Chimei Polylac® PA-746 ABS

chimei polylac pa 746 abs resin

Polylac® PA-746 High Flow Medium Impact ABS Resin

POLYLAC PA-746 has a melt flow index of 29 ml/10min and impact strength of 28 KJ/m2. Ideal for thin-wall parts, offering easy molding of complex shapes. It maintains strength at low temperatures and resists heat well. With 39 MPa tensile strength and 60 MPa flexural strength, PA-746 is perfect for gadget cases and appliance components.

Download PDF

UL Product iQ
Process Guide

Typical property data

Physical Properties
  • Melt Flow Index: 29 ml/10 min (ISO 1133, 220℃ × 10KG)
  • Mass Density: 1.03 g/cm³ (ISO 1183, 23℃)
Mechanical Properties
  • Tensile Strength:
    • Yield: 39 MPa (ISO 527, 50 mm/min)
    • Break: 29 MPa (ISO 527, 50 mm/min)
  • Tensile Elongation: 35% (ISO 527, 50 mm/min)
  • Flexural Strength: 60 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 1.8 GPa (ISO 178, 2 mm/min)
  • Izod Impact Strength (ISO 180/1A, Notched):
    • 23℃: 28 KJ/m²
    • -30℃: 12 KJ/m²
  • Charpy Impact Strength (ISO 179, Notched):
    • 23℃: 30 KJ/m²
    • -30℃: 14 KJ/m²
Thermal Properties
  • Vicat Softening Temperature:
    • 50℃/hr, 1KG: 103℃ (ISO 306)
    • 50℃/hr, 5KG: 94℃ (ISO 306)
  • Heat Distortion Temperature:
    • 1.8 MPa, unannealed: 82℃ (ISO 75/A)
    • 1.8 MPa, annealed: 96℃ (ISO 75/A)
  • Coefficient of Linear Thermal Expansion: 9.2 × 10⁻⁵ (ISO 11359)
Flammability
  • Flammability: HB at 1.5 mm (UL-94)
Mold Shrinkage
  • Shrinkage: 0.4% – 0.7% (ISO 294-4)

Use & Applications

  • Suitable for thin wall and high impact strength molding parts
chimei polylac® pa 746 application

Features & Benefits

High Flowability for Complex Designs

Polylac PA-746 ABS by Chimei offers high flowability (29 ml/10min), making it ideal for thin-walled parts. Its easy molding reduces cycle times and ensures smooth, detailed finishes in tight spaces.

Toughness in Any Environment

With high impact strength (28 kJ/m² at 23°C), this ABS resin withstands drops and stress. It performs reliably even at -30°C, perfect for automotive or outdoor gear needing durability.

Heat Resistance & Safety Compliance

PA-746 resists heat (Vicat 103°C) and meets UL94 HB flammability standards. Low mold shrinkage (0.4–0.7%) ensures stable dimensions, while easy processing (pre-dry at 80–85°C) saves time and costs.

chimei polylac® pa 746

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.