Plastic Granules
CNPC H03M Medical PP Multi-layer Co-extrusion Medical Infusion Bag
CNPC H03M is a medical grade PP for the outer layer of multi-layer infusion bags. It offers high stiffness with 1603 MPa flexural modulus and 156.4°C Vicat softening point. It supports co-extrusion blown film processing and can reduce import material costs by over 20%.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Melt Flow Rate: 2.5 g/10 min (GB/T 3682-2000)
- Layer Use: Outer layer for multi-layer co-extrusion infusion bag
Mechanical Properties
- Flexural Modulus: 1603 MPa (GB/T 9341-2008)
- Tensile Strength: 35.7 MPa (GB/T 1040.2-2006)
- Layer Bonding Strength: >4 N/15 mm
- Layer Bonding Performance: No delamination risk
Impact Properties
- Charpy Notched Impact Strength: 5.6 kJ/m² (GB/T 1043.1-2008)
Thermal Properties
- Vicat Softening Point: 156.4°C (GB/T 2410.2-2008)
- Heat Resistance: High heat resistance for medical infusion bag applications
Processing Parameters
- Recommended Processing Method: Multi-layer co-extrusion blown film process
- Compatible Equipment: W&H and Japanese Fuji equipment
- Production Compatibility: Fully automatic bag-making line
- Typical Application Structure: Inner layer / middle layer / outer layer
- CNPC H03M Position: Outer layer
- Cost Optimization: Can replace imported materials and reduce cost by over 20%
Use & Applications
- Multi-layer co-extrusion medical infusion bag