CNPC H02M is a medical grade PP from PetroChina Lanzhou Petrochemical. It is designed for solid pharmaceutical bottles. It offers low MFR at 1.48 g/10 min, flexural modulus of 1655 MPa, and no cracking after a 1.5 m drop. It passed YBB, USP <661>, and EP 3.1.6 checks.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Mass Flow Rate: 1.48 g/10 min (GB/T 3682.1, 230°C/2.16 kg)
  • Yellow Index: -1.40 (GB/T 39822)
Mechanical Properties
  • Tensile Yield Stress: 34.0 MPa (GB/T 1040.2)
  • Flexural Modulus: 1655 MPa (GB/T 9341)
Impact Properties
  • Charpy Notched Impact Strength at 23°C: 4.9 kJ/m² (GB/T 1043.1)
Optical Properties
  • Yellow Index: -1.40 (GB/T 39822)
Processing Parameters
  • Recommended Process: Injection molding
  • Automation Compatibility: Fully automatic injection molding process
  • Melt Mass Flow Rate for Processing Reference: 1.48 g/10 min (GB/T 3682.1, 230°C/2.16 kg)
  • Suitable Product Forming: Solid pharmaceutical PP bottles
Medical Packaging Performance Data
  • Non-Volatile Matter, 50 mL: 25.4 mg (5.10)
  • Appearance, Black Spots and Colored Particles: 2 particles/kg (SH/T 1541.1)
  • Drop Resistance: No cracking after 1.5 m drop
  • Soluble Matter Flow Rate Reduction: 1.48–1.8 g/10 min
  • Volatile Matter Reduction: 25.4 mg

Use & Applications

  • Solid pharmaceutical PP bottles
  • tablets
  • capsules
  • pill packaging
cnpc kunlun pp 25kg package

Send Us a Message

Please enter your query and share a few details, and we will get back to you shortly.