PC Resin Plastic Pellets
- Home /
- Polycarbonate Resin
PC (Polycarbonate) Resin
As one of the leading polycarbonate resin manufacturers in China, Suke Plastics mainly supply PC plastic particles from these suppliers brands:
- Chimei WONDERLITE® PC
- FORMOSA (FCFC) TAIRILITE® PC
- FORMOSA (FIPC) TARFLON PC
- Covestro Makrolon®PC
- Sabic® PC
- LEXAN™ PC
- LG Chem PC
- Suke Plastics PC
- Huasheng PC








Supply Various Grades of PC pellets
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | PC-110 | Chimei | WONDERLITE | General Purpose Grade. Medium viscosity | General injection molding for vehicle indicator light casings, chocolate containers, high heel shoes |
| PC | PC-110U | Chimei | WONDERLITE | Weather Resistant Grade. Medium viscosity, UV stabilized | Outdoor applications, traffic signs |
| PC | PC-115P | Chimei | WONDERLITE | Medical grade. Comply with Bio-compatibility test(ISO10993-4,5,10,11). Gamma resistance(particular color) | Medical application |
| PC | PC-122 | Chimei | WONDERLITE | General Purpose Grade. High flow | General injection molding for external pen tubing, stationery, toys, water containers, thin wall products, complex transparent molding products |
| PC | PC-122 | Chimei | WONDERLITE | Weather Resistant Grade. High flow, UV stabilized | Outdoor applications, traffic signs |
| PC | PC-6600 | Chimei | WONDERLITE | Flame retardant grade, 1.0mm V-0, Opaque | Electrical appliances |
| PC | PC-6610 | Chimei | WONDERLITE | Flame retardant grade, 1.5mm V-0, Opaque, UV Stabilized, UL 746C f1, Opaque | Electrical appliances, outdoor applications (UL 746C f1) |
| PC | PC-6710 | Chimei | WONDERLITE | Flame retardant grade, Transparent,3.0mm V-0, UV Stabilized, UL 746C f1 | Electrical appliances, outdoor applications (UL 746C f1) |
| PC | PC-115 | Chimei | WONDERLITE | Flame retardant grade. Low viscosity | General injection molding for stationery, external pen tubing, toys, transparent molded products |
| PC | PC-145K | Chimei | WONDERLITE | Flame retardant grade. High flow, good recyclability | Lighting keyboard/transparent products |
| PC | PC-616LS | Chimei | WONDERLITE | Flame retardant grade. 1.0 mm V0, Low smoke density | Rail transportation application/Electrical appliances |
| PC | PC-6700 | Chimei | WONDERLITE | Flame retardant grade. 2.5 mm V0 | Electrical appliances |
| PC | PC-6710NF | Chimei | WONDERLITE | Flame retardant grade (PFAS Free), 3.0 mm V0, Transparent | Electrical appliances, outdoor applications (UL 746C f1) |
| PC | PC-6715NF | Chimei | WONDERLITE | Flame retardant grade (PFAS Free), 1.5 mm V0,Transparent | Railway, Electrical appliances, outdoor applications |
| PC | PC-6715VT | Chimei | WONDERLITE | Flame retardant grade 1.5 mm V0. Transparent | Railway, Electrical appliances, outdoor applications (UL 746C f1) |
| PC | PC-681U | Chimei | WONDERLITE | Flame retardant grade 1.5mm V0. Low temperature impact resistance | Electrical appliances, outdoor applications (UL 746C f1) |
| PC | PC-175 | Chimei | WONDERLITE | High flow grade. High Flowability | Compounding or general injection molding for thin part |
| PC | PC-115U | Chimei | WONDERLITE | Weather Resistant Grade. Low viscosity, UV stabilized | Outdoor applications, traffic signs |
| PC | PC-110P | Chimei | WONDERLITE | Medical grade. Comply with Bio-compatibility test(ISO10993-5/10) | Medical application |
| PC | PC-122P | Chimei | WONDERLITE | Medical grade. Comply with Bio-compatibility test(ISO10993-5/10) / High Flow | Medical application |
| PC | PC-115L | Chimei | WONDERLITE | SAE grade | Automotive head lamp |
| PC | PC-110L | Chimei | WONDERLITE | SAE grade | Automotive head lamp |
| PC | PC-6600 J01 | Chimei | WONDERLITE | Standard Color Basic PC. 1.0mm V0, standard black and pre-colored | Electrical appliances |
| PC | PC-108U | Chimei | WONDERLITE | Extrusion grade. High viscosity; UV stabilized | Skylight Panel; Noise Barrier Wall; Corrugated Roof |
| PC | PC-115D | Chi Mei (Zhenjiang) | WONDERLITE | Light-Diffusing PC Grade | Lighting fixtures |
| PC | PC-25D | Chi Mei (Zhenjiang) | WONDERLITE | Light-Diffusing PC Grade | Lighting fixtures |
| PC | PC-6600C | Chi Mei (Zhenjiang) | WONDERLITE | Flame Retardant Grade. V0 rating at 1.5 mm; weather-resistant and low-temperature resistant. | EV charging stations, electrical equipment, etc. |
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | AC3710 | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. Halogen free, Flame retardant, High flow, Non-transparency | Household appliances, 3C electronic product casings Thin-walled electrical equipment housing such as laptop battery casings, internal components of energy storage devices |
| PC | AC3900 | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. Halogen free, Flame retardant, White color, Non-transparency, High gloss reflection | Home lighting, electronics touch panel module internal accessories such as LED lamp cap, lamp holder, panel white frame |
| PC | AC3610-AF | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. High flow, Non-transparency, Cl, Br, Sb free, Flame retardant | Transformer case, Battery case, Projector housing, Electroomechanical appliance cover |
| PC | AC3600 | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. Halogen free, Flame retardant, High heat resistance, Non-transparency | Adapters, transformers, chargers, batteries, routers casings |
| PC | AC3830 | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. Light diffusion, Mid flow, UV resistance, Halogen free | Diffusion board, Diffusion lamp, Diffusion injection lampshade, Diffusion injection-blow bulb |
| PC | AC3839 | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. Charging shell, battery shell, router shell | Mid flow, Flame retardant, Low temperature impact property, UV resistance, |
| PC | AC3630 | FORMOSA (FCFC) | TAIRILITE | Self Extinguishing Grade. Halogen free, Flame retardant, High flow, Non-transparency,UL weather resistance certification | Household appliances, 3C electronic products , outdoor equipment shell, electric bike battery case, Energy storage device |
| PC | AC1115 | FORMOSA (FCFC) | TAIRILITE | Weather Resistant Grade. Transparency, Mid-low flow, High clean PC, Low gel. | Optical applications, High transparency, PC film, PC sheet. |
| PC | AC3843 | FORMOSA (FCFC) | TAIRILITE | Transparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free. | Transparent flame-retardant injection parts. |
| PC | AC3853 | FORMOSA (FCFC) | TAIRILITE | Transparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free. | Transparent flame-retardant injection parts. |
| PC | AC3854 | FORMOSA (FCFC) | TAIRILITE | Transparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free. | Transparent flame-retardant injection parts. |
| PC | AC3832 | FORMOSA (FCFC) | TAIRILITE | Transparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free. | Transparent flame-retardant sheet and injection parts. |
| PC | AC3873 | FORMOSA (FCFC) | TAIRILITE | Transparent Flame Retardant Grade. Mid-low flow, UV resistance, Halogen free. | Transparent flame-retardant sheet and injection parts. |
| PC | AC2856 | FORMOSA (FCFC) | TAIRILITE | Diffusion Grade. Light diffusion, Mid-high flow, UV resistance | Diffusion injection lampshade, Diffusion injection-blow bulb |
| PC | AC2854 | FORMOSA (FCFC) | TAIRILITE | Diffusion Grade. Light diffusion, Mid-high flow, UV resistance | Diffusion board, Diffusion lamp (LED tube shell) |
