CNPC 0215H ABS Resin

jieyang abs resin package

CNPC 0215H ABS Resin High Flow General Grade

CNPC 0215H is a general-purpose, high-flow ABS resin produced by PetroChina Jilin Petrochemical. It is primarily known for balancing good rigidity, medium-to-high impact resistance, and excellent moldability. Used for home appliance, toys.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Mass Flow Rate (220°C, 10kg): 22 g/10min (GB/T 3682.1-2018)
  • Appearance: Light ivory-colored, granular solid (3mm×3mm).
Mechanical Properties
  • Notched Izod Impact Strength: 24 kJ/m² (GB/T 9341-2008)
  • Tensile Strength: 45 MPa (GB/T 1040.2-2006)
  • Flexural Strength: 73 MPa (GB/T 9341-2008)
  • Flexural Modulus: 2200 MPa (GB/T 9341-2008)
  • Rockwell Hardness (R Scale): 105 (GB/T 3398.2-2008)
Thermal Properties
  • Vicat Softening Temperature: 97°C (GB/T 1633-2000)
Optical Properties
  • Yellow Index: 19 (HG/T 3862-2006)
  • Whiteness: 65 (GB/T 2913-1982)
Flame Characteristics
  • Flammability Rating: HB (UL Certificate)
Processing Parameters
  • Melting Temperature Range: 210–280°C
  • Injection Pressure: 500–1000 bar
  • Injection Speed: Medium to High
  • Drying Conditions Before Processing: 80–90°C for 2 hours

Use & Applications

  • home appliance
  • toys
  • consumer goods
jieyang abs resin package

You Might Also Like

CNPC HF-681 ABS

CNPC 0215A ABS

CNPC 0215E ABS

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.