PMMA Resin Plastic Pellets
- Home /
- PMMA Resin
PMMA
At Suke Plastics, we mainly supply:
- Chimei Acryrex® PMMA CM-205
- Chimei Acryrex® PMMA CM-207
- Chimei Acryrex® PMMA CM-211
Supply Various Grades of PMMA pellets
| Type | Grade No. | Manufacturer | Brand | Grade/Features | Use/Application |
|---|---|---|---|---|---|
| PMMA | CM-205 | Chi Mei | Acryrex | Transparent Grade. Heat resistant / High strength / Extrusion | Car lights / Lenses / Home appliance components |
| PMMA | CM-207 | Chi Mei | Acryrex | Transparent Grade. Medium Strength / Flowability | Daily necessities / Home appliance parts |
| PMMA | CM-211 | Chi Mei | Acryrex | Transparent Grade. High flow/Processability | Daily necessities/Home appliance parts |
What is PMMA Resin?
PMMA (Polymethyl Methacrylate) resin is a transparent thermoplastic often used as a lightweight or shatter-resistant alternative to glass. It is known for its excellent optical clarity, weather resistance, and surface hardness.
Other Names
- Acrylic Resin
- Organic Glass
- Plexiglass Resin
- Lucite
- Perspex
- Polymethyl Methacrylate
Appearance
- Transparent or translucent granules
- Can be colorless or slightly tinted depending on grade
Packaging
- 25kg bags or jumbo bags
HS Code
- 39061000
Key Properties of PMMA Resin
- Exceptional optical clarity and transparency (up to 92% light transmission)
- Excellent weather and UV resistance
- High surface hardness and scratch resistance
- Good dimensional stability and rigidity
- Easy processing by injection molding and extrusion
- Available in transparent, translucent, or colored grades
Technical Data
| Property | General Grade |
|---|---|
| Density (g/cm³) | 1.17 – 1.20 g/cm³ |
| Tensile Strength (MPa) | 50 – 75 MPa |
| Flexural Modulus (MPa) | 2500 – 3500 MPa |
| Izod Impact Strength | 1 – 3 kJ/m² |
| Heat Deflection Temp (°C) | 95 – 105°C |
| Melt Flow Index (MFI) | 1 – 20 g/10 min |
Applications of PMMA Resin
- Automotive lighting components and instrument panels
- Light guide panels and LED diffusers
- Signage and advertising displays
- Optical lenses and protective screens
- Sanitary ware, bathtubs, and shower enclosures
- Consumer goods: furniture, cosmetics packaging, etc.
- Medical devices and dental prosthetics
- Acrylic sheets and 3D printing filament (PMMA-grade)
PMMA Resin Grades We Offer
- Injection Molding Grade
- Extrusion Grade
- Optical Grade
- Weather-Resistant Grade
- Impact-Modified Grade
- High Flow Grade
- Sheet Grade