CNPC RPE02M Medical PP

cnpc kunlun pp 25kg package

CNPC RPE02M Medical Grade Polypropylene (PP)

CNPC RPE02M is a medical grade PP for BFS ampoules, eye drops, inhalation solutions, and injection packaging. It offers 2.2 g/10 min MFR, 26.3 MPa tensile strength, 82% light transmittance, and 121°C steam sterilization resistance. Complies with ISO 10993.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Mass Flow Rate: 2.2 g/10 min (GB/T 3682-2000)
  • Density: 954 kg/m³ (GB/T 9341-2008)
  • Light Transmittance: 82% (GB/T 2410-2008)
Mechanical Properties
  • Tensile Strength: 26.3 MPa (GB/T 1040.2-2006)
  • Flexural Modulus: 954 MPa (GB/T 9341-2008)
Impact Properties
  • Charpy Notched Impact Strength: 6.7 kJ/m² (GB/T 1040.1-2008)
Thermal Properties
  • Heat Deflection Temperature: 66°C (GB/T 1634.2-2004)
  • Steam Sterilization Resistance: 121°C high-temperature steam sterilization supported
  • Crystallization Temperature: 141°C
  • Low Extractables: n-hexane extractables below 520 µg/cm²
Optical Properties
  • Light Transmittance: 82% (GB/T 2410-2008)
  • Appearance Stability: No color migration detected in migration test
  • Clarity Performance: Suitable for medical packaging requiring transparent or translucent PP performance
Processing Parameters
  • Recommended Process: BFS blow-fill-seal integrated process
  • Compatible Process: Co-extrusion blown film process
  • Medical Packaging Use: BFS production line for ampoules and infusion packaging
  • Sterilization Process: Suitable for high-temperature steam sterilization at 121°C
  • Molding Stability: CNPC RPE02M shows stable molding performance on BFS equipment

Use & Applications

  • BFS ampoules
  • eye drops
  • inhalation solutions
  • small-volume injections
  • multilayer co-extruded infusion bag inner layer