PC/ASA alloy exists to solve one problem that no other common engineering plastic solves as economically: unpainted outdoor durability with engineering-grade toughness and heat resistance.
PC/ABS fails outdoors within a couple of years because the butadiene rubber in ABS oxidizes under UV. Substituting ASA — an acrylic rubber that does not have this vulnerability — produces an alloy that keeps PC’s impact strength and heat resistance while surviving a decade or more of direct sun exposure without paint. If your part must stay outdoors, stay strong, and not be painted, PC/ASA is the material to evaluate first. Its weaknesses are cost (above PC/ABS) and chemical resistance (still poor against fuels and solvents).
This is the flagship material of the PC alloy family for exterior applications, and it is a category where peer content is essentially absent. This guide covers what PC/ASA is, why ASA makes the difference, how it performs, and where it earns its place.
1. What Is PC/ASA?
PC/ASA is a thermoplastic alloy of polycarbonate (PC) and acrylate-styrene-acrylonitrile (ASA). Structurally it is the weathering-resistant sibling of PC/ABS: the same amorphous blend architecture, with the butadiene rubber of ABS replaced by an acrylic rubber.
| Component | Role | Key Property |
| PC | Continuous matrix | Impact, heat resistance, toughness |
| ASA | Dispersed phase | UV resistance, surface quality, processability |
| Compatibilizer | Interface | Phase stability, property retention |
| Stabilizer package | Durability | UV, thermal, and color stabilization |
The substitution of ASA for ABS is the whole point. ABS contains polybutadiene rubber, whose backbone has residual double bonds. Those double bonds are attacked by ultraviolet light, and the oxidation products cause the characteristic yellowing, chalking, and embrittlement of weathered ABS. ASA replaces polybutadiene with an acrylic rubber (typically a butyl acrylate copolymer) that has a saturated backbone and therefore no UV-vulnerable double bonds. The result is a rubber phase that survives sunlight.
| Feature | ABS Phase | ASA Phase |
| Rubber type | Polybutadiene | Acrylate (butyl acrylate) |
| Backbone | Unsaturated (C=C) | Saturated |
| UV stability | Poor | Excellent |
| Weatherability | 1–2 years outdoors | 10+ years outdoors |
| Cost | Lower | Higher |
| Impact | Higher | Comparable |
Why the alloy rather than plain ASA. ASA alone is a useful outdoor material but its heat resistance and impact strength are modest. Blending it with PC raises both, producing a material that can carry structural loads and survive elevated temperatures while staying weather-resistant. The alloy is the point — plain ASA is for profiles and cladding, PC/ASA is for structural exterior parts.
2. Weathering: The Reason for the Material
The weathering performance difference is not incremental. It is the difference between a two-year part and a ten-year part.
| Material | Outdoor Service Without Paint | Failure Mechanism |
| ABS | 1–2 years | Butadiene oxidation, yellowing, chalking |
| PC/ABS | 2–4 years (with UV package) | Residual butadiene vulnerability |
| ASA | 10+ years | Acrylic rubber stability |
| PC/ASA | 10+ years | Acrylic rubber stability |
| PMMA | 20+ years | Inherently UV stable |
| PC (UV-stabilized) | 5–10 years | UV absorber depletion |
How weathering damage progresses. The failure sequence in ABS-based materials is consistent: color shift first (yellowing), then surface chalking as degraded material reaches the surface, then loss of gloss, and finally embrittlement and cracking as degradation penetrates deeper. The damage is progressive and irreversible — a weathered ABS part cannot be restored.
Why PC/ASA does not follow this sequence. Because the acrylic rubber has no unsaturated bonds, the primary attack site is absent. The material still needs a UV absorber package to protect the PC matrix and the surface, but the failure mechanism that destroys ABS is not present. Degradation, when it occurs, is far slower and is dominated by surface effects rather than bulk embrittlement.
| Exposure | ABS | PC/ABS | PC/ASA |
| 1,000 h QUV | Visible yellowing | Slight yellowing | Minimal change |
| 2,000 h QUV | Strong yellowing, chalking | Moderate yellowing | Slight change |
| 5,000 h QUV | Severe degradation | Significant, gloss loss | Minor change |
| 10,000 h QUV | Failed | Failed | Acceptable |
The values are indicative rather than universal — the exact outcome depends on the stabilization package and the exposure conditions — but the pattern is robust and is the basis for specifying PC/ASA in the first place.
