CMTRL CH612 is a medium-flow, high-impact polystyrene designed for injection molding from Guangxi Changke. It offers 6 g/10 min MFR, 12 kJ/m² notched Charpy impact strength, 90°C Vicat softening temperature, and 0.4–0.7% molding shrinkage for packaging, office supplies, kitchenware, toys, appliance parts, and consumer electronics housings.

Download PDF

TDS - Data Sheet
MSDS - Safety Data Sheet

Typical property data

Physical Properties
  • Density: 1.04 g/cm³, 23°C (Internal method)
  • Molding Shrinkage: 0.4–0.7% (Internal method)
  • Melt Flow Rate: 6 g/10 min, 200°C, 5 kg (GB/T 3682.1-2018)
Mechanical Properties
  • Tensile Yield Strength: 25 MPa, 50 mm/min, 4.0 mm (GB/T 1040.2-2022)
  • Flexural Strength: 40 MPa, 2.0 mm/min, 4.0 mm (GB/T 9341-2008)
  • Flexural Modulus: 1800 MPa, 2.0 mm/min, 4.0 mm (GB/T 9341-2008)
Impact Properties
  • Notched Charpy Impact Strength: 12 kJ/m², Type A notch, molded, 1.0 J (GB/T 1043.1-2008)
Thermal Properties
  • Vicat Softening Temperature: 90°C, B50, 4.0 mm (GB/T 1633-2000)
Optical Properties
  • Gloss: 70, 60°, 1.0 mm (GB/T 2410-2008)
Flame Characteristics
  • Flammability Rating: HB, 1.5 mm (UL 94)
Processing Parameters
  • Melt Flow Rate: 6 g/10 min, 200°C, 5 kg (GB/T 3682.1-2018)
  • Molding Shrinkage: 0.4–0.7% (Internal method)

Use & Applications

  • General Injection Molding Parts: for office supplies, kitchenware, and toys
  • Food Packaging Products: such as beverage cups and disposable dairy packaging
  • Household Appliance Components: for internal parts and housings for household appliances
  • Consumer Electronics Housings: for consumer electronics housings
guangxi changke hips plastic resin package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.