |
| PA66 | A3WG10 HP BK23325 | Basf | ULTRAMID® | 50% glass fiber reinforced, injection molding grade, heat aging resistant, high stiffness. |
| PA66 | A3WG6 HRX BK23591 | Basf | ULTRAMID® | 30% glass fiber reinforced, injection molding grade, heat aging resistant, hydrolysis resistant. |
| PA66 | A3WG7 HP BK20560 | Basf | ULTRAMID® | 35% glass fiber reinforced, heat stabilized, injection molding grade, high flowability, oil resistance. |
| PA66 | A3WG7 HRX BK23591 | Basf | ULTRAMID® | 35% glass fiber reinforced, injection molding grade, hydrolysis resistant, heat aging resistant. |
| PA66 | A3WG7 LS BK23189 | Basf | ULTRAMID® | 35% glass fiber reinforced, injection molding grade, heat aging resistant, high stiffness, laser-sensitive. |
| PA66 | A4H R01 | Basf | ULTRAMID® | High heat aging resistance, medium viscosity, injection molding grade. |
| PA66 | A3U44G6 | Basf | ULTRAMID® | 40% glass fiber reinforced, injection molding grade, halogen-free flame retardant. |
| PA66 | 101F | Celanese | ZYTEL | Unreinforced Polyamide 66 |
| PA66 | 103HSL | Celanese | ZYTEL | Unreinforced, Heat Stabilized, Polyamide 66 |
| PA66 | 105F | Celanese | ZYTEL | Unreinforced, UV Stabilized, Polyamide 66 |
| PA66 | 135F | Celanese | ZYTEL | Unreinforced, Nucleated, Polyamide 66 |
| PA66 | FN718 | Celanese | ZYTEL | Flexible Polyamide 66 |
| PA66 | 70G43HSLA | Celanese | ZYTEL | 43% Glass Reinforced, Heat Stabilized, Polyamide 66 |
| PA66 | 70G35HSL | Celanese | ZYTEL | 35% Glass Reinforced, Heat Stabilized, Polyamide 66 |
| PA66 | 70G35HSLRA4 | Celanese | ZYTEL | 35% Glass Reinforced, Heat Stabilized, Hydrolysis Resistant, Polyamide 66 |
| PA66 | 80G14A | Celanese | ZYTEL | 14% Glass Reinforced, Toughened |
| PA66 | 80G25HS | Celanese | ZYTEL | 25% Glass Reinforced, Toughened, Heat Stabilized |
| PA66 | 80G33HS1L | Celanese | ZYTEL | 33% Glass Reinforced, Toughened, Heat Stabilized |
| PA66 | FR7026V0F | Celanese | ZYTEL | Unreinforced, Flame Retardant, Non-Halogenated, Heat Stabilized |
| PA66 | FR70M30V0 | Celanese | ZYTEL | 30% Mineral Reinforced, Flame Retardant |
| PA66 | E51HSB | Celanese | ZYTEL | Unreinforced, Heat Stabilized, High Viscosity |
| PA66 | HV125A | INVISTA | / | Excellent processability, high viscosity |
| PA66 | HV125AHSL | INVISTA | / | High viscosity, thermal stability, lubricated |
| PA66 | HV240A | INVISTA | / | Excellent processability, high viscosity |
| PA66 | HV240AHSL | INVISTA | / | High viscosity, thermal stability, lubricated |
| PA66 | HV360A | INVISTA | / | Excellent processability, high viscosity |
| PA66 | HV360AHSL | INVISTA | / | High viscosity, thermal stability, lubricated |
| PA66 | HV80A | INVISTA | / | Excellent processability, medium viscosity |
| PA66 | HV80AL | INVISTA | / | Excellent processability, medium viscosity |
| PA66 | U2501 | INVISTA | / | High flowability, low viscosity |
| PA66 | U2503 | INVISTA | / | High flowability, low viscosity |
| PA66 | U3200 | INVISTA | / | High flowability, low viscosity |
| PA66 | U3501 | INVISTA | / | Good colorability, excellent processability, high flow, low viscosity |
| PA66 | U3600 | INVISTA | / | Good colorability, excellent processability, high flow, low viscosity |
| PA66 | U3602 | INVISTA | / | Good colorability, excellent processability, high flow, low viscosity |
| PA66 | U3671 | INVISTA | / | Good colorability, high flow, low viscosity |
| PA66 | U4200 | INVISTA | / | Versatile, excellent processability, high flow, low viscosity |
| PA66 | U4201 | INVISTA | / | Versatile, high flow, low viscosity |