Accelerated weathering tests you should see in a data sheet:
| Test | Standard | What It Simulates |
| QUV / UV fluorescent | ASTM G154 | UV plus condensation cycling |
| Xenon-arc | ISO 4892-2 / ASTM G155 | Full-spectrum sunlight |
| Carbon-arc | ASTM G153 | Legacy standard |
| Florida exposure | ASTM D1435 | Real-world benchmark |
| Color change | ISO 7724 / ASTM D2244 | ΔE measurement |
Always request the exposure condition and the measured property, not just a pass statement. “Passed 2,000 hours QUV” is meaningless without knowing whether the measured property was color (ΔE), gloss retention, or impact retention — and the acceptance threshold. A part can retain acceptable color while losing most of its impact strength.
3. Property Profile
| Property | PC/ASA | Test Standard |
| Density | 1.13–1.17 g/cm³ | ISO 1183 |
| Tensile strength | 50–58 MPa | ISO 527 |
| Tensile modulus | 2,200–2,500 MPa | ISO 527 |
| Notched Izod, 23 °C | 40–60 kJ/m² | ISO 180 |
| Notched Izod, −30 °C | 10–20 kJ/m² | ISO 180 |
| HDT at 1.8 MPa | 95–110 °C | ISO 75-2 |
| Vicat softening | 110–125 °C | ISO 306 |
| CLTE | 70–85 µm/m·K | ISO 11359 |
| Water absorption | 0.2–0.3% | ISO 62 |
| Density range | 1.13–1.17 g/cm³ | ISO 1183 |
The property profile is close to PC/ABS with better weathering. Impact, heat resistance, and stiffness are comparable; the difference is durability. This is why PC/ASA is usually specified by substituting for an existing PC/ABS part that failed outdoors, rather than by designing from scratch — the mechanical design carries over and only the weathering changes.
| Property | PC/ABS | PC/ASA | Difference |
| Outdoor life | 2–4 years | 10+ years | Major |
| Impact | Comparable | Comparable | Minimal |
| Heat resistance | Comparable | Comparable | Minimal |
| Cost | Lower | 20–40% higher | Moderate |
| Paint requirement | Needed outdoors | Not needed | Major |
4. Coextrusion and Cap Layer Options
A common and economical approach is to use a thin PC/ASA or ASA cap layer over a lower-cost substrate, capturing the weathering benefit at the cost of the substrate.
| Structure | Weathering | Cost | Use |
| Solid PC/ASA | Full thickness | Highest | Structural exterior parts |
| PC/ASA cap over PC/ABS | Cap provides UV protection | Medium | Large panels, cost-sensitive |
| ASA cap over ABS | Cap provides UV protection | Low | Profiles, sheet |
| ASA cap over PVC | Cap provides UV protection | Low | Window profiles |
The cap layer thickness is the design variable. A cap layer of roughly 0.3–0.5 mm is sufficient to provide the weathering protection in most applications, because UV degradation is a surface phenomenon and the cap absorbs the UV before it reaches the substrate. Thinner caps risk incomplete coverage; thicker caps add cost without additional benefit.
Coextrusion requires bond compatibility. The cap and substrate must adhere throughout the service life and through thermal cycling. ASA over ABS and ASA over PVC are established systems; PC/ASA over PC/ABS requires a compatible tie layer or matched formulations. Verify bond strength with a peel test as part of the qualification.
5. Applications
| Application | Why PC/ASA | Grade Direction |
| Automotive exterior trim | Unpainted durability | High-impact, UV-stabilized |
| EV charging station housings | Outdoor, structural, aesthetic | UV-stabilized, FR option |
| Outdoor electrical enclosures | Weather plus impact | UV-stabilized, FR |
| Roofing and window components | Long-term exterior | Extrusion, UV package |
| Outdoor furniture | Weather plus impact | Impact-modified |
| Solar panel frames and junction boxes | UV plus heat | UV-stabilized, FR |
| Agricultural equipment housings | Outdoor plus chemical | UV plus chemical resistance |
| Signs and display structures | Aesthetic durability | Color-stable grades |
EV charging infrastructure is the fastest-growing application. A charging station housing sits outdoors for its whole life, must survive impact and weather, must resist heat from the electronics inside and sun outside, and is usually specified with a flame-retardant requirement. PC/ASA meets all of these without paint, which is significant because painting a large outdoor housing adds cost and introduces a coating that can fail independently of the substrate.
| Requirement | PC/ASA Fit |
| Outdoor 10+ years | Excellent |
| Unpainted | Excellent |
| Impact resistant | Excellent |
| Heat resistant to ~100 °C | Good |
| Flame retardant option | Available |
| Fuel/oil resistance | Poor |
| Cost | Moderate–high |
The one application PC/ASA cannot serve is one that contacts fuel, oil, or solvent. It inherits PC’s poor chemical resistance and is unsuitable for any part that touches automotive fluids. For those, PC/PBT or PBT is the correct family.
