PC ABS Resin Plastic Alloy Pellets

Supply Various Grades of PC ABS pellets

TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PC ABSPC-545ChimeiWonderloyFlame retardant grade. Ultra-High heat, Non-brominated and non-chlorinated flame retardant, 1.2mm V-0, 2.5 mm 5VASet-top boxes, projectors, computers, communication equipment, consumer electronics products, video game consoles, networking products
PC ABSPC-510ChimeiWonderloyFlame retardant grade. High flow, Non-brominated and non-chlorinated flame retardant, 1.5mm V-0, 3.0mm 5VA. (TPP series)Set-top boxes, projectors, computers, communication equipment, consumer electronics products, video game consoles, networking products
PC ABSPC-540ChimeiWonderloyFlame retardant grade. High heat, Non-brominated and non-chlorinated flame retardant, 1.5mm V-0, 2.0 mm 5VB/2.5mm 5VASet-top boxes, projectors, computers, communication equipment, consumer electronics products, video game consoles, networking products
PC ABSPC-540AChimeiWonderloyFlame retardant grade. High heat, Non-brominated and non-chlorinated flame retardant, 1.5mm V-0, 2.0 mm 5VB, 2.5mm 5VASet-top boxes, projectors, computers, communication equipment, consumer electronics products, video game consoles, networking products
PC ABSPC-345ChimeiWonderloyGeneral purpose grade. High flow, 1.5mm HBAutomotive interior part/Consumer electronics product/High-end helmet/Mobile phone casing/General molding product
PC ABSPC-365ChimeiWonderloyGeneral purpose grade. Balanced type, 1.5mm HBAutomotive interior parts, consumer electronics products, high-end helmets, mobile phone casings, general molding products
PC ABSPC-385ChimeiWonderloyGeneral purpose grade. High heat, high impact, 1.5mm HBAutomotive interior parts, consumer electronics products, high-end helmets, mobile phone casings, general molding products
PC/ABS AlloyPC-330KZChi Mei (Zhenjiang)WonderloyGeneral Grade: Impact strength superior to ABS.Widely used for automotive components: navigation systems, decorative trim, truck door panels, etc.
PC/ABS AlloyPC-345KZChi Mei (Zhenjiang)WonderloyGeneral Grade. Impact strength and heat resistance superior to ABS.Decorative rings for kitchen appliances, headlight bases, tailgate trim panels, etc.
PC/ABS AlloyPC-365KZChi Mei (Zhenjiang)WonderloyGeneral Grade: Balanced mechanical strength and heat resistance.Navigation systems, central console bezels, A/C air vents, advertising display frames, etc.
PC/ABS AlloyPC-385KSChi Mei (Zhenjiang)WonderloyGeneral Grade: High impact strength, excellent low-temperature impact resistance, high heat distortion temperature;suitable for extrusion applications. Luggage and bags, safety helmets, etc.
PC/ABS AlloyPC-385KZChi Mei (Zhenjiang)WonderloyGeneral Grade. High impact strength and high heat distortion temperature.Automotive components, electronic product parts, etc.
PC/ABS AlloyPC-330KChi Mei (Zhenjiang)WonderloyLow-odor grade. Low VOC.Automotive interior components, electronic product housings, general molded parts, etc.
PC/ABS AlloyPC-345KChi Mei (Zhenjiang)WonderloyLow-odor grade. Low VOC.Automotive interior components, electronic product housings, general molded parts, etc.
PC/ABS AlloyPC-365KChi Mei (Zhenjiang)WonderloyLow-odor grade. Low VOC. Balanced mechanical strength.Automotive interior components, electronic product housings, general molded parts, etc.
PC/ABS AlloyPC-345KPChi Mei (Zhenjiang)WonderloyEleplating grade. Medium-to-high strength.Electroplated automotive parts, electroplated housings
PC/ABS AlloyPC-345PChi Mei (Zhenjiang)WonderloyEleplating grade. Excellent yield in water plating processes.Automotive door handles, etc.