| PC | AC2820 | FORMOSA (FCFC) | TAIRILITE | Diffusion Grade. Light diffusion, Mid-high flow, UV resistance | Automotive lighting applications, such as DRL, position lights, interior lights |
| PC | AC9140 | FORMOSA (FCFC) | TAIRILITE | Ultra-low Temp Resistance Copolymer. Transparency, Mid flow, UV resistance, | Mobile phone / tablet / laptop / 3C products case, sports equipment / protective gear. |
| PC | AC9144 | FORMOSA (FCFC) | TAIRILITE | Ultra-low Temp Resistance Copolymer.Mid flow, Low temperature impact property, UV resistance, | Mobile phone / tablet / laptop / 3C products case, sports equipment / protective gear. |
| PC | AC9830 | FORMOSA (FCFC) | TAIRILITE | Ultra-low Temp Resistance Copolymer, Mid flow, Flame retardant, UV resistance, | Mobile equipment housing, Connectors, Switches, Outdoor equipment component, Battery pack. |
| PC | AC2916 | FORMOSA (FCFC) | TAIRILITE | High Transparency Grade. High flow | Light guide bar, Daytime running lights for car lamp, LED condenser lens. |
| PC | AC2955 | FORMOSA (FCFC) | TAIRILITE | IR Transmittance Grade, Mid-high flow | Applications in Information transfer, such as remote control, mobile phone PDA and wireless keyboard ect |
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | A1900 | FORMOSA (FIPC) | TARFLON | Standard Color Basic PC | For injection molding or compounding. |
| PC | A2200 | FORMOSA (FIPC) | TARFLON | Standard Color Basic PC | For injection molding or compounding. |
| PC | IR1700 | FORMOSA (FIPC) | TARFLON | General Purpose Grade | Relay cases, Timer cases, Packs, Decorative lighting covers, Cups and glasses, Dishes, Electrical equipment, Safety lamps, Explosion-proof gloves, Contact lens cases. |
| PC | IR1900 | FORMOSA (FIPC) | TARFLON | General Purpose Grade | Relay cases, Timer cases, Packs, Decorative lighting covers, Cups and glasses, Dishes, Electrical equipment, Safety lamps, Explosion-proof gloves, Contact lens cases. |
| PC | IR2200 | FORMOSA (FIPC) | TARFLON | General Purpose Grade | Relay cases, Timer cases, Packs, Decorative lighting covers, Cups and glasses, Dishes, Electrical equipment, Safety lamps, Explosion-proof gloves, Contact lens cases. |
| PC | IR2500 | FORMOSA (FIPC) | TARFLON | General Purpose Grade | Relay cases, Timer cases, Packs, Decorative lighting covers, Cups and glasses, Dishes, Electrical equipment, Safety lamps, Explosion-proof gloves, Contact lens cases. |
| PC | IV1900R | FORMOSA (FIPC) | TARFLON | Weather Resistant Grade | IV-R grade is listed in AMECA, can used for car headlamp, lighting equipment and various outdoor applications. |
| PC | IV2200R | FORMOSA (FIPC) | TARFLON | Weather Resistant Grade | IV-R grade is listed in AMECA, can used for car headlamp, lighting equipment and various outdoor applications. |
| PC | IV2500 | FORMOSA (FIPC) | TARFLON | Weather Resistant Grade | IV grade is mainly used for safety glasses, sun glasses and daylight roof. |
| PC | VT2500 | FORMOSA (FIPC) | TARFLON | Weather Resistant Grade | VT grade is also mainly used for safety glasses, sun glasses and daylight roof. |
| PC | MD1500 | FORMOSA (FIPC) | TARFLON | Optical Grade | CD & DVD disc |
| PC | LC1500 | FORMOSA (FIPC) | TARFLON | Light Guide Grade | For light guide panel and daytime running light. |
| PC | HQ2200 | FORMOSA (FIPC) | TARFLON | Clean Grade (Film grade) | For high-quality film/sheet of LCD or other printing applications. |
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | 1260 | Covestro | Makrolon | Impact modified grades / Low viscosity. MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release | Injection molding |
| PC | 2205 | Covestro | Makrolon | General purpose grades.MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 2207 | Covestro | Makrolon | General purpose grades / Low viscosity. MVR (300 °C/1.2 kg) 35 cm³/10 min; low viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 2407 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 2605 | Covestro | Makrolon | General purpose grades / Medium viscosity. MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 2805 | Covestro | Makrolon | General purpose grades. MVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 9425 | Covestro | Makrolon | 20 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; easy release; available in opaque colors only | Extrusion; Injection molding |
| PC | AG2677 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent colors only | Injection molding; Automotive glazing; Roof modules |
| PC | AL2447 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors | Injection molding; Automotive lighting; Headlamp lenses for automotive forward lighting |
| PC | AL2647 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors | Injection molding; Automotive lighting; Headlamp lenses for automotive forward lighting |
| PC | AX2677 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; UV stabilized; available in black colors only | Injection molding; Automotive exterior roof trim + pillar appliques; High-gloss surfaces with highest requirements; For the use in combination with hard coatings |
| PC | LED2045 | Covestro | Makrolon | MVR (250 °C/2.16 kg) 17 cm³/10 min; PC with highest transmission; low viscosity; easy release;available in color code 000000 only | Injection molding; Light guides |
| PC | LED2245 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; PC with highest transmission; low viscosity; easy release | Injection molding; Light guides; optics and lenses |
| PC | 2205 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding; General purpose |
| PC | 2405 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding; General purpose |
| PC | 2407 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors | Injection molding; General purpose |
| PC | 2807 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors | Injection molding; General purpose |
| PC | AG2677 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in transparent colors only. CQ renewable attributed, Optical quality | Injection molding; Automotive glazing; Roof modules |
| PC | AL2447 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors. CQ renewable attributed, Optical quality | Injection molding; Automotive lighting; Headlamp lenses for automotive forward lighting |
| PC | AX2675 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; available in black colors only | Injection molding; Automotive exterior roof trim + pillar appliques; High-gloss surfaces with highest requirements; for the use in combination with hard coatings |
| PC | DQ5922 FR | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; low diffusion; UV stabilized | Extrusion; Injection molding; Light diffusion |
| PC | DQ5942 FR | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; medium diffusion; UV stabilized | Extrusion; Injection molding; Light diffusion |
| PC | DQ5962 FR | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 5.0 cm³/10 min; high diffusion; UV stabilized | Extrusion; Injection molding; Light diffusion |
| PC | LED2245 EL | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release | Injection molding; Edge lighting material for light guides and optical parts |
| PC | RW2407 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; UV stabilized; variable content of filler for high reflectance application; CQ renewable attributed | Automotive,Electronics, appliances & telecommunications |
