PP Impact Copolymer Pellets

Impact Copolymer PP

PP Impact Copolymer (PP-IC) is a polypropylene resin modified with ethylene-propylene rubber phase to improve toughness and impact resistance. It is tougher and less brittle than standard PP homopolymer, especially at low temperatures.

Suke Plastics supplies PP impact copolymer grades from these producers:

  • CNOOC Shell (CS) Davance™ PP
  • FORMOSA (FCFC) TAIRIPRO® PP
  • FORMOSA (FPC)  YUNGSOX® PP
  • Lotte Chemical Starex® PP
  • Sinochem (Quan Zhou) Fuya® PP
  • Hyosung Topilene® PP
pp impact copolymer granules

Supply PP Impact Copolymer pellets


TypeGrade No.ManufacturerBrandGrade/FeaturesUse/Applications
PP (Impact Copolymer PP)K8025FORMOSA (FCFC)TairiproHigh impact strength, high fluidityAutomotive parts, washing machine parts, tool boxes
PP (Impact Copolymer PP)K3029FORMOSA (FCFC)TairiproHigh fluidity, high impact strengthBumpers, automotive parts, thin-wall products
PP (Impact Copolymer PP)K7005AGFORMOSA (FCFC)TairiproHigh impact strength, high stiffness, good light stabilityAutomotive parts, furniture, appliances, pallets, crate containers
PP (Impact Copolymer PP)K7005ANFORMOSA (FCFC)TairiproHigh impact strength, high stiffnessAutomotive parts, furniture, appliances
PP (Impact Copolymer PP)K7009FORMOSA (FCFC)TairiproHigh stiffness, good impact strengthAutomotive parts, furniture, appliances
PP (Impact Copolymer PP)K7009AHFORMOSA (FCFC)TairiproLong-term thermal aging, high stiffness, good impact strengthElectric appliance parts, automotive parts, RTI = 125℃
PP (Impact Copolymer PP)K7025FORMOSA (FCFC)TairiproHigh fluidity, high impact strengthWashing machine cylinders, appliances
PP (Impact Copolymer PP)K8003FORMOSA (FCFC)TairiproHigh impact strength, good stiffnessBaby-car parts, paint drums, sports appliances, luggage bases
PP (Impact Copolymer PP)K8003ANFORMOSA (FCFC)TairiproExcellent impact strength, high stiffness, excellent anti-static performancePaint drums, sports appliances, luggage bases
PP (Impact Copolymer PP)K8009FORMOSA (FCFC)TairiproHigh impact strength, good fluidityAutomotive parts, battery cases, electrical appliances, furniture
PP (Impact Copolymer PP)K8050FORMOSA (FCFC)TairiproHigh fluidity, good impact strength, high stiffness, low warpageWashing machines, storage boxes, thin-wall products
PP (Impact Copolymer PP)K8065FORMOSA (FCFC)TairiproHigh fluidity, good impact strength, high stiffness, low warpageWashing machines, storage boxes, thin-wall products
PP (Impact Copolymer PP)K8095FORMOSA (FCFC)TairiproHigh fluidity, good impact strength, good stiffnessAutomotive parts
PP (Impact Copolymer PP)K8802FORMOSA (FCFC)TairiproHigh impact strength, excellent resistance to low-temperature brittleness, good lusterSuitcase parts
PP (Impact Copolymer PP)K9010FORMOSA (FCFC)TairiproHigh impact strength, good fluidityAutomotive parts
PP (Impact Copolymer PP)K9017FORMOSA (FCFC)TairiproHigh impact strength, good fluidity, anti-UV additiveAutomotive parts
PP (Impact Copolymer PP)K9030FORMOSA (FCFC)TairiproHigh fluidity, high impact strengthBumpers, automotive parts, thin-wall products
PP (Impact Copolymer PP)KP03BFORMOSA (FCFC)TairiproHigh fluidity, good impact strengthAutomotive parts, storage boxes, thin-wall products
PP (Impact Copolymer PP)B8001FORMOSA (FCFC)TairiproHigh impact strength, excellent resistance to low-temperature brittleness, good lusterPP pipes, thermoforming sheets, blow molding
PP (Impact Copolymer PP)B8001A3FORMOSA (FCFC)TairiproExcellent impact strength, excellent resistance to low-temperature brittlenessPP-B pipes, thermoforming sheets, blow molding
PP (Impact Copolymer PP)T8002FORMOSA (FCFC)TairiproHigh impact strength, excellent resistance to low-temperature brittleness, good lusterCorrugated sheets, bottles, thermoforming sheets
PP (Impact Copolymer PP)H3030FSinochem (Quan Zhou)FuyaHigh rigidity, exceptional transparency, superior processability, pristine purityHigh-value packaging, including glossy, matte, and pearlescent films
PP (Impact Copolymer PP)L5E89Sinochem (Quan Zhou)FuyaChemical resistance, abrasion resistanceWoven bags, color-striped tarpaulins, carpet backing, FIBCs, tarpaulins, ropes, and packaging for grains, fertilizers, sugar, salt, industrial materials, and mineral sands
PP (Impact Copolymer PP)VI-6120NLotte ChemicalStarexMineral-fiber-reinforced 20%, non-halogenHome appliances, electrical components
PP (Impact Copolymer PP)VI-6220NLotte ChemicalStarexFlame-retardant grade, non-halogenE&E applications
PP (Impact Copolymer PP)VP-6020NHLotte ChemicalStarexFlame-retardant grade, non-halogenHome appliances and electronics
PP (Impact Copolymer PP)3003FORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittleness, excellent melt strengthPPB pipes