6. Processing
PC/ASA processes much like PC/ABS, with the same key discipline: drying.
| Parameter | Recommendation | Notes |
| Drying temperature | 100–110 °C | Desiccant dryer |
| Drying time | 3–4 h | To ≤0.02% moisture |
| Melt temperature | 250–280 °C | Avoid exceeding 290 °C |
| Mold temperature | 60–90 °C | Higher for surface quality |
| Injection pressure | Moderate–high | Standard PC alloy range |
| Shrinkage | 0.5–0.7% | Per grade |
| Regrind | 10–20% | Verify color and impact |
Drying is non-negotiable. Like all PC alloys, PC/ASA hydrolyzes if molded wet. Moisture above 0.02% causes splay, silver streaks, and permanent molecular-weight loss. Dry in a desiccant dryer.
Melt temperature control protects the color. PC/ASA is usually a color-critical material — an exterior trim part must match a color standard. Excessive melt temperature degrades the polymer and shifts the color, and the shift is irreversible. Keep melt temperature within the supplier’s window and minimize residence time.
| Defect | Cause | Fix |
| Splay / silver streaks | Moisture | Verify drying to ≤0.02% |
| Color shift | Excessive melt temperature | Lower temperature, shorten residence |
| Flow lines | Low mold temperature | Raise mold temperature |
| Weak weld lines | Low temperature, poor venting | Raise temperature, add vents |
| Warpage | Uneven cooling, anisotropic shrinkage | Balance cooling and gating |
| Gloss variation | Mold temperature variation | Uniform mold temperature |
7. PC/ASA vs Competing Materials
7.1 PC/ASA vs PC/ABS
The direct comparison, and the substitution most often made.
| Factor | PC/ABS | PC/ASA |
| Outdoor life | 2–4 years (with UV package) | 10+ years |
| Cost | Lower | 20–40% higher |
| Paint required outdoors | Yes | No |
| Mechanical properties | Comparable | Comparable |
| Chemical resistance | Poor | Poor |
The calculation is straightforward: if the part is outdoors and unpainted, PC/ASA’s premium is usually cheaper than the paint system PC/ABS would require, and it eliminates a coating that can fail independently. If the part is indoor or painted, PC/ABS is the economical choice.
7.2 PC/ASA vs ASA
| Factor | ASA | PC/ASA |
| Impact strength | Moderate | High |
| Heat resistance | Moderate | Higher |
| Cost | Lower | Higher |
| Typical use | Profiles, cladding, sheet | Structural exterior parts |
ASA is for large, semi-structural forms where toughness and heat resistance are less demanding — siding, profiles, and sheet. PC/ASA is for parts that must carry load, resist impact, and survive heat.
7.3 PC/ASA vs PMMA
PMMA has the best weathering of any common transparent plastic — 20+ years — but it is brittle and has low impact strength. PC/ASA trades some weathering performance for far higher toughness. For a part that must survive an impact, PC/ASA wins; for a purely decorative panel, PMMA can be better.
7.4 PC/ASA vs PA/PPE
PA/PPE (modified polyphenylene ether) is another outdoor-capable engineering plastic with good heat resistance and better chemical resistance than PC/ASA in some media. It is typically more expensive and harder to process, and it does not have PC/ASA’s aesthetic surface quality. Both are valid; selection depends on the specific requirement.
7.5 Comparison Summary
| Material | Outdoor Life | Impact | Heat | Cost |
| PC/ABS | 2–4 years | High | Good | Low |
| PC/ASA | 10+ years | High | Good | Medium |
| ASA | 10+ years | Moderate | Moderate | Low–medium |
| PMMA | 20+ years | Low | Moderate | Medium |
| PA/PPE | 10+ years | High | Very good | High |
| PC (UV-stab.) | 5–10 years | High | Good | Medium |
7.6 The Substitution Rules
Because PC/ASA is most often reached by substituting an existing material, it is worth stating the substitution logic explicitly, in both directions.