PC/ABS AlloyPC-540HChi Mei (Zhenjiang)WonderloyFlame-retardant grade. High flow; V0 rating at 2.0 mm.3C digital products, laptop computers, networking and communication products
PC/ABS AlloyPC-540KChi Mei (Zhenjiang)WonderloyFlame-retardant grade. High heat resistance; V0 rating at 1.5 mm; RTI certified; low-temperature resistant.Networking and communication products, self-balancing scooters
PC/ABS AlloyPC-550KChi Mei (Zhenjiang)WonderloyFlame-retardant grade. High heat resistance; V-0 rating at 1.5 mm, 5VB rating at 2.0 mm; halogen-free flame-retardant material.Set-top boxes, projectors, monitor front bezels, 6C digital products, transformers, video game consoles, small tablet computers, networking and communication products
PC/ABS AlloyPC-6201Chi Mei (Zhenjiang)WonderloyFlame-retardant grade. High heat resistance; V0 rating at 3.0 mm; resistant to low-temperature impact.Miners’ safety helmets, communication products
TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PC ABSAC3100FORMOSA (FCFC)TAIRILOYSelf Extinguishing Grade. Flame retardant,Halogen freeHousehold appliances, 3C electronic products, notebook computers, Netcom products, computer peripheral products
PC ABSAC2300FORMOSA (FCFC)TAIRILOYGeneral Purpose Grade. Metal platingAuto parts, household appliances, 3C electronic products and household goods casings such as wheel covers, handles, Portable storage device
PC ABSAC2000FORMOSA (FCFC)TAIRILOYGeneral Purpose Grade. High impactAuto parts, household appliances, 3C electronic products and houseware shells such as tail lights, cameras, helmets, tablet PC
PC ABSAC2500FORMOSA (FCFC)TAIRILOYGeneral Purpose Grade. Heat resistantAuto parts, household appliances, 3C electronic products,instrument panel. grill ,bathroom accessories, electrical control knobs
PC ABSAC3250FORMOSA (FCFC)TAIRILOYSelf Extinguishing Grade. Flame retardant,Halogen freeNotebook casings, 3C products, Electrical equipment, Dashboard
PC ABSAC3300FORMOSA (FCFC)TAIRILOYSelf Extinguishing Grade. Flame retardant,Halogen freeOA equipment, 3C electronic products, Multi-functional peripheral
TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
FR PC/ABSC2800SabicCYCOLOYStandard grade, non-chlorinated/brominated flame retardant, UL V0 & 5VB.Business equipment, monitors, and enclosures.
FR PC/ABSC2950SabicCYCOLOYHigh heat grade, non-chlorinated/brominated flame retardant, UL V0 & 5VB.Appliances, lighting, and electrical components.
FR PC/ABSC2950HFSabicCYCOLOYHigh heat grade with improved processability, UL V0 & 5VA/B.Appliances, lighting, and electrical components.
FR PC/ABSC2951SabicCYCOLOYHigh heat, non-chlorinated/brominated, UL 94 5VA@3.0mm.Demanding electrical applications.
FR PC/ABSC3650SabicCYCOLOYGeneral purpose, flame retardant, UL V0 & 5VB, suitable for injection molding or sheet forming.Cable channels, meets DIN VDE 0472/815 halogen-free standards.
FR PC/ABSC6200SabicCYCOLOYBalanced heat, flow, and impact performance, non-chlorinated/brominated flame retardant.Various application needs.
FR PC/ABSC6600SabicCYCOLOYFlame retardant, balanced flow, impact, hydrolytic stability, UL 94 V0@1.5mm, 5VB@2.0mm.Good chemical resistance, suitable for opaque colors.
FR PC/ABSC7230PSabicCYCOLOYMineral-filled, flame retardant, good rigidity with balanced flow and impact.Various electrical and industrial applications.
FR PC/ABSC9210SabicCYCOLOYImpact modified, heat resistant, non-chlorinated/brominated, UL 94 V0.Wide variety of large-sized applications.
FR PC/ABSCE3510SabicCYCOLOYHigh impact, flame retardant, UL 94 V0@1.5mm, suitable for injection molding and extrusion.Applications without chlorine/bromine.
FR PC/ABSCM6140SabicCYCOLOYMineral-filled, high modulus, low warpage, UL 94 V0@0.8mm, 5VB@1.5mm.Thin wall applications.