PP (Impact Copolymer PP)3004FORMOSA (FPC)YUNGSOXHigh impact strength, good resistance to stress whitening, excellent resistance to low-temperature brittleness, excellent melt strengthSports appliances, luggage bases, thermoforming sheets, blow molding
PP (Impact Copolymer PP)3005FORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittleness, excellent melt strengthThermoforming sheets, blow molding
PP (Impact Copolymer PP)3010FORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittleness, good stiffnessCorrugated sheets, blow molding
PP (Impact Copolymer PP)3015FORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittleness, good stiffnessPails, sports appliances, luggage bases, heavy-duty containers
PP (Impact Copolymer PP)3015SFORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittleness, excellent heat-sealing strength, low fish-eye level, excellent process stabilityRetort films, CPP films, ALF, aluminum laminate films
PP (Impact Copolymer PP)3040FORMOSA (FPC)YUNGSOXMedium impact strengthAutomotive parts, electric appliance parts, toys, battery cases, furniture
PP (Impact Copolymer PP)3040CFORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittleness, good stiffnessPails, sports appliances, luggage bases, heavy-duty containers
PP (Impact Copolymer PP)3064HFORMOSA (FPC)YUNGSOXHigh stiffness, high heat resistance, high impact strengthAutomotive parts, electric appliance parts, toys, battery cases, furniture
PP (Impact Copolymer PP)3080FORMOSA (FPC)YUNGSOXMedium impact strengthAutomotive parts, electric appliance parts, battery cases, furniture
PP (Impact Copolymer PP)3080PFORMOSA (FPC)YUNGSOXMedium impact strength, excellent heat-sealing strength, low fish-eye level, excellent process stabilityProtective films, CPP films
PP (Impact Copolymer PP)3084FORMOSA (FPC)YUNGSOXMedium impact strengthAutomotive parts, electric appliance parts, battery cases, furniture
PP (Impact Copolymer PP)3084HFORMOSA (FPC)YUNGSOXHigh stiffness, high heat resistance, medium impact strengthElectric appliance parts, automotive parts, battery cases
PP (Impact Copolymer PP)3090FORMOSA (FPC)YUNGSOXMedium impact strengthAutomotive parts, electric appliance parts, battery cases, furniture
PP (Impact Copolymer PP)3155FORMOSA (FPC)YUNGSOXHigh gloss, good resistance to stress whiteningAutomotive parts, electric appliance parts, furniture, luggage
PP (Impact Copolymer PP)3200WFORMOSA (FPC)YUNGSOXHigh gloss, high fluidity, high impact strengthLuggage, automotive parts, furniture
PP (Impact Copolymer PP)3204FORMOSA (FPC)YUNGSOXHigh fluidity, medium impact strengthLarge automotive parts, electric appliance parts, washing machine parts, tool boxes, storage boxes, thin-wall products
PP (Impact Copolymer PP)3300NFORMOSA (FPC)YUNGSOXHigh fluidity, medium impact strength, uniform shrinkageLarge automotive parts, electric appliance parts, washing machine parts, tool boxes, storage boxes, thin-wall products
PP (Impact Copolymer PP)3354FORMOSA (FPC)YUNGSOXHigh fluidity, medium impact strengthLarge automotive parts, electric appliance parts, washing machine parts, tool boxes, storage boxes, thin-wall products
PP (Impact Copolymer PP)3504FORMOSA (FPC)YUNGSOXSuperhigh fluidity, high stiffness, high heat resistanceLarge automotive parts, electric appliance parts, washing machine parts, storage boxes, thin-wall products
PP (Impact Copolymer PP)3600NFORMOSA (FPC)YUNGSOXSuperhigh fluidity, high stiffness, high heat resistance, uniform shrinkageLarge automotive parts, electric appliance parts, washing machine parts, storage boxes, thin-wall products
PP (Impact Copolymer PP)4084FORMOSA (FPC)YUNGSOXHigh impact strength, excellent resistance to low-temperature brittlenessBumpers, automotive parts, heavy-duty containers, pallets
PP (Impact Copolymer PP)4204FORMOSA (FPC)YUNGSOXHigh fluidity, high impact strength, excellent resistance to low-temperature brittlenessBumpers, automotive parts, heavy-duty containers, pallets
PP (Impact Copolymer PP)4304FORMOSA (FPC)YUNGSOXHigh fluidity, high impact strength, excellent resistance to low-temperature brittlenessBumpers, automotive parts, heavy-duty containers, pallets
PP (Impact Copolymer PP)4604FORMOSA (FPC)YUNGSOXHigh fluidity, high impact strength, excellent resistance to low-temperature brittlenessBumpers, automotive parts, heavy-duty containers, pallets
PP (Impact Copolymer PP)EP548R-ZCNOOC Shell (CS)Davance™High stiffness-to-impact balanceHousewares and furniture, toys and leisure products, washing machine components, packaging
PP (Impact Copolymer PP)J340HyosungTopilene®Good stiffness-impact balance, Excellent surface propertyCorrugated sheet, Solid sheet