| PC | 2407 RE25 CQ | Covestro | Makrolon | UV stable, CQ renewable attributed, Transparent | Automotive,Electronics, appliances & telecommunications |
| PC | 2805 RE CQ | Covestro | Makrolon | CQ renewable attributed, Transparent | Automotive,Electronics, appliances & telecommunications |
| PC | AL2447 RP70 CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; melt temperature 280 – 320 °C; available in clear transparent colors and in various signal colors. | automotive lighting; headlamp lenses for automotive forward lighting |
| PC | AL2647 RE CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; UV stabilized; easy release; available in clear transparent colors and in various signal colors | Injection molding; Automotive lighting; Headlamp lenses for automotive forward lighting |
| PC | AL2647 RP70 CQ | Covestro | Makrolon | CQ recycled attributed, UV stable, Transparent, Optical quality | headlamp lenses for automotive forward lighting |
| PC | LED2245 HP RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; high color stability under injection molding conditions; PC with highest transmission; low viscosity; easy release | Injection molding; Light guides; Optics and lenses |
| PC | 2456 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding; Food contact quality |
| PC | 2467 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; UL 94V-2/1.5 mm and 3.0 mm; UV stabilized; easy release; available in transparent, translucent and opaque colors | Electronics, appliances & telecommunications |
| PC | 2656 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colors;Food-contact-compliant | Injection molding; Food contact quality |
| PC | 2856 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; easy release; available in transparent, translucent and opaque colors. Food-contact-compliant. | Injection molding; Food contact quality |
| PC | 2865 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 10 cm³/10 min; UL 94V-2/1.5 mm and 3.0 mm; medium viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 3105 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding; General purpose |
| PC | 6455 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 12 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 6457 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 12 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; UV stabilized; easy release; available in transparent and opaque colors | Injection molding |
| PC | 6485 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 9.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; medium viscosity; easy release; available in opaque colors only | Injection molding |
| PC | 6487 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 9.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; medium viscosity; UV stabilized; easy release; available in opaque colors only | Injection molding |
| PC | 6555 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 10 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding |
| PC | 6557 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 10 cm³/10 min; UL 94V-0/3.0 mm; medium viscosity; UV stabilized; easy release; available in transparent, translucent and opaque colors. | Injection molding |
| PC | 6717 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 3.0 cm³/10 min; V-0 at 2.0 mm (UL 94); high viscosity; branched; UV stabilized; easy release; available in transparent, translucent and opaque colors | |
| PC | 8025 | Covestro | Makrolon | 20 % glass fiber reinforced; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; milled fiber; high viscosity; easy release; available in opaque colors only;Dimensionally stable | Extrusion; Injection molding; Precision parts |
| PC | 8325 | Covestro | Makrolon | 20 % glass fiber reinforced; MVR (300 °C/1.2 kg) 4.0 cm³/10 min; high viscosity; easy release; available in opaque colors only; Dimensionally stable | Extrusion; Injection molding |
| PC | 9125 | Covestro | Makrolon | 20 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 8.0 cm³/10 min; UL 94V-0/1.5 mm; medium viscosity; easy release; available in opaque colors only; Dimensionally stable. | Injection molding |
| PC | 9415 | Covestro | Makrolon | 10 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; easy release; available in opaque colors only; Dimensionally stable. | Injection molding |
| PC | 9417 | Covestro | Makrolon | 10 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; UV stabilized; easy release; available in opaque colors only | Injection Molding |
| PC | ET3113 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; UV stabilized; available in transparent colors only; Impact resistant. | Extrusion;Solid sheet; Corrugated sheet |
| PC | FR6002 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 18 cm³/10 min; low viscosity; easy release | Injection molding |
| PC | FR7087 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 12 cm³/10 min; UL 94V-0/2.2 mm and 5VA/3.0 mm; medium viscosity; UV stabilized; easy release; available in transparent and translucent colors | Injection molding; Electrical/electronic |
| PC | GF9002 | Covestro | Makrolon | 10 % glass fiber reinforced; flame retardant; MVR (300 °C/1.2 kg) 15 cm³/10 min; UL 94V-0/1.2 mm; low viscosity; easy release; available in opaque colors only | Injection molding; Electrical/electronic; Housing parts with low wall thickness |
| PC | XT5010 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; easy processing; low viscosity; easy release; Vicat softening temperature 50 N, 50 °C/h = 110 °C; available in transparent colors only | Injection molding; LCD TV frame |
| PC | 6265 X | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; UL 94V-0/1.5 mm; low viscosity; easy release; available in opaque colors only | Injection molding |
| PC | 6267 X | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 19 cm³/10 min; UL 94V-0/1.5 mm; low viscosity; UV stabilized; easy release; available in opaque colors only | Injection molding |
| PC | 6487 RE | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 9.0 cm³/10 min; UL 94V-0/1.5 mm and 5VA/3.0 mm; medium viscosity; UV stabilized; easy release; available in opaque colors only | Injection molding |
| PC | 6557 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors; Food-contact-compliant, CQ renewable attributed | Injection molding; Food contact quality |
| PC | 2456 RE CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; available in transparent, translucent and opaque colors | Injection molding; Food contact quality |
| PC | 2856 RE CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 9.0 cm³/10 min; food contact quality; medium viscosity; easy release; melt temperature 280 – 320 °C; available in transparent, translucent and opaque color | injection molding |
| PC | 6555 RE CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 10 cm³/10 min; flame retardant; UL 94V-0/3.0 mm; medium viscosity; easy release; melt temperature 280 – 320 °C; available in transparent, translucent and opaque colors | injection molding |
| PC | 6265 X RE25 CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; flame retardant; UL 94V-0/1.5 mm; low viscosity; easy release; melt temperature 280 – 320 °C; available in opaque colors only | injection molding |
| PC | 6265 X RE CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; flame retardant; UL 94V-0/1.5 mm; low viscosity; easy release; melt temperature 280 – 320 °C; available in opaque colors only | Injection molding |
