CNPC EPB05M Medical PP

cnpc kunlun pp 25kg package

CNPC EPB05M Medical PP Multi-layer Co-extrusion Medical Infusion Bag

CNPC EPB05M is a medical grade PP for the outer layer of multi-layer infusion bags. It offers high stiffness with 1603 MPa flexural modulus and 156.4°C Vicat softening point. It supports co-extrusion blown film processing and can reduce import material costs by over 20%.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Flow Rate: 2.5 g/10 min (GB/T 3682-2000)
  • Layer Use: Outer layer for multi-layer co-extrusion infusion bag
Mechanical Properties
  • Flexural Modulus: 1603 MPa (GB/T 9341-2008)
  • Tensile Strength: 35.7 MPa (GB/T 1040.2-2006)
  • Layer Bonding Strength: >4 N/15 mm
  • Layer Bonding Performance: No delamination risk
Impact Properties
  • Charpy Notched Impact Strength: 5.6 kJ/m² (GB/T 1043.1-2008)
Thermal Properties
  • Vicat Softening Point: 156.4°C (GB/T 2410.2-2008)
  • Heat Resistance: High heat resistance for medical infusion bag applications
Processing Parameters
  • Recommended Processing Method: Multi-layer co-extrusion blown film process
  • Compatible Equipment: W&H and Japanese Fuji equipment
  • Production Compatibility: Fully automatic bag-making line
  • Typical Application Structure: Inner layer / middle layer / outer layer
  • CNPC H03M Position: Outer layer
  • Cost Optimization: Can replace imported materials and reduce cost by over 20%

Use & Applications

  • Multi-layer co-extrusion medical infusion bag
cnpc kunlun pp 25kg package