Chimei WONDERLITE® PC-6710NF

Chimei WONDERLITE PC-6710NF Flame Retardant Grade Transparent

WONDERLITE® PC-6710NF is a high-performance, PFAS-free flame-retardant polycarbonate resin offering UL 94 V-0 compliance at 3.0 mm thickness. With exceptional transparency, UV stability, and robust mechanical strength, it’s engineered for industries prioritizing safety, durability, and regulatory compliance.

chimei wonderlite pc 6710nf pc resin

Download PDF

UL Product iQ
Processing Data

Typical property data

Physical Properties
  • Mass Density: 1.2 g/cm³ (ISO 1183)
Mechanical Properties
  • Tensile Strength (Yield): 65 MPa (ISO 527, 50 mm/min)
  • Tensile Strength (Break): 70 MPa (ISO 527, 50 mm/min)
  • Tensile Elongation: 110% (ISO 527, 50 mm/min)
  • Flexural Strength: 95 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.3 GPa (ISO 178, 2 mm/min)
  • Izod Impact Strength (Notched, 23°C): 60 KJ/m² (ISO 180/1A)
  • Charpy Impact Strength (Notched, 23°C): 65 KJ/m² (ISO 179)
Thermal Properties
  • Vicat Softening Temperature (1KG): 148°C (ISO 306, 50°C/hr)
  • Vicat Softening Temperature (5KG): 142°C (ISO 306, 50°C/hr)
  • Heat Distortion Temperature (Unannealed, 1.8 MPa): 125°C (ISO 75/A)
  • Heat Distortion Temperature (Annealed, 1.8 MPa): 140°C (ISO 75/A)
  • Coefficient of Linear Thermal Expansion: 6.8×10−56.8 \times 10^{-5} (ISO 11359)
Mold Shrinkage
  • Shrinkage Range: 0.4–0.6% (ISO 294-4)
Flammability
  • UL-94 Rating: V-0 at 3.0mm thickness
Process Guide
  • Pre-drying Conditions: 120°C for 4 hours (varies with humidity, storage conditions, and dryer performance)
  • Barrel Temperature Settings:
    • Nozzle: 250–310°C
    • Compression Zone: 250–320°C
    • Feeding Zone: 230–300°C
  • Mold Temperature: 70–120°C (varies with thickness, cooling system, gate, and runner design)
  • Purging Recommendation: Use heat-stable resins like polyethylene or polypropylene.

Use & Applications

  • Electrical appliances
  • outdoor applications (UL 746C f1)
chimei wonderlite pc 6710nf application

Features & Benefits

Superior Flame Resistance, PFAS-Free

WONDERLITE® PC-6710NF meets UL 94 V-0 standards (3.0 mm) without harmful PFAS chemicals. Ideal for electrical enclosures or automotive interiors where safety and eco-compliance matter.

High Impact & Thermal Stability

It boasts 65 KJ/m² Charpy impact resistance (23°C) and a Vicat softening temperature of 148°C. Perfect for outdoor equipment or medical devices exposed to harsh conditions.

UL-Certified Outdoor Durability

UV-stabilized and UL 746C f1-rated for outdoor use. Protects components like LED housings or solar connectors from weathering and electrical stress.

wonderlite® pc 6710nf

FAQs

1. Is PC-6710NF genuine Chimei material?

Yes. PC-6710NF is genuine Chimei WONDERLITE®. UL File No. E56070 lists CHI MEI CORPORATION.

2. Is PC-6710NF halogen-free?

Yes. RoHS report EKR24C00689 shows Cl, Br, I, F below reporting limits. Chimei environmental statement confirms no intentional halogen addition. Also PFAS-Free.

3. What colors are UL94 V-0 certified?

UL Product iQ File No. E56070 for PC-6710NF: 3.0–3.3 mm V-0, Color: NC. ISO TDS: 3.0 mm V-0.

4. Can you provide COA per batch?

Yes. Each shipment includes batch-specific COA with MFR, density, tensile, impact, color, moisture.

5. What makes PC-6710NF special?

PFAS-Free, transparent, 3.0 mm V-0 flame retardant. Suitable for electrical appliances and outdoor applications.

6. Is sample available?

Samples 1–5 kg available. Please provide application, color, wall thickness.

PC-6710NF Related Flame Retardant Grades

Disclaimer:Disclaimer: The grades below are potential alternatives for comparison only from Chimei. They are not direct drop-in replacements. UL ratings are color- and thickness-dependent. Typical values are not specifications. All property data is from Chimei ISO TDS unless otherwise stated. Please verify current UL Product iQ status, request TDS/SDS/COA and test samples before substitution.

Grade / Manufacturer Positioning vs. PC-6710NF UL94 (ISO TDS) MFR HDT Notched Izod 23/–30°C Color UV / UL 746C f1
PC-6715NF
Chi Mei
Thin-wall counterpart: 1.5mm V-0 PFAS-Free transparent — same compliance tier 1.5mm V-0 5 ml/10min 125°C (unannealed) 60 / Not available Transparent Not stated
PC-6710
Chi Mei
Same 3.0mm V-0 transparent, non-PFAS-Free legacy FR with UV+f1 — cost reference 3.0mm V-0 10 ml/10min 125 / 140°C 60 / 15 kJ/m² Transparent UV stabilized, UL 746C f1
PC-6700
Chi Mei
Thinner-wall transparent FR: 2.5mm V-0, medium viscosity 2.5mm V-0 10 ml/10min 125 / 140°C 60 / 15 kJ/m² Transparent Not stated

↩ Back to Chimei Flame Retardant PC Resin Hub (11 grades)

Substitution checklist: Before replacing any grade, verify UL94 at the same wall thickness, UL-listed color, halogen-free declaration, MFR/MVR, HDT, notched impact, UV / UL 746C f1 and processing window.