| PC | 6267 X RE CQ | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; flame retardant; UL 94V-0/1.5 mm; low viscosity; UV stabilized; easy release; injection molding – melt temperature 280 – 320 °C; available in opaque colors only | Injection molding |
| PC | 2258 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors | Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C |
| PC | 2558 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 14 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors; Medical. | Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C |
| PC | 2658 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors; Medical. | Injection molding; Medical devices; suitable for ETO and steam sterilization at 121 °C |
| PC | 3158 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors | Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C |
| PC | Rx1452 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 16 cm³/10 min; low viscosity; easy release; Medical, Transparent | Injection molding; Medical devices |
| PC | Rx1805 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; high lipid resistance; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements | Injection molding; Medical devices; Transparent parts for medical devices |
| PC | Rx1851 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 23 cm³/10 min; low viscosity; easy release; Medical, Transparent | Injection molding; Medical devices |
| PC | Rx2530 | Covestro | Makrolon | MVR (300 °C/1.2 kg) 15 cm³/10 min; medium viscosity; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements; Medical, Transparent. | Injection molding; Medical devices; Transparent parts for medical devices. |
| PC | 2258 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 34 cm³/10 min; low viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors | Injection molding; Medical devices; suitable for ETO and steam sterilization at 121 °C |
| PC | 2458 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors. | Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C |
| PC | 2658 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 12 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors. CQ renewable attributed. | Injection molding; Medical devices; suitable for ETO and steam sterilization at 121 °C |
| PC | 2858 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 9.0 cm³/10 min; medium viscosity; easy release; biocompatible according to many ISO 10993-1 test requirements; available in transparent and opaque colors | Injection molding; Medical devices; Suitable for ETO and steam sterilization at 121 °C |
| PC | Rx1805 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 6.0 cm³/10 min; high viscosity; high lipid resistance; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements | Injection molding; Medical devices; Transparent parts for medical devices |
| PC | Rx2530 RE | Covestro | Makrolon | MVR (300 °C/1.2 kg) 15 cm³/10 min; medium viscosity; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements; Medical, CQ renewable attributed | Injection molding; Medical devices; Transparent parts for medical devices |
| PC | 1804 | Covestro | Makrolon | flame retardant; MVR (300 °C/1.2 kg) 6.0 cm³/10 min; UL 94V-2/1.5 mm and 3.0 mm; high viscosity; UV stabilized; optimized for low plate-out; Transparent | Extrusion; Solid sheet; Aircraft construction; Automotive construction; Railway construction |
| PC | 1603 | Covestro | Apec | Heat Resistant Grade. MVR (330°C/2.16 kg) 25 cm³/10 min; high viscosity; UV stabilized; softening temperature (VST/B 120) = 159 °C | Injection molding |
| PC | 1695 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330°C/2.16 kg) 45 cm³/10 min; easy release; softening temperature (VST/B 120) = 158°C | Injection molding; Covers for brake lights and indicator lights; Headlamp reflectors/bezels |
| PC | 1745 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 17 cm³/10 min; easy release; for superheated steam sterilization up to 143 °C; meets criteria of US Pharmacopeia (USP) Class VI; biocompatible according to many ISO 10993-1 test requirements; softening temperature (VST/B 120) = 170 °C | Injection molding; Films for medical packaging; Contact lens holders; Medical vessels; Safety valve for respiration aids; Syringe tops |
| PC | 1795 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 30 cm³/10 min; easy release; low viscosity; softening temperature (VST/B 120) = 173°C | Injection molding; Covers for brake lights and indicator lights; Headlamp reflectors/bezels |
| PC | 1803 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 10 cm³/10 min; high viscosity; UV stabilized; softening temperature (VST/B 120) = 184 °C | Injection molding; Covers for brake lights and indicator lights; Car interior light covers; Domestic lamp covers; Headlamp lenses; Covers for ships’ lights; Connector pieces for halogen systems |
| PC | 1895 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 18 cm³/10 min; easy release; softening temperature (VST/B 120) = 183°C | Injection molding; Covers for brake lights and indicator lights; Recessed light fixtures/reflectors; Raised brake lights; Headlamp reflectors/bezels |
| PC | 1897 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 18 cm³/10 min; easy release; UV stabilized; softening temperature (VST/B 120) = 182 °C | Injection molding; Lamp covers; Headlamp lenses |
| PC | 2095 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 8 cm³/10 min; high viscosity; easy release; softening temperature (VST/B 120) = 203 °C | Injection molding; Covers for brake lights and indicator lights; Recessed light fixtures/reflectors; Blade-type fuses; Headlamp reflectors/bezels |
| PC | 2097 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 8 cm³/10 min; high viscosity; easy release; UV stabilized; softening temperature (VST/B 120) = 202 °C | Injection molding; Lamp covers; Headlamp lenses |
| PC | FR1897 | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; flame retardant, MVR (330°C/2.16 kg) 18 cm³/10 min; low viscosity; easy release; UV stabilized (fulfills the requirements according to EN 170); V-2/1.5mm (UL 94); V-0/3.0mm (UL 94); softening temperature (VST/B 120) = 182°C; available in transparent and opaque colors | Injection molding; Visors for firemen’s helmets |
| PC | 1745 RE | Covestro | Apec | Heat Resistant Grade. Copolycarbonate; MVR (330 °C/2.16 kg) 17 cm³/10 min; easy release; for superheated steam sterilization up to 143 °C; meets criteria of US Pharmacopeia (USP) Class VI; biocompatible according to many ISO 10993-1 test requirements; softening temperature (VST/B 120) = 170 °C; Medical, CQ renewable attributed | Injection molding; Films for medical packaging; Contact lens holders; Medical vessels; Safety valve for respiration aids; Syringe tops |
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | ALS01 | Sabic | Sabic | Injection Molding Grade. Medium-low flow (MFR13), heat and UV stabilized, polycarbonate product with mold release | for use in the automotive lens market. |
| PC | ALS02 | Sabic | Sabic | Injection Molding Grade. medium-high flow (MFR23), heat and UV stabilized, polycarbonate product with mold release | for use in the automotive lens market. |
| PC | PC0700 | Sabic | Sabic | Compounding Grade. low flow (MFR = 7 at 300°C/1.2kg), heat stabilized | for use in the custom compounding market. |
| PC | PC0703R | Sabic | Sabic | Extrusion grade. low flow (MFR = 7 at 300°C/1.2kg), heat and UV stabilized | for use in the extrusion market |
