Supply Various Grades of PBT pellets
111
What is PBT Resin?
PBT (Polybutylene Terephthalate) is a high-performance, semi-crystalline engineering thermoplastic known for its outstanding mechanical strength, thermal resistance, and electrical insulation properties. It offers excellent dimensional stability, low moisture absorption, and fast crystallization, making it ideal for automotive, electrical/electronic, industrial, and appliance applications where precision and durability are essential.
Other Names
- Polybutylene Terephthalate
- PBT Plastic Pellets
- PBT Engineering Resin
Packaging
- 25kg bags
- jumbo bags
Appearance
- Natural (off-white or ivory)
- Black or custom-colored grades available
HS Code
- 39079990
Key Properties of PBT Resin
- High mechanical strength and dimensional stability
- Excellent thermal resistance and electrical insulation
- Low moisture absorption and chemical resistance
- Good surface finish and moldability
- Fast processing cycle times for injection molding
Technical Data
| Property | General Grade |
|---|---|
| Density (g/cm³) | 1.30 – 1.55 g/cm³ |
| Tensile Strength (MPa) | 50 – 80 MPa |
| Flexural Modulus (MPa) | 2000 – 3000 MPa |
| Izod Impact Strength (J/m) | 40 – 80 J/m |
| Heat Deflection Temp (°C) | 120 – 210 °C) |
| Melt Flow Index (MFI, g/10min) | 10 – 60 (varies by grade) |
Note
Values are typical and may vary by specific grade. Please contact us for technical datasheets.
Applications of PBT Resin
- Automotive connectors, sensors, and housings
- Electrical & electronic components (switches, plugs)
- Appliance parts (fan blades, handles, enclosures)
- Industrial machinery components
- LED lighting fixtures and frames
PBT Resin Grades We Offer
- General-purpose grade
- Glass fiber reinforced grade
- Flame retardant (UL94 V-0) grade
- UV-stabilized grade