| PA66 | U4260FL | INVISTA | / | High flowability, high impact resistance, fast molding |
| PA66 | U4300 | INVISTA | / | Versatile, good flowability |
| PA66 | U4301 | INVISTA | / | Versatile, excellent processability, high flow, low viscosity |
| PA66 | U4500 | INVISTA | / | Versatile, excellent processability, high flow |
| PA66 | U4503 | INVISTA | / | Versatile, excellent processability, high flow, low viscosity |
| PA66 | U4591 | INVISTA | / | High flowability |
| PA66 | U4630HSL | INVISTA | / | Excellent flowability, good processability, thermal stability, good heat resistance, lubricated |
| PA66 | U4630HSL BKB01 | INVISTA | / | Excellent flowability, good processability, thermal stability, lubricated |
| PA66 | U4800 | INVISTA | / | Versatile, good color stability, excellent processability |
| PA66 | U4801 | INVISTA | / | Versatile, good color stability, excellent processability |
| PA66 | U4803 | INVISTA | / | Versatile, good color stability, excellent processability |
| PA66 | U4820L | INVISTA | / | Excellent processability, fast molding, versatile, easy demolding, lubricated |
| PA66 | U4840NL | INVISTA | / | Good processability, fast molding, easy demolding, lubricated |
| PA66 | U5000 | INVISTA | / | Good colorability, excellent processability, high flow, low viscosity |
| PA66 | U5101 | INVISTA | / | Versatile, good color stability, excellent processability |
What is PA66 Resin?
PA66 Resin (Polyamide 66), also known as Nylon 66, is a high-performance engineering thermoplastic. It is produced through polycondensation of hexamethylene diamine and adipic acid, forming a highly crystalline polymer structure. PA66 offers excellent mechanical strength, stiffness, heat resistance, abrasion resistance, and chemical stability. Widely used in automotive, electrical & electronics, industrial machinery, and consumer products.
Other Names
- Nylon 66
- Polyamide 66
- Engineering Nylon
- High-temperature Polyamide
Packaging
- 25kg bags
- jumbo bags
Appearance
- Natural color pellets (off-white / milky)
- Black pellets (carbon-reinforced or flame-retardant grades)
- Uniform cylindrical or lenticular granules
- Clean, dry, free-flowing resin pellets
HS Code
39081090
Key Properties
- High tensile strength and rigidity
- Excellent heat resistance and thermal stability
- Outstanding wear resistance and fatigue resistance
- Good chemical resistance to oils, fuels, and solvents
- Excellent electrical insulation properties
- Low creep under long-term mechanical load
- Good surface finish and moldability
Technical Data
| Property | Typical Value |
|---|---|
| Density (g/cm³) | 1.12 – 1.15 |
| Tensile Strength (MPa) | 75 – 95 |
| Flexural Modulus (MPa) | 2,500 – 3,200 |
| Izod Impact Strength (kJ/m²) | 6 – 12 |
| Heat Deflection Temp (°C) | 180 – 260 °C (reinforced grades) |
| Melt Flow Index (MFI) | 10 – 40 g/10 min (depending on grade) |
| Water Absorption (24h) | 1.0 – 1.5 % |
| Melting Point (°C) | Approx. 260 – 265 °C |
Applications
- Automotive: Engine covers, Intake manifolds, Cooling system components, Connectors and clips, Structural brackets
- Electrical & Electronics: Electrical connectors, Circuit breaker components, Coil bobbins, Terminal blocks, Insulation parts
- Industrial & Mechanical: Gears and bearings, Bushings and rollers, Pump housings, Conveyor components
- Consumer & General Industry: Power tool housings, Appliance parts, Fasteners, High-strength molded components
PA6 Resin Grades We Offer
- Injection molding grades
- Extrusion grades
- Glass fiber reinforced grades
- High flow grades
- Flame retardant grades
- Impact modified grades