Physical Properties
  • Melt Flow Index: 15 ml/10 min (ISO 1133, 300°C × 1.2 kg)
  • Mass Density: 1.2 g/cm³ (ISO 1183, 23°C)
Mechanical Properties
  • Tensile Strength:
    • 64 MPa (Yield, ISO 527, 50 mm/min)
    • 70 MPa (Break, ISO 527, 50 mm/min)
  • Tensile Elongation: 120% (ISO 527, 50 mm/min)
  • Flexural Strength: 90 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.4 GPa (ISO 178, 2 mm/min)
  • Izod Impact Strength:
    • 70 KJ/m² (23°C, Notched, 1/8″, ISO 180/1A)
    • Not specified for -30°C
  • Charpy Impact Strength:
    • 70 KJ/m² (23°C, Notched, ISO 179)
    • Not specified for -30°C
Flammability
  • Rating: V-2 (UL-94, 2.5 mm)
Thermal Properties
  • Vicat Softening Temperature:
    • 150°C (50°C/hr, 1 kg, ISO 306)
    • 145°C (50°C/hr, 5 kg, ISO 306)
  • Heat Distortion Temperature (HDT):
    • 128°C (1.8 MPa, unannealed, ISO 75/A)
    • 143°C (1.8 MPa, annealed, ISO 75/A)
  • Coefficient of Linear Thermal Expansion: 6.0–8.0 × 10⁻⁵ (ISO 11359)
Mold Shrinkage
  • Range: 0.5–0.7% (ISO 294-4)
Process Guide
  • Pre-drying: 120°C × 4 hours (depending on humidity, storage conditions, and dryer performance)
  • Barrel Temperature Profile:
    • Nozzle: 250–300°C
    • Compression Zone: 250–310°C
    • Feeding Zone: 230–300°C
  • Mold Temperature: 70–120°C (varies based on thickness, cooling system, and gate/runner design).

Use & Applications

  • General injection molding for stationery
  • External pen tubing
  • Toys
  • Transparent molded products
chimei wonderlite pc 115 application

Features & Benefits

Superior Flow for Precision Molding

The PC-115 plastic material boasts low viscosity, making it a dream for injection molding. It flows effortlessly into complex molds, cutting production time and reducing defects—perfect for engineers aiming for flawless, intricate parts like pen casings or toy components.

Toughness That Lasts

Its high tensile strength (up to 70 MPa) and impact resistance (70 KJ/m²) mean your products withstand rough handling—think sturdy stationery or toys that survive a child’s playtime without cracking.

Crystal-Clear Transparency

Wonderlite PC-115 delivers stunning clarity for transparent applications. Whether it’s sleek external pen tubing or eye-catching molded displays, this resin ensures a premium finish that procurement managers love for boosting product appeal without extra effort.

wonderlite® pc 115

FAQs

1. Is PC-115 genuine Chimei material?

Yes. PC-115 is a genuine Chimei WONDERLITE® grade. UL Product iQ File No. E56070 lists CHI MEI CORPORATION. We provide original Chimei documents and batch COA.

2. Is PC-115 halogen-free?

Yes. RoHS report EKR24C00591M03 shows Chlorine, Bromine, Iodine and Fluorine all below reporting limits. Chimei environmental statement confirms no intentional halogen addition.

3. What are the UL94 ratings?

UL Product iQ File No. E56070 for PC-115(+): 0.4 mm V-2, 1.5 mm V-2, 2.5–2.8 mm V-2, 3.0 mm HB. ISO TDS lists 2.5 mm V-2. Color: ALL.

4. Can you provide COA per batch?

Yes. Each shipment includes batch-specific COA with MFR, density, tensile, impact, color, moisture.

5. Does PC-115 have UV stabilization or UL 746C f1?

Not stated in ISO TDS or UL Yellow Card. Please confirm with us if outdoor use is required.

6. What are typical applications of PC-115??

Low viscosity general PC for stationery, external pen tubing, toys, transparent molded products.

7. Is sample available?

Samples 1–5 kg available. Please provide application, color, wall thickness.

Related Flame-Retardant PC Grades

Disclaimer: The grades below are potential alternatives for comparison only. They are not direct drop-in replacements. UL ratings are color- and thickness-dependent. Typical values are not specifications. All property data is from Chimei ISO TDS unless otherwise stated. Please verify current UL Product iQ status, request TDS/SDS/COA and test samples before substitution.

Grade / ManufacturerUL94 (ISO TDS)MFR / MVRHDTNotched ImpactColorUV / UL 746C f1
PC-6600
Chi Mei
Baseline, 1.0mm V-0, opaque, non-halogen flame retardant
1.0mm V-0; 2.0mm 5VB; 3.0mm 5VA10 ml/10min125 / 140°C60 / 15 kJ/m²OpaqueNot stated
PC-6600 J01
Chi Mei
Same grade, standard black
1.0mm V-0; 2.0mm 5VB; 3.0mm 5VA10 ml/10min125 / 140°C60 / 15 kJ/m²BlackNot stated
PC-616LS
Chi Mei
1.0mm V-0, low smoke density
1.0mm V-0; 2.0mm 5VB; 3.0mm 5VA10 ml/10min125 / 140°C60 / 15 kJ/m²OpaqueUL 746C f1
PC-6610
Chi Mei
1.5mm V-0, opaque, UV stabilized
1.5mm V-0; 3.0mm 5VA10 ml/10min125 / 140°C60 / 15 kJ/m²OpaqueUV stabilized, UL 746C f1
PC-6710
Chi Mei
3.0mm V-0, transparent, UV stabilized
3.0mm V-010 ml/10min125 / 140°C60 / 15 kJ/m²TransparentUV stabilized, UL 746C f1
PC-681U
Chi Mei
1.5mm V-0, opaque, low-temp impact, UV stabilized
1.5mm V-0; 3.0mm 5VA10 ml/10min125 / 140°C60 / 45 kJ/m²OpaqueUV stabilized, UL 746C f1
PC-6600C
Zhenjiang Chi Mei
1.5mm V-0, opaque, weather & low-temp resistant
1.5mm V-09 cm³/10min125 / 134°C55 / 30 kJ/m²OpaqueUV stabilized, UL 746C f1
PC-6700
Chi Mei
2.5mm V-0, transparent, medium viscosity
2.5mm V-010 ml/10min125 / 140°C60 / 15 kJ/m²TransparentNot stated
PC-6710NF
Chi Mei
3.0mm V-0, transparent, PFAS-Free (Provisional)
3.0mm V-010 ml/10min125 / 140°C60 / Not available in ISO TDSTransparentNot stated
PC-6715NF
Chi Mei
1.5mm V-0, transparent, PFAS-Free (Provisional)
1.5mm V-05 ml/10min125°C (unannealed)60 / Not available in ISO TDSTransparentNot stated
PC-6715VT
Chi Mei
1.5mm V-0, transparent, UV stabilized, UL 746C f1
1.5mm V-06 ml/10min125 / 140°C60 / 15 kJ/m²TransparentUV stabilized, UL 746C f1