| PC | PC0800 | Sabic | Sabic | Compounding Grade. low flow (MFR = 8 at 300°C/1.2kg), heat stabilized | for use in the custom compounding market. |
| PC | PC1000 | Sabic | Sabic | Compounding Grade. medium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilized, | for use in the custom compounding market. |
| PC | PC1000R | Sabic | Sabic | Injection Molding Grade. medium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilized, | for use in the general purpose molding market |
| PC | PC1003R | Sabic | Sabic | Injection Molding Grade. medium-low flow (MFR = 10 at 300°C/1.2kg), heat and UV stabilized | for use in the general purpose molding market |
| PC | PC1004R | Sabic | Sabic | Injection Molding Grade. Medium-low flow (MFR = 10 at 300°C/1.2kg), natural, heat stabilized, | for use in the general purpose molding market |
| PC | PC1800 | Sabic | Sabic | Compounding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg), heat stabilized, | for use in the custom compounding market. |
| PC | PC1800R | Sabic | Sabic | Injection Molding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg), heat stabilized, | for use in the general purpose molding market |
| PC | PC1803R | Sabic | Sabic | Injection Molding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg),heat and UV stabilized | for use in the general purpose molding market |
| PC | PC1804R | Sabic | Sabic | Injection Molding Grade. Medium-low flow (MFR = 18 at 300°C/1.2kg),natural, heat stabilized | for use in the general purpose molding market |
| PC | PC2200 | Sabic | Sabic | Compounding Grade. high flow (MFR = 22 at 300°C/1.2kg), heat stabilized | for use in the custom compounding market. |
| PC | PC2200R | Sabic | Sabic | Injection Molding Grade. High flow (MFR = 22 at 300°C/1.2kg), heat stabilized | for use in the general purpose molding market |
| PC | PC2203R | Sabic | Sabic | Injection Molding Grade. High flow (MFR = 22 at 300°C/1.2kg), heat and UV stabilized | for use in the general purpose molding market |
| PC | PC5800 | Sabic | Sabic | Optical Grade. very high flow (MFR = 8.9 at 250°C/1.2kg) | for use in the optical media market. |
| PC | 101 | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. UL94 HB rated. | Suitable for extrusion and injection molding applications. |
| PC | 101R | Sabic | LEXAN | UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR. | for thicker sections without sinks. Internal mold release |
| PC | 102L | Sabic | LEXAN | high viscosity linear polycarbonate resin granulate. | be used as a base material for production of transparent and opaque products |
| PC | 103 | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. UV stabilized. UL94 HB rated. UL746C f1 rated. | for extrusion and injection molding applications |
| PC | 103R | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. UV Stabilized. Mold release. UL94 HB rated. UL746C f1 rated. | for extrusion and injection molding applications |
| PC | 104 | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. Grade designed for food contact. UL94 HB rated | for extrusion and injection molding applications |
| PC | 104R | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. Mold release. UL94 HB rated. | for extrusion and injection molding applications |
| PC | 121M | Sabic | LEXAN | 18 MFR polycarbonate. Improved internal mold release. UL94 HB rated. | |
| PC | 121R | Sabic | LEXAN | 18 MFR polycarbonate, MVR of 21. Mold release. UL94 HB rated. | |
| PC | 121SRM | Sabic | LEXAN | Easy flow, impact modified, super release grade polycarbonate. | |
| PC | 123 | Sabic | LEXAN | UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. | |
| PC | 123M | Sabic | LEXAN | 18 MFR polycarbonate. UV Stabilized. Improved internal mold release. UL94 HB rated. | |
| PC | 123R | Sabic | LEXAN | 18 MFR polycarbonate, MVR of 21. UV Stabilized. Mold release. UL746C f1 rated. UL94 HB rated | |
| PC | 123SRM | Sabic | LEXAN | Easy flow, uv stabilised, impact modified, super release grade | |
| PC | 124R | Sabic | LEXAN | 18 MFR polycarbonate. 21 MVR. Mold release. UL94 HB rated. | |
| PC | 131 | Sabic | LEXAN | 3.5 MFR polycarbonate. UL94 HB rated. For blow molding or extrusion. | Suitable for injection molding. |
| PC | 133R | Sabic | LEXAN | 3.5 MFR polycarbonate, MVR of 3. UV Stabilized. Mold release. UL94 HB rated. | designed for blow molding or extrusion. Suitable for injection molding. |
| PC | 134R | Sabic | LEXAN | 3.5 MFR polycarbonate, MVR of 3. Grade intended for food contact. Mold release. UL94 HB rated. | Designed for blow molding or extrusion. Suitable for injection molding. |
| PC | 141 | Sabic | LEXAN | 11 MFR polycarbonate. UL94 HB rated. | |
| PC | 141R | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 12. Mold release. UL94 HB rated. | |
| PC | 143 | Sabic | LEXAN | UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. | |
| PC | 143R | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 12. UV Stabilized. Mold release. UL94 HB rated. UL746C f1 rated. | |
| PC | 144R | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 12. Mold release. UL94 HB rated. This material is food contact compliant in most jurisdictions | |
| PC | 153R | Sabic | LEXAN | 2.5 MFR Branched polycarbonate. UV Stabilized. Mold release. UL94 HB rated. | |
| PC | 161R | Sabic | LEXAN | a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. | |
| PC | 163R | Sabic | LEXAN | medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. | |
| PC | 164R | Sabic | LEXAN | Medium viscosity, multi purpose polycarbonate resin with added release agent | designed for blow molding or extrusion. |
| PC | 172L | Sabic | LEXAN | low viscosity linear polycarbonate resin granulate | be used as a base material for production of transparent and opaque products. |
| PC | 191 | Sabic | LEXAN | 9 MFR polycarbonate. UL94 HB rated. Improved chemical resistance. Available only in opaque colors. | |
| PC | 201R | Sabic | LEXAN | 7 MFR polycarbonate. Mold release. Flame retardant grade, UL94 V2 rated. | For extrusion and injection molding. |
| PC | 203R | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. UV stabilized. Mold release. Flame retardant grade, UL94 V2 rated. UL746C f1 rated | For extrusion and injection molding. |
| PC | 221R | Sabic | LEXAN | 18 MFR polycarbonate. Mold release. Flame retardant grade, UL94 V2 rated. | |
| PC | 223M | Sabic | LEXAN | 18 MFR polycarbonate. UV Stabilized. Improved mold release. Flame retardant grade, UL94 V2 rated. | |
| PC | 223R | Sabic | LEXAN | 18 MFR polycarbonate, MVR of 21. UV stabilized. Mold release. Flame retardant grade, UL94 V2 rated. UL746C f1 rated. | |
| PC | 223S | Sabic | LEXAN | 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. | |
| PC | 241R | Sabic | LEXAN | ||
| PC | 241S | Sabic | LEXAN | 10.5 MFR. Improved flame retardance. Super mold release. | |
| PC | 243R | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 12. UV stabilized. Mold release. Flame retardant grade, UL94 V2 rated. UL746C f1 rated. | |
| PC | 244R | Sabic | LEXAN | 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. | |
| PC | 244RF | Sabic | LEXAN | a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors | |
| PC | 263R | Sabic | LEXAN | medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. | |
| PC | AD143 | Sabic | LEXAN | medium viscosity, injection molding grade exhibiting low dust attraction. | |
