CNPC 0215E ABS Resin High Gloss General Grade
CNPC 0215E is a specialized, high-gloss Acrylonitrile Butadiene Styrene (ABS) resin produced by the China National Petroleum Corporation (CNPC). The plastic granules feature high gloss, balanced stiffness, and wear resistance. Highly tailored for toy and small home appliance manufacturing.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Melt Mass-Flow Rate (MFR): 21 g/10 min (Tested at 220°C, 10 kg, GB/T 3682.1-2018)
- Appearance: Light ivory-colored granular solid (3 mm × 3 mm)
Mechanical Properties
- Notched Charpy Impact Strength: 21 kJ/m² (GB/T 9341-2008)
- Tensile Strength: 47 MPa (GB/T 1040.2-2006)
- Flexural Strength: 72 MPa (GB/T 9341-2008)
- Flexural Modulus: 2300 MPa (GB/T 9341-2008)
- Rockwell Hardness: 106 (R Scale, GB/T 3398.2-2008)
Thermal Properties
- Vicat Softening Temperature: 97°C (GB/T 1633-2000)
Optical Properties
- Yellowing Index (YI): 20 (HG/T 3862-2006)
- Whiteness: 65 (GB/T 2913-1982)
Flame Characteristics
- Flammability Rating: HB (Tested as per UL Certification)
Processing Parameters
- Recommended Melting Temperature Range: 210°C–280°C
- Injection Pressure: 500–1000 bar
- Injection Speed: Medium-High
- Pre-drying Conditions: Dry at 80°C–90°C for 2 hours to ensure optimal performance.
Use & Applications
- toy
- small home appliance manufacturing