Plastic Granules
Apec 1745 RE Thermoplastic Resin High Heat Grade
Apec® 1745 RE is a high-heat polycarbonate resin. This partially bio-circular grade (via ISCC PLUS mass balance) offers easy release, superheated steam sterilization up to 143°C, USP Class VI compliance, ISO 10993-1 biocompatibility, and a 170°C Vicat softening point. Ideal for reusable medical devices and sustainable solutions.
Download PDF
ISO TDS
Typical property data
Physical Properties (Rheological)
- Melt Volume-Flow Rate (MVR): 17 cm³/10 min (330°C/2.16 kg) (ISO 1133)
- Molding Shrinkage (Parallel/Normal): 0.85 % (60x60x2 mm³, 500 bar) (ISO 294-4)
Mechanical Properties (23 °C, 50% r.h.)
- Tensile Modulus: 2400 MPa (ISO 527-1,-2)
- Yield Stress: 70 MPa (ISO 527-1,-2)
- Yield Strain: 6.8 % (ISO 527-1,-2)
- Nominal Strain at Break: >50 % (ISO 527-1,-2)
- Flexural Modulus: 2400 MPa (ISO 178)
- Ball Indentation Hardness: 120 N/mm² (ISO 2039-1)
Thermal Properties
- Deflection Temperature Under Load (1.80 MPa): 148°C (ISO 75-1,-2)
- Deflection Temperature Under Load (0.45 MPa): 161°C (ISO 75-1,-2)
- Vicat Softening Temperature (50N, 120°C/h): 170°C (ISO 306)
- Coefficient of Linear Thermal Expansion (Parallel/Normal): 0.65 x 10⁻⁴/K (23°C to 55°C) (ISO 11359-1,-2)
- Burning Behavior: UL 94 HB (1.5 mm) (UL 94)
Electrical Properties (23 °C, 50% r.h.)
- Relative Permittivity (100 Hz): 3 (IEC 60250)
- Relative Permittivity (1 MHz): 2.9 (IEC 60250)
- Volume Resistivity: 1E15 Ohm·m (IEC 62631-3-1)
- Surface Resistivity: 1E16 Ohm (IEC 62631-3-2)
- Electrical Strength: 35 kV/mm (IEC 60243-1)
- Comparative Tracking Index (CTI): 250 (IEC 60112)
Other Properties (23 °C)
- Water Absorption (Saturation Value): 0.3 % (ISO 62)
- Water Absorption (Equilibrium Value): 0.12 % (ISO 62)
- Density: 1170 kg/m³ (ISO 1183-1)
Material-Specific Properties
- Refractive Index: 1.578 (ISO 489)
- Luminous Transmittance (1 mm): 88 % (ISO 13468-2)
Use & Applications
- Injection molding
- Films for medical packaging
- Contact lens holders
- Medical vessels
- Safety valve for respiration aids
- Syringe tops
Features & Benefits
Medical-Grade Safety & Compliance
Apec® 1745 RE meets USP Class VI and ISO 10993-1 standards, ensuring biocompatibility for implants and sterilization. Reduces regulatory hurdles for critical healthcare applications.
Sustainable, High-Performance Material
Attributed via ISCC PLUS mass balance, this bio-circular resin cuts carbon footprint without sacrificing heat resistance (170°C VST) or mechanical strength. Ideal for eco-driven procurement.
Reliable Sterilization Resilience
It withstands superheated steam sterilization up to 143°C, enabling reuse of medical components like surgical tools or respiratory valves. Lowers replacement costs and downtime.