Substituting PC/ASA for PC/ABS in an outdoor part:
| Step | Action | What to Verify |
| 1 | Confirm the failure mode is UV | Check for yellowing and chalking, not chemical attack |
| 2 | Verify mechanical equivalence | Compare notched Izod and HDT |
| 3 | Check thermal expansion | CLTE is similar but confirm |
| 4 | Confirm no chemical contact | PC/ASA has the same weakness as PC/ABS |
| 5 | Re-evaluate the paint decision | Paint may no longer be needed |
| 6 | Confirm color match under weathering | ΔE data, not initial color |
Substituting PC/ABS for PC/ASA in an indoor part:
This substitution is a legitimate cost reduction and the logic is the reverse of the above. The one check that matters is whether the part is truly indoor — a part near a window, in a vehicle, or in a partially covered location receives meaningful UV even if it is not directly rained on. When in doubt, verify with a light-exposure assessment rather than assuming.
| Substitution | Direction | Risk |
| PC/ABS → PC/ASA | Upgrading for outdoor use | Cost increases; mechanical design unchanged |
| PC/ASA → PC/ABS | Downgrading for indoor use | Field failure if UV exposure was underestimated |
| PC/ASA → ASA | Cost reduction | Impact and heat resistance both drop |
| PC/ASA → PMMA | Appearance upgrade | Severe impact loss |
| PC/ASA → PA/PPE | Heat upgrade | Cost increases; processing changes |
The downgrade direction is the dangerous one. An engineer who sees “PC/ASA costs 30% more, this part is indoors, switch to PC/ABS” may be correct — or may be removing the only thing preventing a field failure, if the part sits near a window or under a translucent canopy. Establish the actual UV exposure before making the change.
7.7 What the Grade Price Actually Buys
A first-pass cost model helps decide whether PC/ASA is justified.
| Cost Element | PC/ABS + Paint | PC/ASA Unpainted |
| Resin cost | Baseline | +20–40% |
| Paint material | Added | None |
| Paint process | Added (labor, line, energy) | None |
| Paint defects / rework | Added | None |
| Substrate UV package | Required | Included |
| Repaint risk over life | Present | Absent |
| Effective cost | Higher in most unpainted outdoor cases | Lower |
The arithmetic favors PC/ASA in unpainted outdoor applications because the paint system carries material cost, process cost, defect risk, and a durability risk of its own — a coating that can chip, fade, or delaminate independently of the substrate. Removing the paint removes all four. Where the part is painted anyway for appearance reasons, the calculation reverses and PC/ABS is the economical choice.
8. Design Guidance
| Consideration | Guidance | Reason |
| Wall thickness | Uniform where possible | Avoid warp and sinks |
| Radii | Generous, ≥0.5× wall | Stress concentration |
| Ribs | ≤60% of wall thickness | Avoid sink marks |
| CLTE | 70–85 µm/m·K | Design gaps for thermal movement |
| Attachment | Fix one point, float others | Thermal expansion |
| UV exposure | Stabilized grade | Substrate protection |
| Color matching | Verify after processing | Melt temperature affects color |
| Chemical contact | Avoid fuels, oils, solvents | Poor resistance |
CLTE is higher than metal and must be designed for. At 70–85 µm/m·K, PC/ASA expands roughly six times as much as steel across the same temperature change. A one-meter exterior panel moves about 7 mm more than the steel it is attached to over a 100 °C swing, which is enough to close a designed gap. Fix one attachment point and allow controlled movement at the others.
Design for UV-stabilized substrate everywhere, not just on visible faces. Edges, cut surfaces, and interior faces can become exposed, and an unstabilized substrate in those locations will degrade. Specify a stabilized grade for the whole part.
9. Grade Selection and Ordering
| Requirement | Grade to Specify |
| Maximum impact, outdoor | High-impact, UV-stabilized |
| Max heat resistance | Higher HDT grade |
| Flame retardant outdoor | FR + UV-stabilized |
| Extrusion sheet/profile | Extrusion grade, UV package |
| Cost-optimized panel | Cap layer over PC/ABS |
| Color-critical exterior | Color-matched stabilized grade |
| Maximum stiffness | Glass-filled (verify UV) |
Ordering checklist: request (1) accelerated weathering data with the exposure condition and measured property, (2) impact strength before and after weathering, (3) color stability data (ΔE), (4) UL yellow card if FR, (5) CLTE for thermal design, and (6) a COA for the specific lot.
Lot verification. Confirm density (ISO 1183), melt flow (ISO 1133), and notched Izod (ISO 180). For color-critical applications, verify color against the approved standard on a molded plaque, not on pellets — the color of the finished part depends on processing as well as on the resin.
10. Frequently Asked Questions
What is PC/ASA used for?
Automotive exterior trim, EV charging station housings, outdoor electrical enclosures, roofing and window components, outdoor furniture, and solar panel frames. Its defining application is any part that stays outdoors, must survive impact, and does not need to be painted.
Why is PC/ASA better than PC/ABS outdoors?
