BASF Ultramid® A3UG5

basf nylon pa resin 25kg package

BASF ULTRAMID A3UG5 Nylon PA66 Resin

Ultramid® A3UG5 is a high-performance PA66 resin reinforced with 25% glass fiber. Featuring halogen-free flame retardance, ultra-low phosphorus content, and excellent oil resistance, it’s specially designed to tackle demanding industrial and electronic environments with reliability and ease.

Associated Documents

TDS - Data Sheet
SDS - Safety Data Sheet
Processing Data

Typical property data

Physical Properties
  • Density: 1390 kg/m³ (ISO 1183)
  • Water Absorption (Saturation in Water at 23°C): 4%−4.6% (similar to ISO 62)
  • Moisture Absorption (Equilibrium at 23°C/50% RH): 1.1%−1.5% (similar to ISO 62)
Mechanical Properties
  • Tensile Modulus (Dry/Conditioned): 9500/6100 MPa (ISO 527-1/-2)
  • Stress at Break (Dry/Conditioned): 145/90 MPa (ISO 527-1/-2)
  • Strain at Break (Dry/Conditioned): 3%/5% (ISO 527-1/-2)
  • Flexural Modulus (Dry/Conditioned): 9500/6100 MPa (ISO 178)
  • Flexural Strength (Dry/Conditioned): 230/160 MPa (ISO 178)
Impact Properties
  • Charpy Unnotched Impact Strength at 23°C: 65 kJ/m² (ISO 179/1eU)
  • Charpy Notched Impact Strength at 23°C: 7.5/9 kJ/m² (Dry/Conditioned, ISO 179/1eA)
Thermal Properties
  • Melting Temperature (DSC): 260 °C (ISO 11357-1/-3)
  • Deflection Temperature under Load (1.8 MPa, HDT A): 245 °C (ISO 75-1/-2)
  • Deflection Temperature under Load (0.45 MPa, HDT B): 260 °C (ISO 75-1/-2)
  • High-Temperature Limit (20,000 h, with 50% Tensile Strength Retention): 130 °C (IEC 60216)
  • High-Temperature Limit (5000 h, with 50% Tensile Strength Retention): 155 °C (IEC 60216)
  • Coefficient of Thermal Expansion:
    • Parallel: 28×(E-6/K) (ISO 11359-1/-2)
    • Normal: 72×(E-6/K (ISO 11359-1/-2)
Electrical Properties
  • Relative Permittivity (1 MHz, Dry/Conditioned): 3.8/4.6 (IEC 62631-2-1)
  • Dissipation Factor (1 MHz, Dry/Conditioned): 170×(E-4) / 1000×(E-4) (IEC 62631-2-1)
  • Volume Resistivity (Dry/Conditioned): 1E13 / 1E10 (IEC 62631-3-1)
  • Surface Resistivity (Conditioned): 1E13 (IEC 62631-3-2)
  • Comparative Tracking Index (CTI): 600 (IEC 60112)
  • Electric Strength (Dry/Conditioned): 40 / 37 kV/mm (IEC 60243-1)
Flame Characteristics
  • Flammability (UL 94):
    • V−0, Thickness: 0.75 mm, All Colors
    • V−0, 5VAV, Thickness: 1.5 mm, \text{BK & GY Only}
  • Glow-Wire Flammability Index (GWFI): 960 °C at 0.75 mm thickness (IEC 60695-2-12)
Processing Guide
  • Melt Temperature for Injection Molding/Extrusion: 280−300 °C
  • Mold Temperature for Injection Molding: 80−90 °C
  • Melt Volume Rate (MVR): 25 cm³/10min at 275 °C, 5 kg (ISO 1133)
  • Shrinkage:
    • Parallel: 0.4% (ISO 294-4)
    • Normal: 1.2% (ISO 294-4)

Features & Benefits

Outstanding Strength and Durability

Reinforced with 25% glass fiber, Ultramid® A3UG5 delivers superior mechanical properties to support heavy-duty applications.

Halogen-Free Flame Retardance

Achieving UL 94 V-0 classification, it ensures fire safety while meeting health and environmental compliance standards.

Excellent Oil Resistance

Low phosphorus formulation minimizes corrosion risks in electrical contacts, ensuring longevity in harsh operating environments.

basf nylon pa resin 25kg package

Use & Applications

  • Electrical & Electronics: Circuit breakers, switchgear, and insulating housings for enhanced safety and performance.
  • Automotive: Oil sumps, engine covers, and components exposed to elevated temperatures and lubricants.
  • Industrial Equipment: High-strength housings and parts for machinery operating in challenging environments.