| PC | AT1230R | Sabic | LEXAN | ||
| PC | AT2030R | Sabic | LEXAN | ||
| PC | AVP KLL10FR | Sabic | LEXAN | 10% glass fiber filled polycarbonate. UL94 V0 and 5VA rated. | |
| PC | AVP TLL12CU | Sabic | LEXAN | AVP TLL12CU resin is a wide specification polycarbonate. 12 MFR targeted. UV stabilized. UL94 V2 rated. Injection moldable. Available in clear and in opaque colors | designed for applications with high optical requirements in terms of clarity and light transmission |
| PC | AVP TLL80CU | Sabic | LEXAN | wide specification polycarbonate. 20 MFR targeted. UV stabilized. UL94 V2 rated. Injection moldable. Available in clear. | |
| PC | AVP ZLL12CP | Sabic | LEXAN | wide specification polycarbonate. 12 MFR targeted. UL94 V2 rated. Available in limited opaque colors. | |
| PC | AVP ZLL19CU | Sabic | LEXAN | wide specification polycarbonate. 19 MFR targeted. UV stabilized. Available in limited opaque colors. | |
| PC | EM1210 | Sabic | LEXAN | Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions | Automotive interiors. |
| PC | EM3110 | Sabic | LEXAN | 20 MFR polycarbonate. Impact resistant at -20oC. UL94 HB rated. Optimized flow and processability for cost effective thinner wall designs. | for automotive interiors. |
| PC | EX1332T | Sabic | LEXAN | 3 MFR polycarbonate, MVR of 3. UV stabilized. Release agent. UL94 HB rated. | Designed for use in multi-wall sheet or profile extrusion applications. |
| PC | EX1632T | Sabic | LEXAN | 6 MFR polycarbonate, MVR of 6. UV stabilized. Release agent. UL94 HB rated. | Designed for use in multi-wall sheet or profile extrusion applications. |
| PC | EX5681T | Sabic | LEXAN | coextrusion product which is UV stabilized for improved outdoor weathering of LEXAN™ sheet and improved processing. | |
| PC | EX6681T | Sabic | LEXAN | coextrusion product which is UV stabilized for good outdoor weathering of LEXAN™ sheet and excellent processing. | |
| PC | EX7631T | Sabic | LEXAN | highly UV stabilized, 10 MFR polycarbonate. Release agent. | Suitable for co-extrusion / cap layers. Exhibits low plate out and improved outdoor weathering on PC sheets. |
| PC | EX7681T | Sabic | LEXAN | highly UV stabilized 10 MFR polycarbonate, MVR of 10. | Suitable for co-extrusion / cap layers. Exhibits low plate out and improved outdoor weathering on PC sheets. |
| PC | EX8681T | Sabic | LEXAN | coextrusion product which is highly UV stabilized | for improved outdoor weathering of LEXAN™ sheet and excellent processing. |
| PC | EX9332T | Sabic | LEXAN | MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retadant, mold release, UV stabilized, transparent, translucent and opaque colors. | Material typically used in railway applications and building & construction. Multiwall sheet, solid sheet, pipe, profiles |
| PC | GLX143 | Sabic | LEXAN | with MVR of 12. Medium viscosity grade. Excellent candidate. Available in transparent and translucent colors. | for applications with high optical quality requirements such as automotive glazing (vehicle windows). |
| PC | HF1110 | Sabic | LEXAN | 25 MFR polycarbonate. UL94 V2 rated. | |
| PC | HF1110R | Sabic | LEXAN | 25 MFR polycarbonate, MVR of 26. Mold release. UL94 V2 rated. | |
| PC | HF1130 | Sabic | LEXAN | 25 MFR polycarbonate. UV stabilized. UL94 V2 rated. | |
| PC | HF1130R | Sabic | LEXAN | 25 MFR polycarbonate, MVR of 26. UV stabilized. Mold release. UL94 V2 rated. | |
| PC | HF1140 | Sabic | LEXAN | 25 MFR polycarbonate, MVR of 26. Grade designed for food contact. UL94 V2 rated. | |
| PC | HF1140R | Sabic | LEXAN | 25 MFR polycarbonate, MVR of 26. Mold release. UL94 V2 rated. | |
| PC | HF1840R | Sabic | LEXAN | MVR (300°C/1.2kg) 36 cm3/10min, extreme low viscosity, injection molding, mold release, transparent. | This material is food contact compliant in most jurisdictions – exceptions may exist, request a declaration for details. |
| PC | HF3510R | Sabic | LEXAN | 39 MFR polycarbonate, MVR of 34. Mold release. Easy processing. Available only in opaque colors. | Suitable for automotive applications, including bezels |
| PC | HF4010SR | Sabic | LEXAN | excellent flow 42 MFR polycarbonate, MVR of 40. Superior release. High gloss. Available in opaque colors. | Suitable for large parts and thin wall molding. |
| PC | HFR1723 | Sabic | LEXAN | 25 MFR polycarbonate. UV stabilized. Mold release. UL94 V2 rated. | Available in transparent, limited package types, and must meet minimum order quantity requirements. |
| PC | HFR1724 | Sabic | LEXAN | 25 MFR polycarbonate. Grade designed for food contact. Mold release. UL94 V2 rated. | Available in transparent, limited package types, and must meet minimum order quantity requirements. |
| PC | IR1810 | Sabic | LEXAN | high flow (MFR = 22 at 300°C/1.2kg), heat stabilized | for use in the custom compounding market. |
| PC | IR1840 | Sabic | LEXAN | high flow (MFR = 22 at 300°C/1.2kg), heat stabilized | for use in the general purpose molding market. |
| PC | IR2040 | Sabic | LEXAN | 18 MFR polycarbonate, MVR of 21. Grade designed for food contact. Mold release. | Available in transparent, limited package types, and must meet minimum order quantity requirements. |
| PC | IR2110 | Sabic | LEXAN | medium-high flow (MFR = 15 at 300°C/1.2kg), heat stabilized | for use in the custom compounding market. |
| PC | IR2210 | Sabic | LEXAN | medium-low flow (MFR = 10 at 300°C/1.2kg), heat stabilized | for use in the custom compounding market. |
| PC | IR2240 | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 9. Grade designed for food contact. Mold release. | Available in transparent, limited package types, and must meet minimum order quantity requirements. |
| PC | IR2840 | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. Grade designed for food contact. Mold release. Injection moldable. | Available in transparent, limited package types, and must meet minimum order quantity requirements. |
| PC | LS1 | Sabic | LEXAN | 20 MFR polycarbonate, MVR of 21. UV stabilized. UL94 HB rated. UL746C f1 rated. Low viscosity. | For automotive lens applications. AMECA listed. |
| PC | LS2 | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 12. UV stabilized. UL94 HB rated. UL746C f1 rated. Medium viscosity. | For Automotive lens applications. AMECA listed. |
| PC | LSHF | Sabic | LEXAN | 25 MFR polycarbonate, MVR of 24. UV stabilized. | For Automotive lens applications. AMECA listed. |
| PC | LUX1619 | Sabic | LEXAN | 7.5 MFR polycarbonate. UL94 HB rated. | For high light reflectance. Extrudable and injection moldable. |
| PC | LUX2010T | Sabic | LEXAN | Injection moulding grade. Excellent flow properties combined with very high transmission and color stability. | especially designed for manufacturing optical parts |
| PC | LUX2110T | Sabic | LEXAN | Injection moulding grade. Easy flow properties combined with very high transmission and color stability. | especially designed for manufacturing optical parts |
| PC | LUX2114 | Sabic | LEXAN | 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. | |
| PC | LUX2114G | Sabic | LEXAN | 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. | |
| PC | LUX2289 | Sabic | LEXAN | 17 MFR polycarbonate, MVR of 16. UV stabilized. UL94 V2 rated. High light reflectance. Injection moldable. | |
| PC | LUX2614G | Sabic | LEXAN | diffusive, high viscosity, uv stabilized, flame retardant | Developed for injection molding LED applications |