Key Features

  • Better Low-Temperature Impact

    The rubber phase improves toughness at cold temperatures. It helps reduce cracking in containers, automotive parts, and industrial products.

  • Balanced Stiffness and Durability

    PP impact copolymer offers moderate stiffness with higher toughness. It suits parts exposed to handling, dropping, or mechanical stress.

  • Suitable for Multiple Processes

    Grades can be used in injection molding, extrusion, thermoforming, and blow molding. MFI selection depends on wall thickness and cycle speed.

Applications

PP Impact Copolymer is commonly used in:

  • Automotive bumpers and trims
  • Battery cases
  • Industrial storage boxes
  • Pallets and buckets
  • Toys and sporting goods
  • Appliance housings
  • Durable containers
  • Packaging tools
  • Luggage and impact-resistant consumer goods

Frequently Ask Questions

Find answers to the most common questions about PP Impact Copolymer resin. Our expert responses help you make informed sourcing and application decisions.

What makes PP Impact Copolymer different from PP

PP impact copolymer contains a rubbery ethylene-propylene phase. This improves impact strength and low-temperature toughness. PP homopolymer is stiffer and has better heat resistance, but it is more brittle in cold conditions.

What MFI should I choose for PP impact copolymer?

Low MFI grades are suitable for extrusion, pallets, buckets, and thick-wall products. Medium MFI grades are used for general injection molding. High MFI grades support faster cycles and thin-wall molded products.

What are typical mechanical properties of PP impact copolymer?

Typical density is about 0.90–0.91 g/cm³. Typical tensile strength is 20–30 MPa. Flexural modulus is around 800–1500 MPa. Impact strength varies widely by grade and rubber content.

Can PP impact copolymer be used at low temperatures?

Yes. It performs better than PP homopolymer at low temperatures. Many grades can work in applications requiring toughness around -20°C to -30°C, depending on the specific formulation.

Is PP impact copolymer suitable for automotive parts?

Yes. It is widely used in automotive bumpers, interior trims, battery cases, and under-the-hood components. Buyers should confirm impact strength, heat resistance, shrinkage, and OEM requirements before ordering.

Does PP impact copolymer need UV stabilizers for outdoor use?

Yes, for long-term outdoor exposure. Standard grades may degrade under sunlight. UV-stabilized grades or compounded materials are recommended for outdoor containers, automotive parts, and exposed components.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.