CNPC FHP5060 HDPE Resin

cnpc hdpe resin 25kg package

CNPC FHP5060 High Density Polyethylene Resin for Beverage bottle caps

CNPC FHP5060 is an HDPE resin from PetroChina Fushun. It has 0.9565 g/cm³ density, 1.86 g/10 min melt flow rate, and 22.7 MPa yield strength. It offers clean pellets and balanced stiffness for carbonated soft drink caps and beverage bottle caps.

Associated Documents

TDS - Data Sheet
EU Food Contact Material
Bisphenol A

Typical property data

Physical Properties
  • Pellet Appearance: 0 pcs/kg black specks and colored pellets (SH/T 1541.1-2019)
  • Density at 23°C: 0.9565 g/cm³ (GB/T 1033.2-2010)
  • Melt Flow Rate: 1.86 g/10 min (GB/T 3682.1-2018)
Mechanical Properties
  • Tensile Strength at Yield: 22.7 MPa (GB/T 1040.2-2022)
  • Flexural Modulus: 912 MPa (GB/T 9341-2008)
Impact Properties
  • Charpy Notched Impact Strength at 23°C: 8.6 kJ/m² (GB/T 1043.1-2008)
Processing Parameters
  • Melt Flow Rate: 1.86 g/10 min (GB/T 3682.1-2018)
  • Recommended Processing Use: Cap molding applications for carbonated soft drink caps and beverage bottle caps

Use & Applications

  • Cola bottle cap / Beverage bottle cap
cnpc hdpe resin 25kg package

Related Products

CNPC FHP5050 HDPE

CNPC FHP5060 HDPE