| PC | LUX2619 | Sabic | LEXAN | extrusion grade. It is UL94 V-2 rated at 1.5 mm. | designed for high light reflectance. |
| PC | ML3729 | Sabic | LEXAN | an excellent flow polycarbonate with MVR of 36. UV stabilized. UL94 V2 rated. Easy processing. Available in transparent, translucent and opaque colors. | |
| PC | ML3729R | Sabic | LEXAN | 39 MFR polycarbonate, MVR of 36. UV stabilized. Mold release. UL94 V2 rated (US). Easy processing. | |
| PC | OQ1022 | Sabic | LEXAN | an optical quality polycarbonate. High purity resin. Produced in dedicated equipment with stringent production control conditions. | for CD, DVD and BD applications at short cycle times (not UV stabilized). |
| PC | OQ1028 | Sabic | LEXAN | an optical quality polycarbonate. High purity resin. Produced in dedicated equipment with stringent production control conditions. | for CD, DVD and BD applications at short cycle times (not UV stabilized). |
| PC | OQ2720 | Sabic | LEXAN | 7.5 MFR polycarbonate. UV stabilized. Produced in dedicated equipment with stringent production control conditions. Available in transparent and translucent colors. | For ophthalmic or safety lens market. |
| PC | OQ3420 | Sabic | LEXAN | 11 MFR polycarbonate. UV stabilized. Medium viscosity. | Designed for ophthalmic lenses. |
| PC | OQ3820 | Sabic | LEXAN | 7.4 MFR polycarbonate, MVR of 6. UV stabilized. High viscosity. | Designed for ophthalmic lenses. |
| PC | OQ4005 | Sabic | LEXAN | MVR of 8, UV-stabilized PC. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. | Suitable for sunglass and sunvisor markets. |
| PC | OQ4120R | Sabic | LEXAN | 25 MFR polycarbonate, MVR of 21. UV stabilized. Mold release. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. | Suitable for sunglass and sunvisor markets. |
| PC | OQ4320R | Sabic | LEXAN | 13 MFR polycarbonate. UV stabilized. Mold release. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. | Suitable for sunglass and sunvisor markets. |
| PC | OQ4820 | Sabic | LEXAN | polycarbonate with MVR 6. UV stabilized. Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. | Suitable for sunglass and sunvisor markets. |
| PC | PK2870 | Sabic | LEXAN | 2.5 MFR branched polycarbonate, MVR of 2. High viscosity. For blow molding, with high melt strength and high impact resistance. | Excellent candidate for water bottle applications. Available in transparent colors only. |
| PC | PU1230R | Sabic | LEXAN | 11 MFR polycarbonate, MVR of 12. UV stabilized. Medium viscosity. | Designed for Automotive trim applications, excellent PUR coating adhesion. |
| PC | PU2030R | Sabic | LEXAN | 17 MFR polycarbonate, MVR of 18. UV stabilized. Low viscosity. | Designed for Automotive trim applications, excellent PUR coating adhesion. |
| PC | T5R141RC | Sabic | LEXAN | ETP compound, which is formulated with 50wt% post-consumer recycled plastics. | |
| PC | VR1820 | Sabic | LEXAN | high flow (MFR = 22 at 300°C/1.2kg), heat and UV stabilized, polycarbonate product with mold release | designed for use in the general purpose molding market. |
| PC | VR2020 | Sabic | LEXAN | 18 MFR polycarbonate, MVR of 17. UV stabilized. Mold release. UL746C f1 rated. Available in transparent, limited package types, and must meet minimum order quantity requirements. | |
| PC | VR2220 | Sabic | LEXAN | 12 MFR polycarbonate, MVR of 11. UV stabilized. Mold release. UL746C f1 rated. Available in transparent, limited package types, and must meet minimum order quantity requirements. | |
| PC | VR2820 | Sabic | LEXAN | 7 MFR polycarbonate, MVR of 6. UV stabilized. Mold release. Injection moldable. | Available in transparent, limited package types, and must meet minimum order quantity requirements. |
| PC | XLS1110 | Sabic | LEXAN | 35 MVR polycarbonate. | Designed for automotive optical parts requiring excellent flow properties, very high transmission and color stability. AMECA listed for protected applications only. |
| PC | XLS1110T | Sabic | LEXAN | 35 MVR polycarbonate. | Designed for automotive optical parts requiring excellent flow properties, very high transmission and color stability. AMECA listed for protected applications only. |
| PC | XLS1210 | Sabic | LEXAN | 18 MVR polycarbonate. | Designed for automotive optical parts requiring very high transmission and color stability. AMECA listed for protected applications only. |
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | PC1080C-70 | LG Chem | / | General Purpose Grade. Coloring, High Transparency, Ultra High Flow | Compound, CD,DVD, E&E Others |
| PC | PC1300-03 | LG Chem | / | General Purpose Grade. Coloring, High Impact Resistance, High Transparency | Compound, Sheet/Flim |
| PC | PC1300-08 | LG Chem | / | General Purpose Grade. Coloring, High Impact Resistance, High Transparency | Compound, Sheet/Flim |
| PC | PC1300-10 | LG Chem | / | General Purpose Grade. Coloring, High Impact Resistance, High Transparency | Others, Sheet/Flim |
| PC | PC1300-15 | LG Chem | / | General Purpose Grade. Coloring, High Flow, High Transparency | Compound, Sheet/Flim |
| PC | PC1300-22 | LG Chem | / | General Purpose Grade. Coloring, High Flow, High Transparency | Compound, Sheet/Flim |
| PC | PC1300-30 | LG Chem | / | General Purpose Grade. Coloring, High Flow, High Transparency | Compound, Sheet/Flim |
| PC | PC1201HP-08 | LG Chem | / | Extrusion grade. FDA, Good Mold Release, High Impact Resistance, High Transparency | Compound, Sheet/Flim, Food Packaging, E&E Others |
| PC | PC1302-05 | LG Chem | / | Extrusion grade. High Impact Resistance, High Transparency, Weather Resistance | |
| PC | PC1303HP-08 | LG Chem | / | Extrusion grade. Good Mold Release, High Transparency, Weather Resistance | Sheet/Flim, Multiwall Sheet, Sundry Goods |
| PC | PC1201-10P | LG Chem | / | injection molding grade. FDA, Good Mold Release, High Impact Resistance, High Transparency | Sheet/Flim, Vacuum Cleaner, E&E Others |
| PC | PC1201-15 | LG Chem | / | injection molding grade. FDA, Good Mold Release, High Flow, High Transparency | Compound, Food Packaging, Vacuum Cleaner, E&E Others,Sundry Goods |
| PC | PC1201-22 | LG Chem | / | injection molding grade. FDA, Good Mold Release, High Flow, High Transparency | Compound, Food Packaging, Vacuum Cleaner, E&E Others,Sundry Goods |
| PC | PC1201-22C | LG Chem | / | injection molding grade. FDA, Good Mold Release, High Flow, High Transparency | Compound, Food Packaging, Vacuum Cleaner, E&E Others,Sundry Goods |
| PC | PC1301EP-30 | LG Chem | / | injection molding grade. Good Mold Release, High Flow, High Transparency | Washing Machine, CD,DVD, E&E Others, Sundry Goods |
| PC | PC1303-10C | LG Chem | / | injection molding grade. Good Mold Release, High Impact Resistance, High Transparency, Weather Resistance | Auto Lens, Auto Others, E&E Others, Sundry Goods |
| PC | PC1303AH-10 | LG Chem | / | injection molding grade. Good Mold Release, High Impact Resistance, High Transparency, Weather Resistance | Auto Lens |
| PC | PC1303AH-15 | LG Chem | / | injection molding grade. Good Mold Release, High Flow, High Transparency, Weather Resistance | Auto Lens, Auto Others, E&E Others, Sundry Goods |
| PC | PC1303AH-22 | LG Chem | / | injection molding grade. Good Mold Release, High Flow, High Transparency, Weather Resistance | Auto Lens, Auto Others, E&E Others, Sundry Goods |
| PC | PC1303EP-22 | LG Chem | / | injection molding grade. Good Mold Release, High Flow, High Transparency, Weather Resistance | Vacuum Cleaner, E&E Others |
