Plastic Granules
Bayblend® FR3010 RE PC/ABS Resin Flame Retardant
Bayblend® FR3010 RE is a flame-retardant PC+ABS blend offering UL 94 V-0 rating at just 1.5 mm thickness, high heat resistance (Vicat 110°C), and superior impact strength. This bio-circular attributed grade combines sustainability with robust performance for demanding technical applications.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt volume-flow rate: 15 cm³/10 min (240 °C/5 kg, ISO 1133)
- Melt viscosity: 245 Pa·s (1000 s⁻¹/260 °C, ISO 11443-A)
- Molding shrinkage (parallel): 0.5–0.7% (150x105x3 mm³, 240 °C/MT 80 °C, ISO 2577)
- Molding shrinkage (normal): 0.5–0.7% (150x105x3 mm³, 240 °C/MT 80 °C, ISO 2577)
Mechanical properties (23 °C/50 % r. h.)
- Tensile modulus: 2700 MPa (1 mm/min, ISO 527-1,-2)
- Yield stress: 60 MPa (50 mm/min, ISO 527-1,-2)
- Yield strain: 4.0% (50 mm/min, ISO 527-1,-2)
- Izod notched impact strength (23 °C): 35 kJ/m² (ISO 180/A)
- Izod notched impact strength (-30 °C): 10 kJ/m² (ISO 180/A)
Thermal properties
- Deflection temperature under load (1.80 MPa): 90 °C (ISO 75-1,-2)
- Deflection temperature under load (0.45 MPa): 100 °C (ISO 75-1,-2)
- Vicat softening temperature (50 N; 120 °C/h): 110 °C (ISO 306)
- Burning behavior (UL 94): V-0 (1.5 mm, UL 94)
- Glow wire flammability index (GWFI): 960 °C (2.0 mm)
Electrical properties (23 °C/50 % r. h.)
- Relative permittivity (100 Hz): 3.2 (IEC 60250)
- Relative permittivity (1 MHz): 3.1 (IEC 60250)
- Dissipation factor (100 Hz): 50 x 10⁻⁴ (IEC 60250)
- Dissipation factor (1 MHz): 70 x 10⁻⁴ (IEC 60250)
- Volume resistivity: 1E14 Ohm·m (IEC 62631-3-1)
- Surface resistivity: 1E16 Ohm (IEC 62631-3-2)
- Electrical strength: 35 kV/mm (1 mm, IEC 60243-1)
- Comparative tracking index (CTI): 350 (Solution A, IEC 60112)
Other properties (23 °C)
- Density: 1180 kg/m³ (ISO 1183-1)
- Water absorption (saturation): 0.5% (Water at 23 °C, ISO 62)
- Water absorption (equilibrium): 0.2% (23 °C/50% r. h., ISO 62)
Process Guide
- Melt temperature: 240–270 °C (ISO 294)
- Standard melt temperature: 260 °C (ISO 294)
- Mold temperature: 60–90 °C (ISO 294)
- Drying conditions: 80 °C for 4 hours, max moisture content ≤ 0.02%
Use & Applications
- Electronics: Laptop housings, server enclosures, connectors.
- Automotive: EV charging components, interior trims.
- Industrial: Power tool casings, control panels, safety equipment.
- Consumer: Thin-wall appliance parts requiring flame safety.
Features & Benefits
Best-in-Class Flame Retardancy
It achieves UL 94 V-0 compliance at ultra-thin 1.5 mm sections, enabling lighter, cost-efficient designs for electronics and enclosures without sacrificing safety.
Exceptional Heat Resilience
With a Vicat softening temperature of 110°C (ISO 306) and deflection under load up to 100°C (0.45 MPa), it withstands high-temperature environments in automotive and power components.
Reliable Impact Resistance
It boasts 35 kJ/m² notched Izod impact strength (23°C), preventing cracks and breaks in tools, connectors, and housings during rough handling or accidental drops.