Plastic Granules
CNPC LD26D Medical Grade PE Raw Material Polyethylene
CNPC LD26D is a medical grade PE from PetroChina Lanzhou Petrochemical. It is used for PE ampoule bottles, eye drop bottles, and cosmetic soft tubes. It offers low extractables below 15 μg/cm², 2 m drop resistance, and USP Class VI and EP 3.1.5 compliance.
Associated Documents
TDS - Data Sheet
Typical property data
Physical Properties
- Density: 0.926 g/cm³ (GB/T 1033.2-2010)
- Melt Mass-Flow Rate: 0.28 g/10 min (GB/T 3682-2000)
Mechanical Properties
- Tensile Strength: 12.4 MPa (GB/T 1040.2-2006)
- Flexural Modulus: 230 MPa (GB/T 9341-2008)
- Haze: 8% (GB/T 2410-2008)
Thermal Properties
- Vicat Softening Temperature: 105°C (GB/T 1633-2000)
Optical Properties
- Haze: 8% (GB/T 2410-2008)
Processing Parameters
- Recommended Processing Method: Blow-Fill-Seal molding process
- Recommended Processing Method: Injection molding process
- Packaging Compatibility: Suitable for multiple pharmaceutical liquid packaging formats
- Drop Resistance: No breakage at 2 m drop height
- Low Extractables: Extractables below 15 μg/cm²
Use & Applications
- PE ampoule bottles
- eye drop bottles
- cosmetic soft tubes
- Pharmaceutical Liquid Packaging