Because ASA uses an acrylic rubber instead of ABS’s polybutadiene rubber. Polybutadiene contains unsaturated double bonds that UV light attacks, causing yellowing, chalking, and embrittlement within a couple of years. The acrylic rubber has a saturated backbone and is not vulnerable to this mechanism, so the alloy survives 10+ years outdoors.
How long does PC/ASA last outdoors?
Typically 10+ years unpainted, depending on the stabilization package and the exposure conditions. Compare with 2–4 years for PC/ABS even with a UV package.
Does PC/ASA need to be painted?
No — that is its principal advantage over PC/ABS outdoors. It is used unpainted for exterior parts, which eliminates the paint cost and removes a coating that could fail independently.
Is PC/ASA more expensive than PC/ABS?
Yes, typically 20–40% more per kilogram. For an unpainted outdoor part, the premium is usually less than the cost of the paint system PC/ABS would require.
Does PC/ASA resist chemicals?
No. It inherits PC’s poor chemical resistance and should not contact fuels, oils, ketones, or chlorinated solvents. Use PC/PBT or PBT for those environments.
Can PC/ASA be flame retardant?
Yes, FR grades are available and are common for outdoor electrical enclosures and EV charging equipment. Verify that the FR system is compatible with the UV stabilization package.
What is the difference between PC/ASA and plain ASA?
ASA is the base polymer, used for profiles, cladding, and sheet where toughness and heat resistance requirements are moderate. PC/ASA is an alloy with polycarbonate that raises impact strength and heat resistance for structural exterior parts.
How should PC/ASA be dried before molding?
At 100–110 °C for 3–4 hours in a desiccant dryer, to ≤0.02% moisture. Like all PC alloys it hydrolyzes if molded wet, causing splay, silver streaks, and permanent property loss.
Does PC/ASA yellow in sunlight?
Far less than PC/ABS. Some color shift occurs over long exposure, and a UV-stabilized grade with a well-chosen pigment system minimizes it. Verify with ΔE data from accelerated weathering rather than assuming no change.
Can PC/ASA be coextruded over a cheaper substrate?
Yes, and it is a common cost-reduction strategy. A 0.3–0.5 mm cap layer of PC/ASA or ASA over PC/ABS or ABS provides the weathering protection at the cost of the substrate. Verify bond strength with a peel test.
How do I verify an incoming PC/ASA lot?
Check density (ISO 1183), melt flow (ISO 1133), and notched Izod (ISO 180). For color-critical applications, mold a plaque and verify color against the standard — pellet color does not predict part color.
Is PC/ASA recyclable?
PC/ASA is a code 7 (“other”) plastic and is not collected in curbside programs. Industrial regrind is routinely reused at 10–20% in non-critical and non-color-critical parts. For exterior parts where color matters, regrind should be limited or avoided because thermal history shifts the color.
What pigment system is used for outdoor PC/ASA?
Inorganic pigments are generally preferred for long-term UV stability, with organic pigments reserved for shades where inorganics cannot reach the required color. Certain organic pigments accelerate degradation, and the pigment system must be selected together with the UV stabilizer package rather than independently. For a color-critical exterior part, request the pigment chemistry and its weathering performance.
Does PC/ASA need an annealing step?
Annealing is not routinely required, but it benefits parts with high molded-in stress or parts that will be exposed to chemicals. Anneal at about 100–110 °C for 2–4 hours if stress relief is needed. For most exterior applications with no chemical exposure, standard processing and good tool design are sufficient.
How does PC/ASA behave at low temperature?
It retains useful impact strength at −30 °C, typically 10–20 kJ/m² notched Izod, which is adequate for most exterior applications. Below about −40 °C, impact performance falls and the ductile-to-brittle transition becomes a design consideration — verify with data at your minimum service temperature if the part faces extreme cold.
11. Next Steps
The pc/asa alloy earns its place by solving a problem that other engineering plastics cannot solve economically: unpainted outdoor durability with structural properties. The decision is usually simple — if the part is outdoors and unpainted, PC/ASA’s premium is cheaper than a paint system; if it is indoor or painted, PC/ABS is the economical choice; and if it contacts fuel or solvent, neither is suitable.
We supply PC/ASA in UV-stabilized, high-impact, flame-retardant, color-matched, and extrusion grades, with weathering data and color matching support.
Related Reading
- PC/ASA vs ASA vs PC/ABS: Weathering and Cost Compared
- PC/ASA for EV Charging Stations and Outdoor Enclosures
- ASA Plastic: The Complete Guide to Properties and Applications
- PC/ABS Blend: The Complete Guide to Properties, Grades and Applications
- PC/PBT Alloy: Properties, Chemical Resistance and Applications