CNPC DFDA-7042N LLDPE Resin

cnpc fushun lldpe 25kg package

CNPC DFDA-7042N Linear Low Density Polyethylene

CNPC DFDA-7042N is a film-grade LLDPE resin with 1.7–2.3 g/10 min MFR and 0.918–0.923 g/cm³ density. It offers high strength, good film forming, high gloss, ≥400% break strain, and ≥55 g dart impact for packaging, stretch wrap, agricultural, and liner films.

Download PDF

TDS - Data Sheet

Typical property data

Physical Properties
  • Colored Pellets: ≤10 count/kg (SH/T 1541-2006)
  • Snakeskin and Tailed Pellets: ≤15 count/kg (SH/T 1541-2006)
  • Large and Small Pellets: ≤5 g/kg (SH/T 1541-2006)
  • Melt Mass-Flow Rate: 1.7–2.3 g/10 min (GB/T 3682-2000)
  • Density at 23°C: 0.918–0.923 g/cm³ (GB/T 1033.2-2010)
  • Fish Eyes, 0.8 mm: ≤6 count/1520 cm² (GB/T 11115-2009)
  • Fish Eyes, 0.4 mm: ≤15 count/1520 cm² (GB/T 11115-2009)
Mechanical Properties
  • Tensile Yield Stress: ≥8.5 MPa (GB/T 1040.2-2006)
  • Nominal Tensile Strain at Break: ≥400% (GB/T 1040.2-2006)
Impact Properties
  • Dart Impact Failure Mass: ≥55 g at 0.030 mm film thickness (GB/T 9639.1-2008)
Optical Properties
  • Haze: Measured % (GB/T 2410-2008)
  • Visual Performance: CNPC DFDA-7042N is specified with high gloss and good film-forming properties.
Processing Parameters
  • Recommended Processing Form: Film extrusion
  • Film Thickness Reference for Dart Impact Test: 0.030 mm
  • Melt Flow Range for Processing Control: 1.7–2.3 g/10 min (GB/T 3682-2000)
  • Material Form: Natural-colored pellets
  • Additive Note: CNPC DFDA-7042N has no antiblocking or slip properties. Buyers should confirm additive packages based on film line requirements.

Use & Applications

• Packaging films for everyday goods
• Agricultural films
• Liner films
• Stretch wrap films
• Blending materials

cnpc fushun lldpe 25kg package