FR PC/ABSCM6210SabicCYCOLOYHigh impact, mineral-filled, UL 94 V0@1.5mm.Wide range of electrical applications.
FR PC/ABSCM6220SabicCYCOLOYHigh modulus (6GPa), low warpage, flame resistant for thin walls.Electrical housings and thin wall components.
FR PC/ABSCM6240SabicCYCOLOYHigh modulus, low warpage, UL 94 V0@0.8mm, 5VB@1.5mm.Thin wall applications.
FR PC/ABSCY5025SabicCYCOLOYGeneral-purpose thin wall flame retardant, UL V0 & 5VB.Thin wall applications.
FR PC/ABSCY6025SabicCYCOLOYStandard thin wall flame retardant, UL V0 & 5VB.Thin wall injection molding applications.
FR PC/ABSCY6110SabicCYCOLOYImpact modified, high flow, UL 94 V0@1.5mm, 5VB@2.5mm.Used extensively in thin wall and large-size components.
FR PC/ABSCY6120SabicCYCOLOYGood flame retardancy, flow properties, UL 94 V0@1.2mm.Thin wall applications.
FR PC/ABSCY6310SabicCYCOLOYHigh flow, heat resistant, UL 94 V0@1.5mm, 5VA@2.9mm, 5VB@2.3mm.Large-sized applications.
FR PC/ABSCY6414SabicCYCOLOYMedium flow, high heat, UL 94 V0@1.2mm, 5VB@2.5mm.Injection molding applications.
PC/ABSC1200HFSabicCYCOLOYExcellent flow, impact, low-temperature ductility, high heat resistance.General-purpose applications.
PC/ABSC4210HFSabicCYCOLOY10% glass-filled, high flow, high heat resistance, good strength.Structural applications requiring rigidity.
PC/ABSC4220SabicCYCOLOY20% glass-filled, excellent heat resistance and strength.High-rigidity applications.
PC/ABSCM8622SabicCYCOLOYHigh heat, low thermal expansion, good modulus and appearance.Electrical and appearance-focused applications.
PC/ABSCM8823SabicCYCOLOYHigh heat, low thermal expansion, good modulus and aesthetics.Electrical and appearance-focused applications.
PC/ABSCP8320SabicCYCOLOYMedium heat, suitable for electroplating.Automotive plating applications.
PC/ABSCY8630SabicCYCOLOYHeat-resistant PC/ABS for automotive.Automotive applications.
PC/ABSHC1104HFSabicCYCOLOYHigh heat resistance, excellent flow and impact performance.General heat and impact-resistant applications.
PC/ABSHC1204HFSabicCYCOLOYHigh heat resistance, biocompatible for medical and pharmaceutical use.Medical devices, pharmaceutical applications.
PC/ABSLG9000SabicCYCOLOYLow gloss PC/ABS.Automotive interiors or low gloss applications.
PC/ABSMC1300SabicCYCOLOYHigh impact, excellent flow, plating and painting capable.Plating and painting applications.
PC/ABSMC8002SabicCYCOLOYLow viscosity, high toughness.General-purpose injection molding.
PC/ABSMC8100SabicCYCOLOYExtrusion and blow molding grade.Extrusion and blow molding applications.
PC/ABSMC8800SabicCYCOLOYHigh heat, high impact, low thermal expansion.Structural applications with high heat requirements.
PC/ABSXCM830SabicCYCOLOY8% talc-filled, high stiffness and impact performance.Applications requiring rigidity and impact resistance.
PC/ABSXCY620HFSabicCYCOLOYHigh flow and high heat resistance.Electrical components.
PC/ABSXCY620SabicCYCOLOYExcellent hydrolytic stability.Electrical components and general requirements.
PC/ABSXCY620SSabicCYCOLOYStandard black and natural colors, excellent hydrolytic stability.Electrical components.
Type Grade No. Manufacturer Brand Grade/Features Use/Applications
PC ABS 2953 Covestro Bayblend Electroplating Grade. Vicat/B 120 temperature = 113 °C Injection molding; Electroplating
PC ABS FR3020 Covestro Bayblend Flame retardant grade. 5 % mineral filled;Vicat/B 120 temperature = 103 °C; HDT/A ≥ 85 °C; very good UL recognition in small wall thicknesses (V-0 at 0.75 mm); low smoke density Injection molding; Thin-wall applications
PC ABS FR3021 Covestro Bayblend Flame retardant grade. 15 % mineral filled;Vicat/B 120 temperature = 98 °C; high stiffness; tensile modulus = 4800 MPa; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm Injection molding
