CNPC FHP5050 is an HDPE resin for edible oil and cooking oil bottle caps. It has a density of 0.9543 g/cm³, MFR of 3.23 g/10 min, 23.0 MPa yield strength, and 685% tensile strain at break for stable cap molding and reliable use.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Pellet Appearance: 2 pcs/kg black specks and colored pellets (SH/T 1541.1-2019)
  • Density at 23°C: 0.9543 g/cm³ (GB/T 1033.2-2010)
  • Melt Flow Rate: 3.23 g/10 min (GB/T 3682.1-2018)
Mechanical Properties
  • Tensile Strength at Yield: 23.0 MPa (GB/T 1040.2-2006)
  • Nominal Tensile Strain at Break: 685% (GB/T 1040.2-2006)
Impact Properties
  • Charpy Notched Impact Strength at 23°C: 9.8 kJ/m² (GB/T 1043.1-2008)
Processing Parameters
  • Processing Suitability: CNPC FHP5050 is designed for HDPE bottle cap applications, including edible oil caps and cooking oil bottle caps.
  • Melt Flow Rate for Processing Reference: 3.23 g/10 min (GB/T 3682.1-2018)

Use & Applications

  • edible oil caps / cooking oil (bottle) caps