PC PBT Resin Alloy Pellets

PC PBT Alloy Resin

At Suke Plastics, we mainly supply:

  • Sabic Xenoy™ PC/PBT
pc pbt resin alloy plastic

Supply Various PC PBT pellets

TypeGrade No.ManufacturerBrandKey FeaturesTypical Applications
PC PBT1102SabicXENOY™Unreinforced PC/polyester alloy. Offers excellent low-temperature impact strength and chemical resistance to automotive fluids.Automotive parts requiring low-temperature toughness and resistance to oils, fuels, cleaners, and other automotive fluids.
PC PBT1103SabicXENOY™Unreinforced, impact-modified PBT+PC alloy. Provides excellent low-temperature impact strength and chemical resistance. Available in gray and black colors.Automotive applications, exterior and under-hood parts requiring chemical resistance and low-temperature impact performance.
PC PBT1105SabicXENOY™Non-reinforced, impact-modified PBT/PC blend for injection molding. Offers excellent low-temperature toughness and very good paintability.Painted automotive components, exterior trims, housings, and molded parts requiring toughness and paintable surface quality.
PC PBT1731SabicXENOY™Impact- and chemical-resistant PC/polyester alloy. UV-stabilized with excellent physical property retention for outdoor automotive use.Automotive exterior parts, outdoor vehicle components, and applications requiring UV stability and chemical resistance.
PC PBT1731HSSabicXENOY™Hydrostable PC/polyester alloy. Impact- and chemical-resistant with excellent property retention in automotive exterior environments.Automotive exterior parts, outdoor trims, and components exposed to humidity, weathering, and automotive fluids.
PC PBT1760ESabicXENOY™11% glass-reinforced PC/PBT alloy. High-flow version of XENOY™ 1760. Offers impact resistance, chemical resistance, and exterior property retention.Automotive exterior parts, structural molded components, and complex injection-molded parts requiring flow, strength, and dimensional stability.
PC PBT1760HSabicXENOY™11% glass-fiber-reinforced PC/PBT alloy. Impact modified and chemically resistant with excellent physical property retention outdoors.Automotive exterior components, reinforced molded parts, brackets, housings, and parts requiring strength and chemical resistance.
PC PBT1760TSabicXENOY™Easy-flow 11% glass-reinforced PC/PBT material. Provides excellent strength and dimensional stability.Door handles, mirror housings, automotive exterior parts, and complex molded components requiring easy flow and stable dimensions.
PC PBT2230SabicXENOY™Unreinforced, opaque polycarbonate-based alloy. Offers chemical resistance, dimensional stability, and balanced mechanical performance.General automotive parts, housings, covers, and molded components requiring chemical resistance and dimensional stability.
PC PBT5220USabicXENOY™Unreinforced, impact-modified PBT+PC alloy. Improved mechanical property retention under UV exposure with excellent low-temperature impact and chemical resistance.Automotive exterior components, unpainted exterior parts, and outdoor molded applications requiring UV stability.
PC PBT5720SabicXENOY™Unreinforced PBT+PC alloy. Provides outstanding low-temperature impact strength and chemical resistance.Automotive parts, exterior trims, housings, and molded components requiring low-temperature impact and chemical resistance.
PC PBT5720USabicXENOY™Unfilled PBT+PC alloy. UV-stabilized version with outstanding low-temperature impact strength and chemical resistance.Outdoor automotive parts, exterior trims, and UV-exposed molded components requiring impact and chemical resistance.
PC PBT6370SabicXENOY™30% glass-reinforced, impact-modified thermoplastic alloy. Provides improved toughness, ductility, stiffness, and dimensional stability.Reinforced automotive parts, structural housings, brackets, and injection-molded components requiring stiffness and toughness.
PC PBT6620SabicXENOY™Unreinforced, impact-modified PBT+PC thermoplastic alloy. Offers outstanding low-temperature impact performance.Automotive exterior and interior parts, housings, trims, and parts used in cold environments.
PC PBT6620USabicXENOY™Unfilled, impact-modified, UV-stabilized PBT+PC alloy. Offers outstanding low-temperature impact strength and chemical resistance.Unpainted automotive exterior parts, outdoor trims, and UV-exposed components requiring chemical resistance.
PC PBTCL100SabicXENOY™Unfilled, impact-modified, UV-stabilized PC/PBT blend. Offers excellent solvent resistance and good low-temperature ductility. ISO1043: PC+PBT-I.Unpainted exterior automotive applications, body components, trims, and parts exposed to solvents or occasional chemical contact.
PC PBTCL100SSabicXENOY™PC/PBT blend developed for good low-temperature impact strength, excellent UV stability, and resistance to occasional solvent and gasoline contact.Unpainted exterior automotive body components, exterior trims, and parts exposed to sunlight, gasoline, and solvents.
PC PBTCL101SabicXENOY™Unfilled, impact-modified PC/PBT blend. Offers excellent solvent resistance and low-temperature ductility. ISO1043: PC+PBT-I.Off-line painted exterior automotive applications, painted body components, trims, and chemical-resistant exterior parts.