PC ABS FR3010 RE Covestro Bayblend Flame retardant grade. Vicat/B 120 temperature = 110 °C; increased heat resistance; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; improved chemical resistance and stress cracking behavior Injection molding
PC ABS FR3021 RE Covestro Bayblend Flame retardant grade. 15 % mineral filled; Vicat/B 120 temperature = 98 °C; high stiffness; tensile modulus = 4800 MPa; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm Injection molding
PC ABS T45 PG Covestro Bayblend Electroplating grade. Vicat/B 120 temperature = 112 °C. Impact resistant Injection molding; Electroplating
PC ABS T65 HI Covestro Bayblend high impact grade. Vicat/B 120 temperature = 120 °C; grade with improved low-temperature impact strength and chemical resistance Injection molding; Automotive parts; Also suitable for extrusion/extrusion blow molding and electroplating applications
PC ABS T65 PG Covestro Bayblend Electroplating grade. Vicat/B 120 temperature = 120 °C; easy flowing; good heat resistance Injection molding; Electroplating
PC ABS T80 XG Covestro Bayblend General Purpose Grade. Vicat/B 120 temperature = 130 °C; excellent flow; optimized surface quality for metallization (steam treatment); Impact resistant Injection molding
PC ABS T85 HG Covestro Bayblend General Purpose Grade. Vicat/B 120 temperature = 130 °C; easy flowing; high gloss; brilliant colors; Impact resistant, Heat resistant Injection molding
PC ABS T90 XG Covestro Bayblend General Purpose Grade. Vicat/B 120 temperature = 130 °C; easy flowing; high gloss; brilliant colors; Impact resistant, Heat resistant Injection molding
PC ABS T95 MF Covestro Bayblend Medium Flow Grade.9 % mineral filled; Vicat/B 120 temperature = 142 °C; very good heat resistance; reduced coefficient of thermal expansion; tensile modulus = 3350 MPa; Dimensionally stable, Heat resistant Injection molding
PC ABS T45 PG RE Covestro Bayblend Electroplating grade.Vicat/B 120 temperature = 112 °C;Impact resistant, CQ renewable attributed Injection molding; Electroplating
PC ABS T70 X RE Covestro Bayblend General Purpose Grade. Vicat/B 120 temperature = 124 °C; good injection molding processing behaviour (easy flowing); excellent long-term ageing behaviour under humid conditions; good painting performance; improved chemical resistance; low VOC emissions and odour Injection molding; General purpose
PC ABS T85 XF RE Covestro Bayblend High flow grade. Vicat/B 120 temperature = 130 °C; improved flow compared with Bayblend® T85; Impact resistant, CQ renewable attributed, Heat resistant Injection molding
PC ABS FR1514 Covestro Bayblend Flame retardant grade.Heat resistant. Vicat/B 120 temperature = 136 °C; ball indentation temperature ≥ 125 °C; UL recognition 94 V-0 at 1.5 mm Injection molding; Supporting material for energized parts
PC ABS FR3001 Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 103 °C; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; Flame retardant Injection molding
PC ABS FR3002 Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 99 °C; UL recognition 94 V-0 (1.0 mm); glow wire temperature (GWFI): 960 °C at 2.0 mm Injection molding; Notebooks and thin-wall applications
PC ABS FR3008 Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 103 °C; improved chemical resistance; HDT/A ≥ 85 °C; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; good light stability Injection molding
PC ABS FR3009 Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 103 °C; UL recognition 94 5VB at 1.8 mm; Improved hydrolysis resistance Injection molding
