Plastic Granules
Apec 1695 Thermoplastic Resin Heat Resistant UV-stabilized
Covestro Apec 1695 is a heat-resistant copolycarbonate resin. With an MVR of 45 cm³/10 min (330°C/2.16 kg) and easy-release properties, it excels in automotive lighting applications, offering superior flow and a softening temperature of 158°C. Ideal for demanding, precision-driven components.
Typical property data
Rheological Properties
- Melt volume-flow rate (330 °C / 2.16 kg): 45 cm³/10 min (ISO 1133)
- Melt mass-flow rate (330 °C / 2.16 kg): 46 g/10 min (ISO 1133)
- Molding shrinkage, parallel: 0.75% (ISO 294-4)
- Molding shrinkage, normal: 0.75% (ISO 294-4)
Mechanical Properties (23 °C / 50% r.h.)
- Tensile modulus (1 mm/min): 2350 MPa (ISO 527-1,-2)
- Yield stress (50 mm/min): 68 MPa (ISO 527-1,-2)
- Yield strain (50 mm/min): 6.2% (ISO 527-1,-2)
- Nominal strain at break (50 mm/min): > 50% (ISO 527-1,-2)
- Flexural modulus (2 mm/min): 2400 MPa (ISO 178)
- Flexural strength (2 mm/min): 100 MPa (ISO 178)
- Ball indentation hardness: 120 N/mm² (ISO 2039-1)
Thermal Properties
- Temperature of deflection under load (1.80 MPa): 136 °C (ISO 75-1,-2)
- Temperature of deflection under load (0.45 MPa): 149 °C (ISO 75-1,-2)
- Vicat softening temperature (50 N, 120 °C/h): 158 °C (ISO 306)
- Relative temperature index (Tensile strength): 140 °C (UL 746B)
- Coefficient of linear thermal expansion (23 to 55 °C, parallel): 0.65 × 10⁻⁴/K (ISO 11359-1,-2)
- Coefficient of linear thermal expansion (23 to 55 °C, normal): 0.65 × 10⁻⁴/K (ISO 11359-1,-2)
- Burning behavior (1.5 mm): HB (UL 94)
- Glow wire test (GWFI, 2.0 mm): 850 °C (IEC 60695-2-12)
Electrical Properties (23 °C / 50% r.h.)
- Relative permittivity (100 Hz): 3 (IEC 60250)
- Relative permittivity (1 MHz): 2.9 (IEC 60250)
- Dissipation factor (100 Hz): 10 × 10⁻⁴ (IEC 60250)
- Dissipation factor (1 MHz): 90 × 10⁻⁴ (IEC 60250)
- Volume resistivity: 1E15 Ohm·m (IEC 62631-3-1)
- Surface resistivity: 1E16 Ohm (IEC 62631-3-2)
- Electrical strength (1 mm): 35 kV/mm (IEC 60243-1)
- Comparative tracking index (CTI A): 250 (IEC 60112)
Other Properties (23 °C)
- Water absorption (saturation value): 0.3% (ISO 62)
- Water absorption (equilibrium value, 50% r.h.): 0.12% (ISO 62)
- Density: 1180 kg/m³ (ISO 1183-1)
Material Specific Properties
- Refractive index: 1.578 (ISO 489)
- Luminous transmittance (1 mm, clear transparent materials): 89% (ISO 13468-2)
Use & Applications
- Automotive Lighting: Brake/indicator light covers, Headlamp reflectors & bezels
- Injection-Molded Components: Heat-resistant housings; Precision optical parts
Features & Benefits
Exceptional Heat Resistance
Apec® 1695 withstands temperatures up to 158°C (VST/B 120), ensuring stability in high-heat environments like headlamp assemblies. Prevents warping during prolonged use.
Easy Flow & Release
Optimized melt flow (45 cm³/10 min) reduces injection pressure and cycle times. Simplifies molding of thin-walled parts like light covers without sticking.
Superior Dimensional Stability
Low, uniform shrinkage (0.75% parallel/normal) maintains tight tolerances in complex geometries. Critical for seamless fit in automotive reflectors.