PC PBTHTX575SabicXENOY™30% high-strength glass-fiber-reinforced resin. Provides excellent strength, stiffness, and heat resistance. Designed to survive e-coating and baking up to about 200°C.E-coating capable molded parts, EV components, front-end modules, grille opening reinforcements, structures, and grille shutters.
PC PBTHTX975SabicXENOY™35% high-strength glass-fiber-reinforced resin. Higher modulus than HTX575 with excellent strength, stiffness, and heat resistance. Designed for baking up to about 200°C.EV components, front-end modules, grille opening reinforcements, structural parts, grille shutters, and e-coating process parts.
PC PBTHX5600HPSabicXENOY™PBT-based semi-crystalline blend with balanced flow and impact. Improved chemical resistance to lab disinfectants and chemicals. Biocompatible, ISO10993 or USP Class VI. EtO, gamma, and steam sterilizable.Healthcare enclosures, medical device housings, lab equipment housings, and parts requiring disinfectant resistance and sterilization compatibility.
PC PBTHX6600HPSabicXENOY™PBT-based semi-crystalline blend with balanced flow and impact. Improved resistance to healthcare disinfectants and chemicals. Biocompatible, ISO10993 or USP Class VI. EtO, gamma, and steam sterilizable.Healthcare device enclosures, medical housings, lab equipment parts, and sterilizable components exposed to disinfectants.
PC PBTRCX201SabicXENOY™Information not confirmed in the provided document. Datasheet review is recommended before publishing detailed features.Automotive parts, Electrical housings, Industrial equipment components
PC PBTX2420SabicXENOY™10% glass-filled, high-flow, impact-modified injection molding grade. Offers enhanced melt flow, impact ductility, and broad color space.Thin-wall or complex injection-molded parts, automotive components, housings, and applications requiring high flow and impact strength.
PC PBTX4820SabicXENOY™7.5% mineral-filled PC/PBT blend with low CTE, high modulus, high ductility, high chemical resistance, very low creep, fatigue resistance, and dimensional stability.Body panels, window rails, door panels, power tool housings, door handles, medical device enclosures, and EV components.
PC PBTX4830SabicXENOY™Hydrostable, high-modulus, low-temperature ductile PC/PBT blend. Provides high chemical resistance, very low creep, low CTE, fatigue resistance, and heat dimensional stability.Body panels, safety equipment, housings, door handles, spring-loaded applications, medical device enclosures, and outdoor sports equipment.
PC PBTX4850SabicXENOY™12% mineral-filled PC/PBT blend with low CTE, high modulus, high ductility, high chemical resistance, very low creep, fatigue resistance, and heat dimensional stability.Body panels, window rails, safety equipment, housings, door handles, spring-loaded parts, medical device enclosures, and EV components.
PC PBTX5100SabicXENOY™Semi-crystalline, impact-modified PC/PBT blend with excellent flow. ISO1043: PC+PBT-I.Injection-molded automotive components, housings, trims, and parts requiring good flow and impact performance.
PC PBTX5300WXSabicXENOY™Unreinforced, opaque PBT+PC alloy. UV-stabilized with chemical resistance, good mechanical performance, and excellent weatherability.Outdoor automotive components, exterior trims, housings, and weather-resistant molded parts.
PC PBTX5600WXSabicXENOY™Unreinforced, opaque polyester+PC alloy. UV-stabilized with mold release, chemical resistance, dimensional stability, and mechanical performance.Outdoor molded parts, automotive exterior components, housings, and parts requiring UV stability and easy release.
PC PBTXL1339SabicXENOY™High-heat grade for applications where chemical resistance is not required. Data generated in BOZ labs.High-heat molded parts and components that require thermal performance but do not require strong chemical resistance.
PC PBTXL1562SabicXENOY™Impact-modified PBT+PC blend with outstanding chemical resistance, good UV stability, and good flow properties.Automotive exterior parts, housings, trims, and molded components requiring chemical resistance, UV stability, and processability.

What is PC PBT Resin?

PC/PBT (Polycarbonate + Polybutylene Terephthalate) resin is a high-performance thermoplastic blend that combines the toughness and impact resistance of polycarbonate with the chemical resistance, dimensional stability, and processability of PBT.

Other Names

  • PC+PBT Alloy
  • PC/PBT Blend Resin

Appearance

  • Natural (light beige or ivory)
  • Black or custom colors available

Packaging

  • 25kg bags
  • jumbo bags

HS Code

  • 39079990

Key Properties

Technical Data

PropertyGeneral Grade
Density (g/cm³)1.20 – 1.35
Tensile Strength (MPa)55 – 75
Flexural Modulus (MPa)2000 – 3000
Izod Impact Strength (J/m)60 – 120
Heat Deflection Temp (°C)100 – 130
Melt Flow Index (MFI, g/10min)10 – 40

Applications

Grades We Offer

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.