BASF ULTRAMID B3WG3

basf nylon pa resin 25kg package

BASF ULTRAMID B3WG3 Nylon PA66 Resin

Ultramid® B3WG3 is a 15% glass fiber-reinforced, heat-stabilized PA66 resin offering exceptional strength, dimensional stability, and oil resistance. Ideal for automotive and industrial uses, it ensures reliable performance in high-temperature and demanding environments.

Associated Documents

TDS - Data Sheet
SDS - Safety Data Sheet
Processing Data

Typical property data

Physical Properties
  • Density: 1230 kg/m³ (ISO 1183)
  • Water Absorption, Saturation in Water at 23°C: 8% (similar to ISO 62)
  • Moisture Absorption, Equilibrium at 23°C/50% Relative Humidity: 2.6%
Mechanical Properties
  • Tensile Modulus: 5800 MPa (dry) (ISO 527-1/-2)
  • Stress at Break: 130 MPa (dry) (ISO 527-1/-2)
  • Strain at Break: 3.5% (dry) (ISO 527-1/-2)
  • Flexural Modulus: 5300 MPa (dry) (ISO 178)
  • Flexural Strength: 200 MPa (dry) (ISO 178)
Impact Properties
  • Charpy Unnotched Impact Strength (23°C): 50 kJ/m² (ISO 179/1eU)
  • Charpy Unnotched Impact Strength (-30°C): 45 kJ/m² (ISO 179/1eU)
  • Charpy Notched Impact Strength (23°C): 6 kJ/m² (ISO 179/1eA)
  • Charpy Notched Impact Strength (-30°C): 5 kJ/m² (ISO 179/1eA)
Thermal Properties
  • Deflection Temperature Under Load, 1.8 MPa (HDT A): 195°C (ISO 75-1/-2)
  • Deflection Temperature Under Load, 0.45 MPa (HDT B): 218°C (ISO 75-1/-2)
Electrical Properties
  • Volume Resistivity: >1E13 Ohm·m (dry) (IEC 62631-3-1)
Processing Guide
  • Melt Temperature (Injection Moulding/Extrusion): 250–270°C
  • Mould Temperature: 80–90°C
  • MVR (275°C/5kg): 65 cm³/10min (ISO 1133)
  • Moulding Shrinkage (Constrained): 0.45%

Features & Benefits

Reinforced for Superior Strength

Ultramid® B3WG3’s 15% glass fiber reinforcement delivers high tensile and flexural strength, making it perfect for load-bearing applications.

Engineered for Heat Resistance

Heat-stabilized to withstand temperatures up to 218°C, it offers reliable performance in challenging, high-temperature environments.

Oil Resistance for Longevity

Designed to resist oil degradation, Ultramid® B3WG3 ensures durability in automotive components, industrial machinery, and heavy-duty equipment.

basf nylon pa resin 25kg package

Use & Applications

1. Automotive Industry
2. Industrial Equipment
3. Consumer Goods
4. Electrical and Electronic Parts
5. Aerospace and Transportation