Chimei WONDERLITE® PC-6715NF

WONDERLITE PC-6715NF Flame Retardant Grade Transparent

WONDERLITE® PC-6715NF is a transparent, PFAS-free polycarbonate resin offering UL 94 V-0 flame retardancy at 1.5mm thickness. Engineered for safety and durability, it combines UV stabilization, high impact resistance, and compliance with global electrical/thermal standards—ideal for railways, appliances, and outdoor applications.

chimei wonderlite pc 6715nf pc resin

Download PDF

UL Product iQ
Process Guide

Typical property data

Physical Properties
  • Mass Density: 1.2 g/cm³ (ISO 1183, 23°C)
  • Melt Flow Index: 5 ml/10 min (ISO 1133, 300°C × 1.2 kg)
Mechanical Properties
  • Tensile Strength:
    • At Yield: 60 MPa (ISO 527, 50 mm/min)
    • At Break: 55 MPa (ISO 527, 50 mm/min)
  • Tensile Elongation: 70% (ISO 527, 50 mm/min)
  • Flexural Strength: 99 MPa (ISO 178, 2 mm/min)
  • Flexural Modulus: 2.2 GPa (ISO 178, 2 mm/min)
  • Izod Impact Strength:
    • 23°C (Notched): 60 kJ/m² (ISO 180/1A)
Flammability
  • UL-94 Rating: 1.5 mm V-0
Thermal Properties
  • Vicat Softening Temperature:
    • 1 kg: 150°C (ISO 306, 50°C/hr)
    • 5 kg: 143°C (ISO 306, 50°C/hr)
  • Heat Distortion Temperature: 125°C (ISO 75/A, 1.8 MPa, unannealed)
  • Coefficient of Linear Thermal Expansion: 6.8×10−56.8 \times 10^{-5} (ISO 11359)
Mold Shrinkage
  • Range: 0.4–0.6% (ISO 294-4)
Process Guide
  • Pre-drying: 120°C × 4 hrs (depends on humidity, storage conditions, and dryer performance)
  • Barrel Temperature Settings:
    • Nozzle: 280–310°C
    • Compression Zone: 280–320°C
    • Feeding Zone: 260–300°C
  • Mold Temperature: 70–120°C (varies with part thickness, cooling system, and gating design)

Use & Applications

  • Railway: Seat components, cabin panels, and lighting covers requiring flame retardancy and impact resistance.
  • Electrical Appliances: Connectors, circuit breaker housings, and enclosures needing UL-certified safety.
  • Outdoor Applications: UV-resistant traffic signs, LED streetlight covers, and solar panel frames.
chimei wonderlite pc 6715nf application

Features & Benefits

PFAS-Free Flame Retardancy

WONDERLITE® PC-6715NF meets UL 94 V-0 flammability standards without hazardous PFAS chemicals. This ensures compliance with strict safety regulations, making it perfect for electrical enclosures and public infrastructure where fire safety is critical.

UV Resistance for Outdoor Durability

UV-stabilized to resist yellowing and degradation, this material maintains clarity and strength in harsh sunlight. Use it for outdoor lighting covers, traffic signs, or railway components exposed to weather.

High Impact Strength

With 60 KJ/m² Izod impact resistance at 23°C, PC-6715NF withstands sudden shocks and vibrations. Ideal for automotive interiors, appliance housings, or protective covers in demanding environments.

wonderlite® pc 6715nf

FAQs

1. Is PC-6715NF genuine Chimei material?

Yes. PC-6715NF is genuine Chimei WONDERLITE®. UL File No. E56070 lists CHI MEI CORPORATION.

2. Is PC-6715NF halogen-free?

Yes. RoHS report EKR24C00688 shows Cl, Br, I, F below reporting limits. Chimei environmental statement confirms no intentional halogen addition. Also PFAS-Free.

3. What colors are UL94 V-0 certified?

UL Product iQ File No. E56070 for PC-6715NF(a): 1.5 mm V-0, 2.0 mm V-0, 3.0 mm V-0, Color: NC, BK. ISO TDS: 1.5 mm V-0.

4. Can you provide COA per batch?

Yes. Each shipment includes batch-specific COA with MFR, density, tensile, impact, color, moisture.

5. What makes PC-6715NF special?

PFAS-Free, transparent, 1.5 mm V-0 flame retardant. Suitable for railway, electrical appliances, outdoor applications.

6. Is sample available?

Samples 1–5 kg available. Please provide application, color, wall thickness.

PC-6715NF Related Flame Retardant Grades

Disclaimer:Disclaimer: The grades below are potential alternatives for comparison only from Chimei. They are not direct drop-in replacements. UL ratings are color- and thickness-dependent. Typical values are not specifications. All property data is from Chimei ISO TDS unless otherwise stated. Please verify current UL Product iQ status, request TDS/SDS/COA and test samples before substitution.

Grade / Manufacturer Positioning vs. PC-6715NF UL94 (ISO TDS) MFR HDT Notched Izod 23/–30°C Color UV / UL 746C f1
PC-6710NF
Chi Mei
Thicker-wall counterpart: 3.0mm V-0 PFAS-Free transparent — same compliance tier 3.0mm V-0 10 ml/10min 125 / 140°C 60 / Not available Transparent Not stated
PC-6715VT
Chi Mei
Same 1.5mm V-0 transparent, non-PFAS-Free legacy FR with UV+f1 — cost reference 1.5mm V-0 6 ml/10min 125 / 140°C 60 / 15 kJ/m² Transparent UV stabilized, UL 746C f1
PC-6710
Chi Mei
Thicker-wall transparent FR: 3.0mm V-0 with UV+f1 for outdoor covers 3.0mm V-0 10 ml/10min 125 / 140°C 60 / 15 kJ/m² Transparent UV stabilized, UL 746C f1

↩ Back to Chimei Flame Retardant PC Resin Hub (11 grades)

Substitution checklist: Before replacing any grade, verify UL94 at the same wall thickness, UL-listed color, halogen-free declaration, MFR/MVR, HDT, notched impact, UV / UL 746C f1 and processing window.

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.