CNPC 0215A ABS Resin

jieyang abs resin package

CNPC 0215A ABS Resin Medium Impact General Grade

CNPC 0215A ABS Plastic Resin is a high-performance material offering superior gloss, rigidity, and toughness. Designed for durability and versatility, it excels in manufacturing small appliances, electronics, consumer goods, and toys.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Flow Rate (MFR): 22 g/10min at 220°C, 10kg (GB/T 3682.1-2018)
  • Appearance: Light ivory-colored solid granules (3mm × 3mm)
Mechanical Properties
  • Notched Impact Strength: 22 kJ/m² (GB/T 9341-2008)
  • Tensile Strength: 45 MPa (GB/T 1040.2-2006)
  • Flexural Strength: 74 MPa (GB/T 9341-2008)
  • Flexural Modulus: 2300 MPa (GB/T 9341-2008)
  • Rockwell Hardness (R Scale): 106 (GB/T 3398.2-2008)
Thermal Properties
  • Vicat Softening Temperature: 96°C (GB/T 1633-2000)
Optical Properties
  • Yellowing Index: 20 (HG/T 3862-2006)
  • Whiteness: 64% (GB/T 2913-1982)
Flame Characteristics
  • Flammability Rating: HB (UL Certification)
Processing Parameters
  • Recommended Melt Temperature Range: 210°C to 280°C
  • Injection Pressure: 500–1000 bar
  • Injection Speed: Medium to high
  • Drying Conditions: 80°C–90°C for 2 hours (prior to processing)

Use & Applications

  • Home Appliances
  • Automotive: Interior and exterior trim parts
  • Consumer Goods
jieyang abs resin package

You Might Also Like

CNPC HF-681 ABS

CNPC 0215H ABS

CNPC 0215E ABS

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.