CNPC RPE16I Medical PP

polypropylene pp resin

CNPC RPE16I Medical PP Plastic Raw Material

CNPC RPE16I is a medical grade PP for infusion and oral liquid bottle caps. It offers 16.0 g/10 min melt flow, <8 s injection cycle, and 27.6 MPa tensile strength. It supports high-speed molding, stable sealing, and automated packaging.

Associated Documents

TDS - Data Sheet

Typical property data

Physical Properties
  • Melt Mass Flow Rate: 16.0 g/10 min (GB/T 3682-2000)
  • Tensile Modulus: 976 MPa (GB/T 9341-2008)
  • Haze: 9.8% (GB/T 2410.2-2008)
  • Light Transmittance: 85.6% (GB/T 2410.2-2008)
Mechanical Properties
  • Tensile Strength: 27.6 MPa (GB/T 1040.2-2006)
  • Flexural Modulus: 976 MPa (GB/T 9341-2008)
Impact Properties
  • Notched Charpy Impact Strength: 6.8 kJ/m² (GB/T 1040.1-2008)
Thermal Properties
  • Low-Temperature Performance: Stable from -20°C to 60°C
  • Welding Sealing Performance: Leakage rate < 0.01%
Optical Properties
  • Light Transmittance: 85.6% (GB/T 2410.2-2008)
  • Haze: 9.8% (GB/T 2410.2-2008)
Processing Parameters
  • Recommended Processing Method: High-speed injection molding
  • Compatible Equipment: Dedicated bottle-cap injection molding equipment
  • Packaging Compatibility: Fully automatic inspection and packaging line
  • Injection Cycle: < 8 s
  • Opening Torque: 0.6–0.8 N·m
  • Melt Mass Flow Rate: 16.0 g/10 min (GB/T 3682-2000)

Use & Applications

  • Infusion bottle outer cap
  • Oral liquid bottle cap