PC ABS FR3013 Covestro Bayblend Flame Retardant Grade. impact modified; easy flowing; Vicat/B 120 temperature = 95 °C Injection molding; Information technology
PC ABS FR3025 Covestro Bayblend Flame Retardant Grade. impact modified; mineral filled; Vicat/B 120 temperature = 102 °C; UL recognition 94 V-0 at 1.2 mm; low warpage; improved stiffness and surface quality Injection molding; Notebooks and thinwall applications
PC ABS FR3030 Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 115°C; good extrusion and vacuum-forming behaviour; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 1.0 mm Extrusion
PC ABS FR630 GR Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 108 °C; UL recognition 94 V-0 at 1.5 mm Injection molding; Housing; Information technology
PC ABS FR3000 HI Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 97 °C; compared to Bayblend® FR3000 improved chemical resistance and stress cracking behavior; UL recognition 94 V-0 at 1.5 mm; Impact resistant, Chemical resistant Injection molding
PC ABS FR3006 HF Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 108 °C; easy flowing version of Bayblend® FR3006; increased heat resistance; UL recognition 94 V-1 at 1.5 mm, V-0 at 1.8 mm and 5VB at 1.8 mm Injection molding
PC ABS FR3008 HR Covestro Bayblend Flame Retardant Grade. impact modified;Vicat/B 120 temperature = 103 °C; very good hydrolysis resistance Injection molding
PC ABS FR3008 RE Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 103 °C; improved chemical resistance; HDT/A ≥ 85 °C; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; good light stability Injection molding
PC ABS FR3010 HF Covestro Bayblend Flame Retardant Grade. easy flowing; Vicat/B 120 temperature = 108 °C; UL recognition 94 V-0 at 1.5 mm; glow wire temperature (GWFI): 960 °C at 2.0 mm; optimized processability; good light stability Injection molding
PC ABS FR3021 GR Covestro Bayblend Flame Retardant Grade. 15 % mineral filled;Vicat/B 120 temperature = 97 °C; increased stiffness; tensile modulus = 4600 MPa; UL recognition 94 V-0 at 1.5 mm; Dimensionally stable, Flame retardant, CQ mechanical recycled Injection molding
PC ABS FR3040 R35 Covestro Bayblend Flame Retardant Grade. CQ mechanical recycled Injection molding; Notebooks and thin-wall applications
PC ABS FR3110 TV Covestro Bayblend Flame Retardant Grade. easy flowing; Vicat/B 120 temperature = 110 °C; increased heat resistance; UL recognition 94 V-0 at 1.5 mm Injection molding
PC ABS FR3200 TV Covestro Bayblend Flame Retardant Grade. easy flowing; Vicat/B 120 temperature = 96 °C; UL recognition 94 V-0 at 1.2 mm Injection molding
PC ABS FR3210 TV Covestro Bayblend Flame Retardant Grade. easy flowing; Vicat/B 120 temperature = 93 °C; improved surface quality; UL recognition 94 V-0 at 1.2 mm Injection molding
PC ABS FR3311 TV Covestro Bayblend Flame Retardant Grade. 15 % glass fibre reinforced;easy flowing; Vicat/B 120 temperature = 96 °C; UL recognition 94 V-1 at 1.2 mm and V-0 at 1.5 mm Injection molding
PC ABS M301 FR Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 105 °C; Manufactured according to GMP; tested only according to ISO 10993-5 and ISO 10993-10 for contact with uncompromised skin only Injection molding; Electrical and electronic devices
PC ABS FR3020 W BBS910 Covestro Bayblend Flame Retardant Grade. impact modified; 5 % mineral filled; flame retardant; UV-stabilized; Vicat/B 120 temperature = 102 °C; UL recognition 94 V-0 (0.6mm); low smoke density Injection molding
PC ABS FR3040 W RE Covestro Bayblend Flame Retardant Grade.impact modified; flame retardant; CQ renewable attributed, CQ mechanical recycled Injection molding; Notebooks and thin-wall applications
