Covestro Bayblend® FR3021
Bayblend® FR3021 PC/ABS Resin Covestro Bayblend FR3021 is a mineral-reinforced, flame-retardant PC+ABS blend engineered for high-stiffness applications. With UL 94 V-0 certification at 1.5mm, exceptional dimensional stability (tensile modulus: 4800 MPa), and thermal resilience (Vicat 98°C), it ensures safety and reliability in demanding environments. Key technical data (ISO) Download Application Features & Benefits Related Apec®
Covestro Bayblend® FR3021 Read More »