| PC | PC8000-05 | LG Chem | / | Silicon copolymer. Chemical Resistance, High Impact Resistance, Low Haze, Low Temp. Impact Resistance | Compound |
| PC | PC8010-10 | LG Chem | / | Silicon copolymer. Chemical Resistance, High Impact Resistance, Low Haze, Low Temp. Impact Resistance | Compound |
| PC | PC1301V-10 | LG Chem | / | high performance characteristics. Good Mold Release, High Impact Resistance, High Transparency, Non-Halogen | E&E Others, Sundry Goods |
| PC | PC1302UV-05 | LG Chem | / | high performance characteristics. High Impact Resistance, High Transparency, UV Cut_Off, Weather Resistance | Goggles, Sunglass, E&E Others, Sundry Goods |
| PC | PC1303UV-08 | LG Chem | / | high performance characteristics. Good Mold Release, High Impact Resistance, High Transparency, UV Cut_Off, Weather Resistance | Goggles, Sunglass, E&E Others, Sundry Goods |
| Type | Grade No. | Manufacturer | Brand | Key Features | Typical Applications |
|---|---|---|---|---|---|
| PC | HS102R | Huasheng | / | Medium viscosity, Good demolding performance | General use |
| PC | HS102U | Huasheng | / | Medium viscosity, Good demolding performance, UV resistance | General use |
| PC | HS032S | Huasheng | / | High viscosity, Good thermal stability | Drinking water bucket |
| PC | HS033S | Huasheng | / | High viscosity, Good thermal stability | Drinking water bucket |
Explore Resources
- Flame Retardant Grade PC
- General Purpose Grade PC
- Optical Grade PC
- Weather Resistant Grade PC
- Food Contact Grade PC
- Medical Grade PC
What is PC Resin?
PC (Polycarbonate) resin is a high-performance engineering plastic renowned for its exceptional combination of strength, transparency, and heat resistance. This versatile material offers solutions for a wide range of industries, from automotive to electronics and beyond.
Other Names
- Polycarbonate Resin
- PC Polymer
- PC Plastic
- Transparent PC
- PC Pellets
- PC Granules
Appearance
- Transparent
- Light amber (natural color)
- High-gloss finish
Packaging
- 25kg bags or jumbo bags
- Palletized for bulk shipping
HS Code
- 39074000
Key Properties of PC Resin
- High impact strength (250 times stronger than glass)
- Excellent transparency (up to 90% light transmission)
- Good dimensional stability
- Heat resistance up to 135°C
- Flame retardant grades available (UL94 V-0)
- Easy to process via injection molding and extrusion
Processing Features
- Manufacturing Versatility: Suitable for injection molding, extrusion, thermoforming, and blow molding.
- Advanced Grades: Enhancements include flame retardancy, UV resistance, and scratch-resistant coatings.
- Material Blending: Customizable blends (e.g., PC/ABS) for tailored properties.
- Sustainability: Recyclable for environmentally conscious applications.
Frequently Ask Questions
Find answers to the most common questions about PC resin. Our expert responses help you make informed sourcing and application decisions.
Yes, polycarbonate is often blended with resins like ABS, PBT, or PET to achieve improved performance properties. For example, PC/ABS blends combine the toughness of polycarbonate with the processability of ABS, making the material suitable for applications like automotive interiors and electronics housing.
PC stands out among engineering plastics due to its combination of optical clarity and high mechanical performance. Key distinguishing factors include:
- Exceptional Toughness: PC’s impact resistance is significantly higher than many other transparent plastics, making it ideal for safety and protective applications.
- Versatility in Processing: It can be processed by injection molding, extrusion, and thermoforming, with a consistent melt flow index (MFI) that offers reliable predictability during manufacturing.
- Balanced Thermal and Mechanical Properties: Its high glass transition temperature and rigidity make it suitable for applications requiring long-term durability under varying temperature conditions.
These data points are reflected in comparative studies and standardized test results across the polymer industry.
Quality control in PC production is critical to maintain its high-performance characteristics. Manufacturers typically employ several measures, including:
- Raw Material Verification: Only high-grade bisphenol A (BPA) and phosgene derivatives, or BPA alternatives, are used, with strict supplier certifications in place.
- In-Process Monitoring: Key parameters such as reaction temperature, pressure, and viscosity are continuously monitored to ensure a uniform product.
- Standardized Testing: Final products undergo rigorous testing (ASTM D790 for flexural properties and ASTM D256 for impact resistance) to verify that they meet established industry standards.
- Certifications: Many PC products are certified to meet international standards like ISO 9001 and are compliant with industry-specific safety requirements.
These procedures ensure that each batch of PC consistently meets the technical specifications and quality expectations demanded by various applications.
Standard PC is made from BPA, but we offer BPA-free grades upon request, especially for food-contact and medical applications.
MOQ varies by grade. For standard PC resin, our MOQ starts at 1 ton. Contact us for details.
The manufacturing of PC relies on carefully selected raw materials and catalysts:
- Bisphenol A (BPA): Serves as the primary monomer, offering the backbone for the polymer structure.
- Phosgene: A reactive compound that facilitates the linking of BPA molecules to form high-molecular-weight PC.
- Catalysts: Tertiary amines or quaternary ammonium salts are commonly used to accelerate the reaction while ensuring high quality and consistency in the final product.
Each of these components is chosen for purity and performance, with supplier quality verification ensuring that they meet stringent industry criteria.
Yellowing can be minimized by using UV-blocking additives or coatings, selecting grades with inherent UV resistance, and limiting prolonged exposure to direct sunlight. Regular maintenance and cleaning with appropriate materials can also help slow the yellowing process.
PC Resin is hygroscopic, meaning it absorbs moisture from the air, which can impact its properties during molding or extrusion. Therefore, it is crucial to thoroughly dry the resin before processing. Failure to do so can lead to defects such as bubbling or reduced mechanical properties in the final product.
Key factors include the application’s requirements for impact resistance, transparency, UV stability, temperature tolerance, moldability, and compliance with regulatory standards (such as FDA or medical-grade requirements). Additionally, consider if advanced properties like flame retardancy or color stability are necessary.
Given the use of hazardous chemicals such as phosgene in PC production, strict environmental and safety protocols are in place:
- Containment Systems: Enclosed production environments minimize the risk of toxic exposures and accidental releases.
- Emission Controls: Advanced scrubbers and filtration systems capture and neutralize any harmful emissions, ensuring compliance with environmental regulations.
- Waste Management: By-products and residues are treated according to strict guidelines, with recycling and proper disposal practices in effect.
- Regulatory Compliance: Facilities adhere to international safety standards, including OSHA and EPA guidelines, with regular audits to maintain these standards.