PC ABS M750 Covestro Bayblend (PC+ABS) blend; Vicat/B 120 temperature = 126 °C; meet certain requirements of ISO Standard 10993-1 Injection molding; Medical devices
PC ABS M303 FR Covestro Bayblend Flame Retardant Grade. Vicat/B 120 temperature = 115 °C; Manufactured according to GMP; tested only according to ISO 10993-5 and ISO 10993-10 for contact with uncompromised skin only Injection molding; Extrusion; Electrical and electronic devices
PC ABS M850 XF Covestro Bayblend (PC+ABS) blend; easy flowing; Vicat/B 120 temperature = 131 °C; meet certain requirements of ISO Standard 10993-1 Injection molding; Medical devices
PC ABS M750 RE CQ Covestro Bayblend General Purpose Grade. Vicat/B 120 temperature = 126 °C; meet certain requirements of ISO Standard 10993-1;Medical, CQ renewable attributed Injection molding; Medical devices
PC ABS M850 XF RE Covestro Bayblend easy flowing; Vicat/B 120 temperature = 131 °C; meet certain requirements of ISO Standard 10993-1; Medical, CQ renewable attributed Injection molding; Medical devices
TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PC ABS3016Suke Plastics/Flame Retardant Grade. Halogen-free, High impactElectrical &electronic, Office supplies, Router
PC ABS3016GLSuke Plastics/Flame retardant grade. Halogen-free, High fluidity.Electrical &electronic, Office supplies, Router.
PC ABS3016NHSuke Plastics/Flame retardant grade. Halogen-free, Excellent chemical resistance.Electrical &electronic, Office supplies, Bluetooth headset.
PC ABS3016NWSuke Plastics/Flame Retardant Grade. Halogen-free, High temperature resistance.Electrical &electronic, Office supplies, Bluetooth headset, Tablet
PC ABS3020Suke Plastics/Flame retardant grade. Halogen-free, High flame retardancy.Electrical &electronic, Office supplies.
PC ABS3040Suke Plastics/Flame retardant grade. Halogen-free, Good comprehensive performance.Electrical &electronic, Office supplies, POS machine.
PC ABS1030Suke Plastics/General Purpose Grade. Good comprehensive performanceElectrical &electronic, Office supplies
PC ABS1045Suke Plastics/General Purpose Grade. Good comprehensive performanceElectrical &electronic, Office supplies
PC ABS1065Suke Plastics/General Purpose Grade. Good comprehensive performanceElectrical &electronic, Office supplies
PC ABSD535Suke Plastics/General Purpose Grade. Good comprehensive performanceElectrical &electronic, Office supplies
PC ABSD555Suke Plastics/General Purpose Grade. Good comprehensive performanceElectrical &electronic, Office supplies
PC ABSD570Suke Plastics/General Purpose Grade. Good comprehensive performanceElectrical &electronic, Office supplies

What is PC ABS Resin?

PC/ABS resin is a thermoplastic alloy made by blending Polycarbonate (PC) and Acrylonitrile Butadiene Styrene (ABS). This combination results in a material that offers the excellent toughness, heat resistance, and rigidity of PC with the processability and impact strength of ABS. It is widely used in industries that require high-performance plastic with superior mechanical and thermal properties.

Other Names

  • PC+ABS Alloy
  • PC/ABS Blend
  • PC ABS Plastic Pellets

Packaging

  • 25kg bags
  • jumbo bags

Appearance

  • Opaque or semi-transparent granules
  • Typically off-white, beige, or customized colors

HS Code

39079990

Key Properties of PC ABS Resin

Technical Data

PropertyGeneral Grade
Density (g/cm³)1.10-1.20
Tensile Strength (MPa)45-60
Flexural Modulus (MPa)2000-2500
Izod Impact Strength400-800 J/m
Heat Deflection Temp (°C)90-120
Melt Flow Index (MFI)10-30 g/10min (230°C/3.8kg)

Applications of PC ABS

PC ABS Resin Grades We Offer

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.