CNPC RP340R Medical PP

polypropylene pp resin

CNPC RP340R Medical Grade PP for Disposable Syringe Barrels

CNPC RP340R is a medical-grade PP for disposable syringe barrels. It offers 21 g/10 min melt flow, 85.9% transmittance, and 8.8% haze. It supports thin-wall injection molding down to 0.8 mm and meets YY/T 0242-2007.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Mass Flow Rate: 21.0 g/10 min (GB/T 3682-2000)
  • Haze: 8.8% (GB/T 2410.2-2008)
Mechanical Properties
  • Tensile Strength: 26.9 MPa (GB/T 1040.2-2006)
  • Flexural Modulus: 895 MPa (GB/T 9341-2008)
Impact Properties
  • Charpy Notched Impact Strength: 6.2 kJ/m² (GB/T 1040.1-2008)
Optical Properties
  • Transmittance: 85.9% (GB/T 2410.2-2008)
  • Haze: 8.8% (GB/T 2410.2-2008)
  • Color Difference: ΔE < 0.5
Processing Parameters
  • Processing Method: Precision injection molding
  • Assembly Compatibility: Fully automatic assembly production line
  • Recommended Product Wall Thickness: Minimum wall thickness up to 0.8 mm
  • Flowability: High flowability, melt flow rate 21.0 g/10 min (GB/T 3682-2000)

Use & Applications

  • Disposable sterile syringe barrels
  • 5 mL syringe barrels
  • 10 mL syringe barrels
  • 20 mL syringe barrels
  • Thin-wall medical injection molded parts
  • Automated syringe assembly components