Plastic Granules
BASF ULTRAMID 8202HS BK102 Black Color PA6 Resin
Ultramid® 8202HS BK102 is a versatile, heat-stabilized Nylon Polyamide 6 resin by BASF. Designed for injection molding, this low-viscosity material offers an excellent combination of strength, toughness, and chemical resistance, making it ideal for precision components and thin-profile products.
Typical property data
Physical Properties
- Density: 1130 kg/m³ (ISO 1183)
- Water Absorption: Saturation in water at 23 °C: 9.5% (similar to ISO 62)
- Moisture Absorption: Equilibrium at 23 °C and 50% r.h.: 2.7% (similar to ISO 62)
Mechanical Properties
- Tensile Modulus: 3100 MPa / 970 MPa (ISO 527-1/-2)
- Yield Stress: 85 MPa / 36 MPa (ISO 527-1/-2)
- Yield Strain: 4% / 16% (ISO 527-1/-2)
- Nominal Strain at Break: 25% / >50% (ISO 527-1/-2)
Impact Properties
- Charpy Notched Impact Strength (23 °C): 3 kJ/m² (ISO 179/1eA)
Thermal Properties
- Melting Temperature (DSC): 220 °C (ISO 11357-1/-3)
- Deflection Temperature under Load (1.8 MPa, HDT A): 60 °C (ISO 75-1/-2)
Electrical Properties
- Volume Resistivity: >1E13 Ω·m (IEC 62631-3-1)
Flame Characteristics
- UL94 Flammability Rating: V-2 (for 0.7 mm thickness, IEC 60695-11-10)
Process Guide
- Processing Temperature: Melting temperature is 220 °C (ISO 11357-1/-3).
Features & Benefits
Heat Stabilized for High-Temperature Durability
Ultramid® 8202HS BK102 retains its strength and properties even in elevated temperatures. This makes it suitable for demanding environments like manufacturing gears or automotive components.
Superior Flow for Thin-Wall Molding
The low viscosity of this resin ensures it easily fills thin walls and intricate designs during injection molding.
Exceptional Chemical and Abrasion Resistance
Ultramid® 8202HS BK102 stands strong against harsh chemicals and abrasions, extending the lifespan of parts such as handles, fittings, and fasteners.
Use & Applications
- Automotive: Gear wheels, casings, and connectors.
- Industrial Equipment: Bearings, casters, and fasteners in factory operations.